journal article·2021-05

Corrosion performance of slurry aluminide coatings in molten NaCl–KCl

B. Grégoire, C. Oskay, T.M. Meißner, M.C. Galetz

Publisher page

Abstract

Abstract The corrosion performance of water-based slurry aluminide coatings elaborated on iron- and nickel-based materials is investigated in molten chlorides as candidate heat transfer fluids (HTF) for thermal energy storage (TES) in third generation concentrated solar power (CSP) plants. This work presents a screening of four different materials (ferritic-martensitic P91 steel, austenitic stainless steel 316L, Inconel 600 and high-purity nickel) to investigate the influence of the alloying elements (e.g. Fe, Cr, Ni contents) on the microstructure and corrosion performance of slurry aluminide coatings. Individual metallic samples were diffusion-coated with slurries containing Al microparticles and subsequently exposed to molten NaCl–KCl at 700 °C for 100 h under argon. The experimental observations indicate that the performance of the aluminide coatings is governed by the precipitation of secondary phases within the B2 aluminide matrix rather than its intrinsic Al concentration (where B2 refers to either FeAl, (Fe,Ni)Al or NiAl intermetallic compounds). Of those, Fe-rich aluminide coatings were found to be more resistant to molten chlorides than Ni-rich ones. This is attributed to the greater solubility of Cr in iron aluminides than in nickel aluminides, preventing the precipitation of Cr-rich intermetallic compounds and/or Cr-rich carbides within the B2 matrix. Cr-rich phases were selectively dissolved upon exposure leaving the coating matrix with void channels. According to residual coating thickness measurements, the following ranking with increasing corrosion resistance can be given for Al-slurry coated materials: Inconel 600
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Adsorption and Cooling Systems · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Heat transfer fluids for concentrating solar power systems – a review10.1016/j.apenergy.2015.01.125 ↗
2. Advanced heat transfer fluids for direct molten salt line-focusing CSP plants10.1016/j.pecs.2018.02.002 ↗
3. Concentrating solar power tower technology: present status and outlook10.1515/nleng-2017-0171 ↗
4. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
5. Burgaleta · 2011
6. Impact of solar salt aging on corrosion of martensitic and austenitic steel for concentrating solar power plants10.1016/j.solmat.2019.110162 ↗
7. Materials compatibility for the next generation of concentrated solar power plants10.1016/j.ensm.2018.02.023 ↗
8. Corrosion mechanisms in molten salt thermal energy storage for concentrating solar power10.1016/j.rser.2019.109328 ↗
9. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review10.1007/s11705-018-1720-0 ↗
10. Purification strategy and effect of impurities on corrosivity of dehydrated carnallite for thermal solar applications10.1039/C9RA09352D ↗
11. Corrosion resistance of MCrAlX coatings in a molten chloride for thermal storage in concentrating solar power applications10.1038/s41529-017-0012-3 ↗
12. High temperature corrosion of Inconel 600 in NaCl-KCl molten salts
13. Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: Pre-oxidation treatment and isothermal corrosion tests10.1016/j.solmat.2017.02.019 ↗
14. Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. II: Electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
15. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
16. Effect of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl-KCl-MgCl2 salt at different temperatures10.1016/j.corsci.2018.08.021 ↗
17. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
18. Molten chloride salts for next generation concentrated solar power plants: Mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
19. Corrosion of corrosion-resistant and high-temperature nickel-based alloys in chloroaluminate melts10.1149/06404.0217ecst ↗
20. Corrosive resistance of nickel Hastelloy G-35 superalloy in various aggressive media10.1149/08614.0155ecst ↗
21. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part I: NaCl-KCl binary system10.1016/j.solmat.2020.110659 ↗
22. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part II: NaCl-KCl-MgCl2 ternary system10.1016/j.solmat.2020.110675 ↗
23. Ozeryanaya · 1985 · vol. 423 · 184
24. Electrochemistry of molten salt corrosion10.1016/0921-5093(91)90265-O ↗
25. Standard electrode potentials in molten chlorides10.1016/0013-4686(68)85016-9 ↗
26. Constantes électrochimiques des sels fondus, Techniques de l'Ingénieur
27. High temperature molten salt corrosion behavior of aluminide and nickel-aluminide coatings for heat storage in concentrated solar power plants10.1016/j.surfcoat.2018.05.081 ↗
