Changes in hydrogen concentration and defect state density at the poly-Si/SiOx/c-Si interface due to firing

Christina Hollemann, Nils Folchert, Steven P. Harvey, Paul Stradins, David L. Young, Caroline Lima Salles de Souza, Michael Rienäcker, Felix Haase, Rolf Brendel, Robby Peibst

Publisher page

Abstract

Abstract We determined the density of defect states of poly-Si/SiOx/c-Si junctions featuring a wet chemical interfacial oxide from lifetime measurements using the MarcoPOLO model to calculate recombination and contact resistance in poly-Si/SiOx/c-Si-junctions. In samples that did not receive any hydrogen treatment, the Dit,cSi is about 2 × 1012 cm−2 eV⁻1 before firing and rises to 3–7 × 1012 cm⁻2 eV⁻1 during firing at measured peak temperatures between 620 °C and 863 °C. To address the question of why AlOx/SiNy stacks in contrast to pure SiNy layers for hydrogenation during firing provides better passivation quality, we have measured the hydrogen concentrations at the poly-Si/SiOx/c-Si interface as a function of AlOx layer thickness and compared these to J0 and calculated Dit,c-Si values. We observe an increase of the hydrogen concentration at the SiOx/c-Si interface upon firing as a function of the firing temperature that exceeds the defect concentrations at the interface several times. However, the AlOx layer thickness appears to cause an increase in hydrogen concentration at the SiOx/c-Si interface in these samples rather than exhibiting a hydrogen blocking property.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Design rules for high-efficiency both-sides-contacted silicon solar cells with balanced charge carrier transport and recombination losses10.1038/s41560-021-00805-w ↗
2. Laser contact openings for local poly-Si-metal contacts enabling 26.1%-efficient POLO-IBC solar cells10.1016/j.solmat.2018.06.020 ↗
3. 2021
4. Full Wafer Size IBC Cell with Polysilicon Passivating Contacts
5. Study of screen printed metallization for polysilicon based passivating contacts10.1016/j.egypro.2017.09.242 ↗
6. n-Type polysilicon passivating contact for industrial bifacial n-type solar cells10.1016/j.solmat.2016.06.034 ↗
7. Firing stability of doped polysilicon passivation layers. 5 pages/37th European photovoltaic solar energy conference and exhibition; 188-192
8. On the hydrogenation of Poly-Si passivating contacts by Al2O3 and SiN thin films10.1016/j.solmat.2020.110592 ↗
9. Polycrystalline silicon passivated tunneling contacts for high efficiency silicon solar cells10.1557/jmr.2016.77 ↗
10. Design and application of ion-implanted polySi passivating contacts for interdigitated back contact c-Si solar cells10.1063/1.4940364 ↗
11. Yang · 2018 · 40026
12. A passivating contact for silicon solar cells formed during a single firing thermal annealing10.1038/s41560-018-0239-4 ↗
13. Study of screen printed metallization for polysilicon based passivating contacts10.1016/j.egypro.2017.09.242 ↗
14. monoPoly™ cells: large-area crystalline silicon solar cells with fire-through screen printed contact to doped polysilicon surfaces10.1016/j.solmat.2018.05.059 ↗
15. On the passivation mechanism of poly-silicon and thin silicon oxide on crystal silicon wafers10.1016/j.solener.2019.10.064 ↗
16. On the influence of the SiN x composition on the firing stability of poly‐Si/SiN x stacks
17. Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristics10.1016/j.solmat.2013.09.017 ↗
18. Analysis of hydrogen distribution and migration in fired passivating contacts (FPC)10.1016/j.solmat.2019.110018 ↗
19. C. Hollemann, M. Rienäcker, A. Soeriyadi, C. Madumelu, F. Haase, J. Krügener, B. Hallam, R. Brendel, R. Peibst, Firing stability of tube furnace-annealed n-type poly-Si on oxide junctions, Prog. Photovoltaics Res. Appl. accepted for publication.
20. Defects in single-crystal silicon induced by hydrogenation10.1103/PhysRevB.35.4166 ↗
21. Atomic‐layer‐deposited Al 2 O 3 as effective barrier against the diffusion of hydrogen from SiN x :H layers into crystalline silicon during rapid thermal annealing10.1002/pssr.202000367 ↗
22. Study on the interfacial oxide in passivating contacts
23. A simple method for pinhole detection in carrier selective polo-junctions for high efficiency silicon solar cells10.1016/j.solmat.2017.05.041 ↗
24. SIMS measurement of hydrogen and deuterium detection limits in silicon: comparison of different SIMS instrumentation
25. Measurement of the emitter saturation current by a contactless photoconductivity decay method
26. Improved parameterization of auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
27. Optical dielectric function and infrared absorption of hydrogenated amorphous silicon nitride films: Experimental results and effective-medium-approximation analysis10.1103/PhysRevB.42.3666 ↗
28. Modeling recombination and contact resistance of poly‐Si junctions10.1002/pip.3327 ↗
29. Determination of Si-SiO/sub 2/interface recombination parameters using a gate-controlled point-junction diode under illumination10.1109/16.2441 ↗
30. Modelling the annealing of poly-Si/SiOx/c-Si junctions
31. A freeware 1D Emitter model for silicon solar cells
32. A simple model describing the symmetric I-V characteristics of p polycrystalline Si/n monocrystalline Si, and n polycrystalline Si/p monocrystalline junctions10.1109/JPHOTOV.2014.2310740 ↗
33. Working principle of carrier selective poly-Si/c-Si junctions: is tunnelling the whole story?10.1016/j.solmat.2016.05.045 ↗
34. Impact of illumination level and oxide parameters on Shockley–Read–Hall recombination at the Si‐SiO 2 interface10.1063/1.350782 ↗
35. Nicollian · 1982
36. Hydrogen passivation of poly-Si/SiO x contacts for Si solar cells using Al 2 O 3 studied with deuterium10.1063/1.5031118 ↗
37. Stress‐related problems in silicon technology10.1063/1.349282 ↗
38. Hydrogen-induced platelets in disordered silicon10.1016/0038-1098(96)00283-9 ↗
39. Hydrogen-induced platelets in silicon: separation of nucleation and growth10.4028/www.scientific.net/MSF.83-87.33 ↗
40. Nucleation mechanism of hydrogen-induced platelets in single crystal and polycrystalline silicon10.1016/S0921-4526(99)00452-4 ↗
41. Hydrogen in crystalline semiconductors10.1016/0921-4526(91)90104-M ↗
42. Electrical measurements on ion-implanted LPCVD polycrystalline silicon films10.1016/0038-1101(83)90021-7 ↗
43. Impact of silicon nitride film properties on hydrogen in-diffusion into crystalline silicon
44. Molecular models and activation energies for bonding rearrangement in plasma-deposited a−SiNx:H dielectric thin films treated by rapid thermal annealing10.1103/PhysRevB.63.245320 ↗
45. Optimization of Al fire-through contacts for AlO X –SiN X rear passivated bifacial p -PERC10.1109/JPHOTOV.2020.2983006 ↗