Abstract
Abstract We investigate the thermal stability of silicon surface passivation provided by aluminium oxide (Al 2 O 3 ) films deposited using atmospheric pressure chemical vapour deposition (APCVD) and fired in a belt furnace at a peak temperature of ~810 °C. Firing stability is investigated for p - and n -type substrates as a function of Al 2 O 3 film thickness both with and without a plasma-enhanced chemical vapour deposition (PECVD) SiN x capping layer, and for boron-diffused surfaces with a ~10 nm Al 2 O 3 film only. Excellent thermal stability of the passivation is demonstrated, with effective carrier lifetimes in n -type silicon wafers remaining stable or even improving after firing, and lifetimes in p -type wafers initially degrading slightly but recovering to above their initial values following ~10 min illumination by a halogen lamp at ~20 mW/cm 2 . Film thickness appears to be unimportant to stability, as does the presence of the capping layer. Surface recombination velocities of less than 3 cm/s for 1.35 Ω cm p -type and less than 2 cm/s for 1.2 Ω cm n -type substrates are measured after firing and illumination. The passivation of boron-diffused surfaces is also shown to improve slightly following firing, with a post-firing saturation current density of 42 fA/cm 2 on a diffusion with a sheet resistance of 100 Ω/□ and surface dopant concentration of ~1.3×10 19 cm −3 . Capacitance–voltage ( C – V ) measurements show that short firing times result in an initial reduction of the interface defect density D it and a slight increase of the negative insulator fixed charge density Q f , while longer firing results in a substantial increase in both Q f and D it .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Ultralow surface recombination of c-Si substrates passivated by plasma-assisted atomic layer deposited Al2O310.1063/1.2240736 ↗
2. Very low surface recombination velocities on p-type silicon wafers passivated with a dielectric with fixed negative charge10.1016/j.solmat.2006.04.014 ↗
3. High-speed spatial atomic-layer deposition of aluminum oxide layers for solar cell passivation10.1002/adma.201000766 ↗
4. Spatially separated atomic layer deposition of Al2O3, a new option for high-throughput Si solar cell passivation10.1002/pip.1092 ↗
5. Very low surface recombination velocity on p-type c-Si by high-rate plasma-deposited aluminum oxide10.1063/1.3250157 ↗
6. High quality aluminum oxide passivation layer for crystalline silicon solar cells deposited by parallel-plate plasma-enhanced chemical vapor deposition10.1143/APEX.3.012301 ↗
7. Low-temperature surface passivation of silicon for solar cells10.1149/1.2096673 ↗
8. Surface passivation of c-Si by atmospheric pressure chemical vapour deposition of Al2O310.1063/1.4718596 ↗
9. Effective surface passivation of crystalline silicon by rf sputtered aluminum oxide10.1002/pssr.200903140 ↗
10. Process control of reactive sputter deposition of AlOx and improved surface passivation of crystalline silicon10.1109/JPHOTOV.2012.2214765 ↗
11. Thermal stability of the Al2O3 passivation on p-type silicon surfaces for solar cell applications10.1002/pssr.200903209 ↗
12. B. Vermang, X. Loozen, C. Allebé, J. John, E. van Kerschaver, J. Poortmans, and R. Mertens, Characterization and implementation of thermal ALD Al2O3 as surface passivation for industrial Si solar cells, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 1051–1054.
13. Effective surface passivation of crystalline silicon using ultrathin Al2O3 films and Al2O3/SiNx stacks10.1002/pssr.200903272 ↗
14. Comparison of the thermal stability of single Al2O3 layers and Al2O3/SiNx stacks for the surface passivation of silicon10.1016/j.egypro.2011.06.141 ↗
15. Stability of Al2O3 and Al2O3/a-SiNx:H stacks for surface passivation of crystalline silicon10.1063/1.3264572 ↗
16. Comparison of ICP-AlOx and ALD-Al2O3 layers for the rear surface passivation of c-Si solar cells10.1016/j.egypro.2012.07.080 ↗
17. A. Richter, S. Henneck, J. Benick, M. Hörteis, M. Hermle, and S.W. Glunz, Firing stable Al2O3/SiNx layer stack passivation for the front side boron emitter of n-type silicon solar cells, in: P roceedings of the 25th European Photovoltaic Solar Energy Conference, Valencia, Spain, 2010, pp. 1453–1459.
18. B. Vermang, H. Goverde, A. Lorenz, A. Uruena, G. Vereecke, J. Meersschaut, E. Cornagliotti, A. Rothschild, J. John, J. Poortmans, and R. Mertens, On the blistering of atomic layer deposited Al2O3 as Si surface passivation, in: Proceedings of the 37th IEEE Photovoltaic Specialists Conference, Seattle, USA, 2011, pp. 3562–3567.10.1109/PVSC.2011.6185916 ↗
19. B. Vermang, H. Goverde, A. Lorenz, A. Uruena, J. Das, P. Choulat, E. Cornagliotti, A. Rothschild, J. John, J. Poortmans, and R. Mertens, On the blistering of Al2O3 passivation layers for Si solar cells, in: Proceedings of the 26th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2011, pp. 1129–1131.
20. L. Hennen, E.H.A. Granneman, and W.M.M. Kessels, Analysis of blister formation in spatial ALD Al2O3 for silicon surface passivation, in: Proceedings of the 38th IEEE Photovoltaic Specialists Conference, Austin, USA, 2012, pp. 1049–1054.10.1109/PVSC.2012.6317783 ↗
21. L.E. Black, K.M. Provancha, and K.R. McIntosh, “Surface passivation of crystalline silicon by APCVD aluminium oxide”, in: Proceedings of the 26th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2011, pp. 1120–1124.
22. Improved quantitative description of Auger recombination in crystalline silicon10.1103/PhysRevB.86.165202 ↗
23. J. Brody, A. Rohatgi, and A. Ristow, Guidelines for more accurate determination and interpretation of effective lifetime from measured quasi-steady-state photoconductance, in: Proceedings of the 11th Workshop on Crystalline Silicon Solar Cell Materials and Processes, Estes Park, Colorado, August 19–22 2001, pp. 163–167.
24. Accurate measurements of the silicon intrinsic carrier density from 78 to 340K10.1063/1.354551 ↗
25. Improved method for the oxide thickness extraction in MOS structures with ultrathin gate dielectrics10.1109/66.843630 ↗
26. Nicollian · 1982
27. Surface states at steam-grown silicon-silicon dioxide interfaces10.1109/T-ED.1966.15827 ↗
28. Injection dependence of the effective lifetime of n-type Si passivated by Al2O3: an edge effect?
29. Light induced curing (LIC) of passivation layers deposited on native silicon oxide10.1016/j.egypro.2012.07.075 ↗
30. Imaging interstitial iron concentrations in boron-doped crystalline silicon using photoluminescence10.1063/1.2903895 ↗
31. M. Kuhn and E.H. Nicollian, Nonequilibrium effects in quasi-static MOS measurements, 118, 1971, 370–37310.1149/1.2408053 ↗
32. Modeling recombination at the Si–Al2O3 interface10.1109/JPHOTOV.2013.2247464 ↗
33. Determination of Si–SiO2 interface recombination parameters using a gate-controlled point-junction diode under illumination,10.1109/16.2441 ↗
34. L.E. Black, T. Allen, and K.R. McIntosh, Safe and inexpensive Al2O3 deposited by APCVD with single-source precursor, in: Proceedings of the 28th European Photovoltaic Solar Energy Conference, Paris, France, 2013, in press.