journal article·2019-09Open access

Annealing prior to contact firing: A potential new approach to suppress LeTID

Chandany Sen, Catherine Chan, Phillip Hamer, Matthew Wright, Utkarshaa Varshney, Shaoyang Liu, Daniel Chen, Aref Samadi, Alison Ciesla, CheeMun Chong, Brett Hallam, Malcolm Abbott

Abstract

In this work, we introduce a new approach to suppress light and elevated temperature-induced degradation (LeTID) by applying a pre-fire annealing step using rapid thermal processing (RTP) and discuss the impact of this process on the evolution of bulk and surface lifetime components. We demonstrate that pre-fire annealing at low temperatures and/or shorter holding times allows a significant amount of hydrogen to migrate into the bulk to passivate bulk defects as including grain boundaries and dislocation clusters, without causing surface deterioration. As such, the addition of the pre-fire annealing step results in larger improvements in bulk and surface lifetime than that of the control samples. These conditions also significantly suppress LeTID. Increasing pre-fire annealing temperature and duration is shown to completely mitigate LeTID. However, this process may cause surface deterioration, possibly due to the excessive effusion of hydrogen out of the dielectric layer. Injection-dependent lifetime analysis shows that at the most degraded state, the bulk lifetime of the pre-fire annealed samples (650 °C–1 min and 3 min) remains relatively higher (∼110 μs–∼120 μs) than that of the control sample (∼40 μs). Applying pre-fire annealing process at 700 °C on Cz-Si samples and testing the boron-oxygen (B-O) generation behavior suggest that these processes cause a reduction in the hydrogen concentration in the bulk, resulting in slower B-O regeneration rate and reduction of regeneration extent. This result also implies that the suppression of LeTID in mc-Si by applying a pre-fire thermal treatment is likely due to a reduction of hydrogen in the bulk, and this highlights that the proposed method of pre-fire annealing may be unsuitable for material such as p-type Cz silicon subjected to B-O related degradation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Light induced degradation of rear passivated Mc-Si solar cells
2. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
3. A new mc-Si degradation effect called LeTID
4. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature-induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
5. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
6. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
7. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
8. Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22 %10.1016/j.egypro.2017.09.308 ↗
9. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
10. Lifetime degradation in multicrystalline silicon under illumination at elevated temperature: indications for the involvement of hydrogen
11. Evaluating root cause: the distinct roles of hydrogen and firing in activating light- A nd elevated temperature-induced degradation10.1063/1.5041756 ↗
12. Hydrogen-induced degradation
13. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
14. Evaluating the impact of SiN x thickness on lifetime degradation in silicon
15. Influence of silicon nitride and its hydrogen content of carrier-induced degradation in multicrystalline silicon
16. Influence of Al2O3 and SiNx passivation layers on LeTID
17. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
18. H loss mechanism during anneal of silicon nitride: chemical dissociation10.1063/1.1321730 ↗
19. The role of hydrogenation and gettering in enhancing the efficiency of next-generation Si solar cells: an industrial perspective
20. < 700 mV open-circuit voltages on defect-engineered P-type silicon heterojunction solar cells on Czochralski and multicrystalline wafers
21. 21.63% industrial screen-printed multicrystalline Si solar cell10.1002/pssr.201600453 ↗
22. Assessing the impact of thermal profiles on the elimination of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2874769 ↗
23. States of hydrogen in crystalline silicon10.1016/0921-4526(91)90130-7 ↗
24. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
25. Influence of the high-temperature “firing” step on high-rate plasma deposited silicon nitride films used as bulk passivating antireflection coatings on silicon solar cells
26. Dissociation reactions of hydrogen in remote plasma-enhanced chemical-vapor-deposition silicon nitride10.1116/1.1398538 ↗
27. Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4833243 ↗
28. Study of the composition of hydrogenated silicon nitride SiNx:H for efficient surface and bulk passivation of silicon10.1016/j.solmat.2009.01.023 ↗
29. REC Group · 2019
30. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
31. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
32. System performance loss due to LeTID10.1016/j.egypro.2017.09.260 ↗
33. Acceleration and mitigation of carrier-induced degradation in p-type multi-crystalline silicon10.1002/pssr.201510437 ↗
34. S. Liu, D. Payne, D. Chen, U. Varshney, A. Samadi, C. Sen, A. Ciesla, M. Abbott, C. Chan, Acceleration and mitigation of hydrogen induced degradation in p -type cast-mono silicon, Asia-Pacific Sol. Res. Conf. (n.d.) 9–10.
35. 2018
36. Dupont · 2015
37. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
38. Instability of increased contact resistance in silicon solar cells following post-firing thermal processes10.1002/solr.201700129 ↗
39. Impact of extended contact cofiring on multicrystalline silicon solar cell parameters10.1109/JPHOTOV.2016.2621342 ↗
40. Temperature induced degradation of the contact resistance of Ag-screen printed p-type silicon solar cells
41. The behavior and transport of hydrogen in silicon solar cells observed through changes in contact resistance
42. The behavior and transport of hydrogen in silicon solar cells observed through changes in contact resistance
43. Should the refractive index at 633 nm be used to characterize silicon nitride films?
44. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
45. High speed regeneration of BO-defects: improving long term solar cell performance within seconds
46. A quasi-steady-state open-circuit voltage method for solar cell characterization
47. Generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors10.1063/1.371633 ↗
48. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
49. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
50. Light-induced degradation variation in industrial multicrystalline PERC silicon solar cells10.1063/1.5049332 ↗
51. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
52. Evolution of LeTID defects in p-type multicrystalline silicon during degradation and regeneration10.1109/JPHOTOV.2017.2695496 ↗
53. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon : introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
54. High-efficiency solar cells on edge-defined film-fed grown (18.2%) and string ribbon (17.8%) silicon by rapid thermal processing10.1063/1.1638636 ↗
55. Boron reactivation kinetics in hydrogenated silicon after annealing in the dark or under illumination10.1103/PhysRevB.43.4361 ↗
56. Structural and passivating properties of SiNx: H deposited using different precursor gases
57. The interaction of hydrogen with deep level defects in silicon10.4028/www.scientific.net/SSP.71.173 ↗