Quick test for reversible and irreversible PID of bifacial PERC solar cells
Source abstract
Abstract
Abstract High voltage stress at the rear side of bifacial PERC cells leads to severe power losses. In contrast to monofacial PERC solar cells, reversible de-polarization related potential induced degradation (PID-p) and irreversible corrosive potential induced degradation (PID-c) can occur. Our results show that a reliable assessment of the solar cells power losses requires a modified PID test method which includes illumination in addition to the high voltage stress test. Furthermore, a recovery step needs to be added to the test scheme to separate reversible PID-p contributions from irreversible PID-c damages. We show that both, the degree of degradation as well as the contributions of PID-p and PIC-c depend sensitively on the solar cell under consideration. Thus, we propose to include both illumination during PID stress as well as a recovery step in the PID test scheme for bifacial PERC cells. Additionally, we show that the most sensitive cell parameter for the detection of rear side PID is given by the rear side measurement of the short circuit current. Finally, we present results showing that a 0.1 sun illumination during this characterization step is sufficient for an assessment of the PID. Based on these results, we propose a test setup which combines the required stress test conditions with an in-situ tracking of the PID.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules10.1002/pip.3028 ↗
2. Investigation of the impact of illumination on the polarization-type potential-induced degradation of crystalline silicon photovoltaic modules10.1109/JPHOTOV.2018.2843791 ↗
3. Physics of potential-induced degradation in bifacial p-PERC solar cells10.1016/j.solmat.2019.109950 ↗
4. Local corrosion of silicon as root cause for potential‐induced degradation at the rear side of bifacial PERC solar cells10.1002/pssr.201900163 ↗
5. Root cause analysis on corrosive potential-induced degradation effects at the rear side of bifacial silicon PERC solar cells10.1016/j.solmat.2019.110062 ↗
6. Microstructural analysis of local silicon corrosion of bifacial solar cells as root cause of potential‐induced degradation at the rear side10.1002/pssa.201900334 ↗
7. Potential-induced degradation of bifacial PERC solar cells under illumination10.1109/JPHOTOV.2019.2937231 ↗
8. PERC+: industrial PERC solar cells with rear Al grid enabling bifaciality and reduced Al paste consumption10.1002/pip.2712 ↗
9. Potential induced degradation of solar cells and panels
10. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
11. Swanson · 2005
12. Rapid progression and subsequent saturation of polarization-type potential-induced degradation of n-type front-emitter crystalline-silicon photovoltaic modules10.7567/JJAP.57.122301 ↗
13. Electronic and chemical properties of the c-Si/Al2O3 interface10.1063/1.3587227 ↗
14. On the discrepancy between leakage currents and potential-induced degradation of crystalline silicon modules
15. Importance of defect photoionization in silicon-rich SiNx dielectrics for high PID resistance
16. Naumann · 2014
17. Silicon nitride and related materials10.1111/j.1151-2916.2000.tb01182.x ↗
18. Self‐healing breakdown measurements of pyrolytic aluminum oxide films on silicon10.1063/1.1659779 ↗
19. Electrical conduction and dielectric breakdown in aluminum oxide insulators on silicon10.1109/16.817577 ↗
20. Spectral characterization of solar cells and modules using LED-based solar simulators10.1016/j.solmat.2019.02.007 ↗
21. Interlaboratory study to determine repeatability of the damp-heat test method for potential-induced degradation and polarization in crystalline silicon photovoltaic modules10.1109/JPHOTOV.2014.2361650 ↗
22. Elucidating the mechanism of potential induced degradation delay effect by ultraviolet light irradiation for p-type crystalline silicon solar cells10.1016/j.solener.2020.02.034 ↗
23. Electrically active sodium-related defect centres in silicon10.1088/0268-1242/28/10/105010 ↗