journal article·2021-07

New insights on LeTID/BO-LID in p-type mono-crystalline silicon

Dehang Lin, Zechen Hu, Qiyuan He, Deren Yang, Lihui Song, Xuegong Yu

Publisher page

Abstract

Abstract In this work, light-induced degradation (LID) experiments were performed on p-type boron-doped Czochralski silicon (Cz-Si) wafers under different conditions, aiming to separately characterize boron-oxygen related LID (BO-LID) and “light and elevated temperature-induced degradation” (LeTID). We found that the regeneration rate of BO-LID, as well as the extent and kinetics of LeTID, were strongly influenced by peak firing temperature. These dependences can be explained by the variation of hydrogen concentration, which was modulated by peak firing temperature. Furthermore, we found that extending the duration of dark annealing pre-treatment decelerates the subsequent regeneration of BO defects. This result revealed that, under dark annealing, the evolution of LeTID was accompanied by a notable decrease in the mobile hydrogen concentration. Supported by this phenomenon, a hydrogen-related model based on reversible reaction is proposed to describe the LeTID behavior in crystalline silicon.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Development of the PERC solar cell10.1109/JPHOTOV.2019.2899460 ↗
2. Electronic properties of light-induced recombination centers in boron-doped Czochralski silicon10.1063/1.371186 ↗
3. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
4. Fundamental boron-oxygen-related carrier lifetime limit in mono- and multicrystalline silicon10.1002/pip.586 ↗
5. Investigations on the long time behavior of the metastable boron–oxygen complex in crystalline silicon10.1002/pip.779 ↗
6. Deactivation of the boron–oxygen recombination center in silicon by illumination at elevated temperature10.1002/pssr.200802009 ↗
7. Light induced degradation of rear passivated mc-Si solar cells
8. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
9. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
10. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
11. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
12. Correlation of the LeTID amplitude to the Aluminium bulk concentration and Oxygen precipitation in PERC solar cells10.1016/j.solmat.2018.06.009 ↗
13. Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22 %10.1016/j.egypro.2017.09.308 ↗
14. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
15. Impact of dark annealing on the kinetics of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2866325 ↗
16. Influence of Al2O3 and SiNx passivation layers on LeTID10.1016/j.egypro.2016.07.079 ↗
17. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
18. Understanding the light-induced lifetime degradation and regeneration in multicrystalline silicon10.1016/j.egypro.2016.07.060 ↗
19. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
20. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
21. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
22. Influence of bound hydrogen states on BO-regeneration kinetics and consequences for high-speed regeneration processes10.1016/j.solmat.2014.06.027 ↗
23. Formation, dissociation, and diffusion of various hydrogen dimers in silicon10.1002/pssb.201600779 ↗
24. Contactless determination of current–voltage characteristics and minority‐carrier lifetimes in semiconductors from quasi‐steady‐state photoconductance data10.1063/1.117723 ↗
25. Lifetime recovery in p-type Czochralski silicon due to the reconfiguration of boron–oxygen complexes via a hole-emitting process10.1063/1.3581215 ↗
26. Impact of hydrogen concentration on the regeneration of light induced degradation10.1016/j.egypro.2011.06.100 ↗
27. BO-related defects: overcoming bulk lifetime degradation in crystalline Si by regeneration10.4028/www.scientific.net/SSP.242.80 ↗
28. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
29. Kinetics of the boron-oxygen related defect in theory and experiment10.1063/1.3517155 ↗
30. Impact of rapid firing thermal processes on meta-stable defects: preformation of the LeTID and the suppression of B-O defects
31. Multiple pathways for permanent deactivation of boron-oxygen defects in p-type silicon10.1016/j.solmat.2017.06.041 ↗
32. Hydrogen solubility and defects in silicon10.4028/www.scientific.net/MSF.143-147.861 ↗
33. Hydrogen molecules in boron-doped crystalline silicon10.1088/0268-1242/14/1/011 ↗
34. Boron reactivation kinetics in hydrogenated silicon after annealing in the dark or under illumination10.1103/PhysRevB.43.4361 ↗
35. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
36. On the impact of dark annealing and room temperature illumination on p-type multicrystalline silicon wafers10.1016/j.solmat.2018.09.018 ↗
37. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
38. Defect formation under high temperature dark-annealing compared to elevated temperature light soaking10.1016/j.solmat.2018.06.043 ↗
39. Possible candidates for impurities in mc-Si wafers responsible for light-induced lifetime degradation and regeneration10.1002/solr.201700159 ↗
40. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