28. Slurry aluminizing: a solution for molten nitrate salt corrosion in concentrated solar power plants10.1016/j.solmat.2015.11.024 ↗
29. Scale formation and degradation of diffusion coatings deposited on 9% Cr steel in molten solar salt10.3390/coatings9100687 ↗
30. High temperature corrosion beneath carbonate melts of aluminide coatings for CSP application10.1016/j.solmat.2020.110514 ↗
31. A novel type of environmentally friendly slurry coatings
32. Corrosion behaviour of various model alloys with NaCl-KCl coating10.1016/j.matchemphys.2005.03.015 ↗
33. Models describing the degradation of FeAl and NiAl alloys induced by ZnCl2-KCl melt at 400-450°C10.1016/j.corsci.2003.10.019 ↗
34. Thermo-economic analysis of high-temperature sensible thermal storage with different ternary eutectic alkali and alkaline earth metal chlorides10.1016/j.solener.2018.10.008 ↗
35. The role of combustion synthesis in the formation of slurry aluminization10.1016/j.intermet.2013.08.002 ↗
36. Cyclic oxidation and mechanical behaviour of slurry aluminide coatings for steam turbine components10.1016/j.surfcoat.2006.11.033 ↗
37. Microstructural evolution of slurry Fe aluminide coatings during high temperature steam oxidation10.4028/www.scientific.net/MSF.595-598.251 ↗
38. Slurry aluminizing mechanisms of Ni-based superalloys incorporating an electrosynthesized ceria diffusion barrier10.1016/j.matchemphys.2013.09.022 ↗
40. 1991
41. Donachie · 2002
42. International Standard · 2015 · 17245
43. Water-free methods of preparation for the analyses of chlorides in the high temperature oxidation in chloride containing atmospheres10.1515/pm-1998-360207 ↗
44. Concepts derived from phase diagram studies for the strengthening of Fe-Al based alloys10.1016/j.intermet.2004.10.015 ↗
45. Experimental investigation of phase equilibria in the Al-Cr-Fe system10.1016/j.calphad.2019.101638 ↗
46. The Heusler phase Ti25(Fe50-xNix)Al25 (0≤x≤50); structure and constitution10.1007/s11669-008-9389-6 ↗
47. Steam oxidation of aluminide coatings under high pressure and for long exposures10.1016/j.corsci.2018.08.053 ↗
48. Assessment of the Fe-Ni-Al system10.1016/j.intermet.2005.11.021 ↗
49. Ferritic Fe-Al-Ni-Cr alloys with coherent precipitates for high-temperature applications10.1016/j.msea.2004.01.108 ↗
50. Oxidation performance of repaired aluminide coatings on austenitic steel substrates10.1016/j.surfcoat.2017.07.059 ↗
51. Characterisation of aluminium diffusion coatings elaborated on austenitic stainless steels and on ferritic-martensitic steels10.1016/j.surfcoat.2018.01.086 ↗
52. Mechanisms of formation of diffusion aluminide coatings on nickel-based superalloys10.1007/BF00604047 ↗
53. Precipitation of α-Cr in B2-ordered NiAl10.1016/S0966-9795(98)00015-6 ↗
54. Precipitation of chromium containing phases in aluminide coated nickel-base superalloy single crystals10.1007/BF01154941 ↗
55. Thermodynamic modeling of the Al-Cr system10.1016/j.jallcom.2007.06.046 ↗
56. Microstructures of two-stage aluminized coatings on Inconel 60010.1016/0921-5093(95)09899-2 ↗
57. Microstructural degradation and interdiffusion behavior of NiAl and Ge-modified NiAl coatings deposited on Alloy 602 CA10.1016/j.surfcoat.2019.02.048 ↗
58. Thermodynamic properties of the Ni-Al-Cr system10.1016/S0966-9795(98)00138-1 ↗
59. Microstructures and interfaces in Ni-Al martensite: comparing HRTEM observations with continuum theories10.1016/S0020-7683(02)00167-1 ↗
60. Effect of alloying elements on martensitic transformation in the binary NiAl(β) phase alloys10.1007/BF02652338 ↗
61. Martensitic transformation in CVD NiAl and (Ni,Pt)Al bond coatings10.1016/S0257-8972(02)00585-6 ↗
62. Failure mechanism of an out-of-pack nickel aluminide coating cyclically oxidised at 1100°C with water accelerated cooling10.1016/j.surfcoat.2015.05.046 ↗
63. Transformation temperatures of martensite in β-phase nickel aluminide10.1007/BF02668010 ↗
64. Plastic flow and fracture of B2 NiAl-based intermetallic alloys containing a ductile second phase10.2355/isijinternational.31.1172 ↗
65. International Standard · 2012 · 26146
66. Reaction morphologies developed by nickel aluminides in type II hot corrosion conditions: The effect of chromium10.1016/j.corsci.2015.08.029 ↗
67. Intermetallic formation of Al-Fe and Al-Ni phases by ultrafast slurry aluminization (flash aluminizing)10.1016/j.surfcoat.2020.126011 ↗
68. Stability of protective oxide films in waste incineration environment – solubility measurement of oxides in molten chlorides10.1016/S0010-938X(01)00059-2 ↗
69. Hot corrosion of materials: fundamental studies
70. Chloride- and sulphate-induce hot corrosion mechanism of super austenitic stainless steel S13254 under dry gas environment10.1016/j.corsci.2019.108295 ↗