Lifetimes exceeding 1ms in 1-Ωcm boron-doped Cz-silicon

D.C. Walter, B. Lim, K. Bothe, R. Falster, V.V. Voronkov, J. Schmidt

Publisher page

Abstract

Abstract We perform carrier lifetime investigations on oxygen-rich boron-doped Czochralski-grown silicon (Cz-Si) wafers. As a characteristic feature of oxygen-rich boron-doped silicon materials, their lifetime is generally limited by boron–oxygen-related defects, intensifying their recombination-active properties under illumination or, more generally speaking, minority-carrier injection. In this study, we examine the following characteristic lifetime values of boron-doped Cz-Si: τ 0 after annealing in darkness (i.e. complete boron–oxygen defect deactivation), τ d after illumination at room-temperature (i.e. in the completely degraded state) and τ 0 p after illumination at elevated temperature (i.e. after ‘permanent recovery’). We show that the permanent recovery process can be strongly influenced by a rapid thermal annealing (RTA) step performed in a conventional belt-firing furnace in advance of the permanent recovery process. We show that all measured lifetimes, i.e. τ 0 , τ d as well as τ 0 p , are strongly influenced by the RTA process. We observe a strong increase of the lifetime after permanent recovery, depending critically on the RTA process parameters. On 1-Ω cm Cz-Si material after permanent recovery we measure lifetimes of τ 0p (Δ n =1.5×10 15 cm −3 )=210 µs without applying the RTA process and up to τ 0p (Δ n =1.5×10 15 cm −3 )=2020 µs using optimized RTA conditions. Apart from the very high lifetimes achieved, the applied RTA process step also strongly influences the kinetics of the permanent recovery process. The recovery process is accelerated by almost two orders of magnitude, compared to a non-treated sample, which proves the industrial relevance of the process. We discuss the results within a recently proposed defect model which ascribes the observed dependence of the kinetics of the recovery process to the presence of boron nano-precipitates and their interaction with free interstitial boron atoms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. H. Fischer and W. Pschunder, Investigation of photon and thermal induced changes in silicon solar cells, in: Proceedings 10th IEEE PVSC, Palo Alto, CA IEEE, New York, 1973 1974, p. 404.
2. J. Schmidt, A.G. Aberle, R. Hezel, Investigation of carrier lifeime instabilities in Cz-grown silicon, in Proceedings of the 26th IEEE PVSC, 1997.
3. S.W. Glunz, S. Rein, W. Warta, J. Knobloch W. Wettling, On the degradation of Cz-Silicon solar cells, in: Proceedings of the 2nd WC-PVSEC, Vienna, Austria WIP, Munich, 1998 p. 1343.
4. Room-temperature method for minimizing light-induced degradation in crystalline silicon10.1063/1.4769809 ↗
5. A. Herguth, G. Schubert, M. Kaes and G. Hahn, A new approach to prevent the negative impact of the metastable defect in boron doped Cz silicon solar cells, in: Proceedings of the of the 32nd IEEE PVSC (4th WCPEC), Waikoloa, USA, 2006, p.940.10.1109/WCPEC.2006.279611 ↗
6. K. Bothe, J. Schmidt, R. Hezel, Effective reduction of the metastable defect concentration in boron-doped Czochralski silicon for solar cells, in: Proceedings of the 29th IEEE PVSC, New Orleans, LA IEEE, New York, 2002, p. 194.10.1109/PVSC.2002.1190489 ↗
7. Effective surface passivation of crystalline silicon using ultrathin Al2O3 films and Al2O3/SiNx stacks10.1002/pssr.200903272 ↗
8. Very low surface recombination velocities on p- and n-type c-Si by ultrafast spatial atomic layer deposition of aluminum oxide10.1063/1.3505311 ↗
9. Comparison of the thermal stability of single Al2O3 layers and Al2O3/SiNx stacks for the surface passiviation of silicon10.1016/j.egypro.2011.06.141 ↗
10. Improved parameterization of auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
11. Deactivation of the boron–oxygen recombination center in silicon by illumination at elevated temperature10.1002/pssr.200802009 ↗
12. Kinetics of the boron-oxygen related defect in theory and experiment10.1063/1.3517155 ↗
13. Light-induced boron-oxygen recombination centres in silicon: understanding their formation and elimination10.4028/www.scientific.net/SSP.205-206.3 ↗
14. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
15. Light-induced boron-oxygen defect generation in compensated p -type Czochralski silicon10.1063/1.3121208 ↗
16. Latent complexes of interstitial boron and oxygen dimers as a reason for degradation of silicon-based solar cells10.1063/1.3309869 ↗
17. Permanent recovery of electron lifetime in pre-annealed silicon samples: a model based on Ostwald ripening10.1063/1.4768688 ↗
18. Effect of rapid thermal annealing on recombination centres in boron-doped Czochralski-grown silicon10.1063/1.4863674 ↗
19. Investigations on the long time behavior of the metastable boron–oxygen complex in crystalline silicon10.1002/pip.779 ↗
20. Influence of hydrogen on the regeneration of boron–oxygen related defects in crystalline silicon10.1063/1.4804310 ↗