Highly crystallized tungsten doped indium oxide film stabilizes silicon heterojunction solar cells in sodium environment
Source abstract
Abstract
High-efficient silicon heterojunction (SHJ) solar cells are ideal bifacial devices. In this application context, Na+ ions induced degradations from encapsulation soda-lime glass are of significance. We conducted accelerated Na+ ions aging experiments at 85 °C, 85% relative humidity without encapsulation to simulate damp heat test in soda-lime glass for SHJ solar cells. It is found that Na+ ions accelerated the formation of metal In and In(OH)3 or InOOH in damp heat condition, which destroyed the capping metal oxide, i.e., tungsten doped indium oxide (IWO). Interestingly, it demonstrates that the device stability is highly dependent on the crystallinity of IWO films. IWO films with large grains are more resistive to Na+ ions erosion, and consequently, account for the enhanced device stability of SHJ solar cells. We believe this work provides a guide for designing more reliable bifacial SHJ solar cells installed in hot climates and coastal areas.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. High-efficiency silicon heterojunction solar cells: a review10.1515/green-2011-0018 ↗
2. Achievement of more than 25% conversion efficiency with crystalline silicon heterojunction solar cell10.1109/JPHOTOV.2014.2352151 ↗
3. Development status of high-efficiency HIT solar cells10.1016/j.solmat.2010.04.030 ↗
4. 25.11% efficiency silicon heterojunction solar cell with low deposition rate intrinsic amorphous silicon buffer layers10.1016/j.solmat.2020.110643 ↗
5. Silicon heterojunction solar cell with interdigitated back contacts for a photoconversion efficiency over 26%10.1038/nenergy.2017.32 ↗
6. 2020
7. Evaluation of the performance and degradation of crystalline silicon-based photovoltaic modules in the Saharan environment10.1016/j.energy.2018.03.135 ↗
8. Effects of SiOx barrier layer prepared by plasma-enhanced chemical vapor deposition on improvement of long-term reliability and production cost for Cu-plated amorphous Si/crystalline Si heterojunction solar cells10.1016/j.solmat.2016.12.029 ↗
9. Damp heat induced degradation of silicon heterojunction solar cells with Cu-plated contacts10.1109/JPHOTOV.2019.2941693 ↗
10. A reliability study of silicon heterojunction photovoltaic modules exposed to damp heat testing10.1016/j.mee.2019.111081 ↗
11. Reduction in the short-circuit current density of silicon heterojunction photovoltaic modules subjected to potential-induced degradation tests10.1016/j.solmat.2016.12.027 ↗
12. The role of stacking faults for the formation of shunts during potential-induced degradation of crystalline Si solar cells10.1002/pssr.201307090 ↗
13. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
14. Sodium accumulation at potential-induced degradation shunted areas in polycrystalline silicon modules10.1109/JPHOTOV.2016.2601950 ↗
15. Consideration on Na diffusion and recovery phenomena in potential-induced degradation for crystalline Si photovoltaic modules10.7567/JJAP.55.02BF10 ↗
16. The influence of sodium ions decorated micro-cracks on the evolution of potential induced degradation in p-type crystalline silicon solar cells10.1016/j.solener.2018.08.082 ↗
17. Origin of Na causing potential-induced degradation for p-type crystalline Si photovoltaic modules10.1063/1.5040516 ↗
18. Changes in the current density-voltage and external quantum efficiency characteristics of n-type single-crystalline silicon photovoltaic modules with a rear-side emitter undergoing potential-induced degradation10.1016/j.solmat.2016.03.003 ↗
19. Multistage performance deterioration in n-type crystalline silicon photovoltaic modules undergoing potential-induced degradation10.1016/j.microrel.2018.03.018 ↗
20. Rapid progression and subsequent saturation of polarization-type potential-induced degradation of n-type front-emitter crystalline-silicon photovoltaic modules10.7567/JJAP.57.122301 ↗
21. Influence of sodium on the potential-induced degradation for n-type crystalline silicon photovoltaic modules
22. Potential-induced degradation of bifacial PERC solar cells under illumination10.1109/JPHOTOV.2019.2937231 ↗
23. Microstructural analysis of local silicon corrosion of bifacial solar cells as root cause of potential‐induced degradation at the rear side10.1002/pssa.201900334 ↗
24. Local corrosion of silicon as root cause for potential‐induced degradation at the rear side of bifacial PERC solar cells10.1002/pssr.201900163 ↗
25. Root cause analysis on corrosive potential-induced degradation effects at the rear side of bifacial silicon PERC solar cells10.1016/j.solmat.2019.110062 ↗
26. Physics of potential-induced degradation in bifacial p-PERC solar cells10.1016/j.solmat.2019.109950 ↗
27. Potential-induced degradation of Cu(In,Ga)Se2photovoltaic modules10.7567/JJAP.54.08KC13 ↗
28. Potential-induced degradation of Cu(In,Ga)Se2 solar cells: alkali metal drift and diffusion effects10.1109/JPHOTOV.2018.2858549 ↗
29. Experimental evidence of PID effect on CIGS photovoltaic modules10.3390/en13030537 ↗
30. Rapid and accurate determination of series resistance and fill factor losses in industrial silicon solar cells
31. The amorphous/crystalline silicon interface research of HIT solar cells by simulation10.4028/www.scientific.net/AMR.773.124 ↗
32. An approach for improving the carriers transport properties of a-Si:H/c-Si heterojunction solar cells with efficiency of more than 27%10.1016/j.solener.2013.07.019 ↗
33. Underdense a-Si:H film capped by a dense film as the passivation layer of a silicon heterojunction solar cell10.1063/1.4966941 ↗
34. Physical and chemical degradation behavior of sputtered aluminum doped zinc oxide layers for Cu(In,Ga)Se2 solar cells10.1016/j.tsf.2013.10.149 ↗
35. A new grain boundary scattering model for metals
36. Damp-heat-stable, high-efficiency, industrial-size silicon heterojunction solar cells10.1016/j.joule.2020.03.003 ↗
37. Quantitative analyses of damp-heat-induced degradation in transparent conducting oxides10.1016/j.solmat.2013.12.014 ↗
38. Hydrogenated indium oxide window layers for high-efficiency Cu(In,Ga)Se2 solar cells10.1063/1.4921445 ↗
39. Damp heat stability and annealing behavior of aluminum doped zinc oxide films prepared by magnetron sputtering10.1016/j.tsf.2005.12.130 ↗
40. RF magnetron sputtered ZnO:Al thin films on glass substrates: a study of damp heat stability on their optical and electrical properties10.1016/j.solmat.2007.07.008 ↗
41. Stability of TCO window layers for thin-film CIGS solar cells upon damp heat exposures: part II
42. Positron annihilation studies on the damp heat degradation of ZnO:Al transparent conductive oxide layers for CIGS solar cells10.1109/JPHOTOV.2018.2863788 ↗
43. Influence of TCO and a-Si:H doping on SHJ contact resistivity10.1109/JPHOTOV.2021.3051206 ↗
44. Systematic XPS studies of metal oxides, hydroxides and peroxides10.1039/a908800h ↗
45. Characterization of Indium-Tin oxide interfaces using X-ray photoelectron spectroscopy and redox processes of a chemisorbed probe molecule effect of surface pretreatment conditions10.1021/la011101t ↗