journal article·2020-12Open access

Investigation of light-induced degradation in N-Type silicon heterojunction solar cells during illuminated annealing at elevated temperatures

Chukwuka Madumelu, Brendan Wright, Anastasia Soeriyadi, Matthew Wright, Daniel Chen, Bram Hoex, Brett Hallam

Abstract

Abstract In this paper, we study a light-induced degradation (LID) mechanism observed in commercial n-type silicon heterojunction (SHJ) solar cells at elevated temperatures using dark- and illuminated annealing for a broad range of illumination intensities (1–40 kWm−2) at temperatures from 25 to 180 °C. Three key results are identified. Firstly, an increase in solar conversion efficiency (η) of up to 0.3% absolute is observed after 3 min of dark annealing at 160 °C, attributed to improved surface passivation and a reduction in series resistance. Secondly, a temperature-dependent light-induced degradation behaviour is observed at temperatures as low as 85 °C under 1-sun equivalent illumination, with increasing degradation extent and rate for increasing temperatures. At 160 °C, an average η loss of 0.5 ± 0.3% absolute is observed after only 5 min and exceeding 0.8% in some cells. Thirdly, a subsequent light intensity-dependent recovery occurs with continued illumination exposure. Under 1-sun illumination at 160 °C, a reduction in net η loss up to 0.05 ± 0.1% absolute is observed after 2 h. Increasing the illumination intensity to 40 kWm−2 accelerates the recovery and can result in a net η improvement of 0.2% absolute at 150 °C within 100 s. The results suggest that attempts to improve the efficiency of SHJ solar cells using illuminated annealing could be detrimental to cell performance if not carefully optimised. Further investigation is required to identify the exact nature of the underlying defect mechanism(s) and develop appropriate mitigation strategies on commercially suitable timescales.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. 24.7% record efficiency hit solar cell on thin silicon wafer10.1109/JPHOTOV.2013.2282737 ↗
2. Silicon heterojunction solar cell with interdigitated back contacts for a photoconversion efficiency over 26%10.1038/nenergy.2017.32 ↗
3. Temperature dependence of amorphous/crystalline silicon heterojunction solar cells
4. Demaurex · 2014
5. Silicon heterojunction solar cells: recent technological development and practical aspects - from lab to industry
6. N-type solar cells: advantages, issues, and current scenarios
7. Itrpv · 2019 · 1
8. Silicon heterojunction system field performance10.1109/JPHOTOV.2017.2765680 ↗
9. Degradation analysis of a-si, (hit) hetro-junction intrinsic thin layer silicon and m-c-si solar photovoltaic technologies under outdoor conditions10.1016/j.energy.2014.05.078 ↗
10. Damp heat induced degradation of silicon heterojunction solar cells with cu-plated contacts10.1109/JPHOTOV.2019.2941693 ↗
11. Effect of p-μc-si1-xox:h layer on performance of hetero-junction microcrystalline silicon solar cells under light concentration10.1016/j.cap.2011.08.011 ↗
12. Light-induced performance increase of silicon heterojunction solar cells
13. Increasing the efficiency of silicon heterojunction solar cells and modules by light soaking10.1016/j.solmat.2017.06.023 ↗
14. Light induced changes in the amorphous - crystalline silicon heterointerface10.1063/1.4821235 ↗
15. Very fast light-induced degradation of a-si:h/c-si(100) interfaces
16. Insights into the degradation of amorphous silicon passivation layer for heterojunction solar cells
17. Reversible conductivity changes indischarge-produced amorphous si
18. Fabrication of amorphous silicon carbide films using vhf-pecvd for triple-junction thin-film solar cell applications10.1016/j.solmat.2008.11.048 ↗
19. Hydrogenated amorphous silicon oxide solar cells fabricated near the phase transition between amorphous and microcrystalline structures10.1143/JJAP.48.122402 ↗
20. Staebler-wronski effect in hydrogenated amorphous silicon and related alloy films10.1143/JJAP.43.3257 ↗
21. Light-induced dangling bonds in hydrogenated amorphous silicon10.1063/1.92402 ↗
22. Light-induced metastable defects in hydrogenated amorphous silicon: a systematic study
23. The role of hydrogen in the staebler-wronski effect of a-si:h. Japanese10.1143/JJAP.24.L838 ↗
24. Dependence of letid on brick height for different wafer suppliers with several resistivities and dopants
25. A new mc-si degradation effect called letid
26. Light-induced degradation of pecvd aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
27. Ramspeck · 2012 · vol 53 · 1689
28. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
29. Investigation of letid where we can control it - application of fz silicon for defect studies10.1063/1.5123893 ↗
30. Evaluating root cause: the distinct roles of hydrogen and firing in activating light- a nd elevated temperature-induced degradation10.1063/1.5041756 ↗
31. Hydrogen-induced degradation
32. Evaluating the impact of sinx thickness on lifetime degradation in silicon10.1109/JPHOTOV.2019.2896671 ↗
33. Modulation of carrier-induced defect kinetics in multi-crystalline silicon perc cells through dark annealing10.1002/solr.201600028 ↗
34. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon perc modules
35. Rapid stabilization of high-performance multicrystalline p-type silicon perc cells
36. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
37. Does letid occur in c-si even without a firing step?10.1063/1.5123898 ↗
38. Stefani · 2020
39. Kinetics and dynamics of the regeneration of boron-oxygen defects incompensated n-type silicon
40. Series resistance effects on solar cell measurements10.1016/0365-1789(63)90063-8 ↗
41. Impact of carrier recombination on fill factor for large area heterojunctioncrystalline silicon solar cell with 25.1% efficiency
42. Advanced hydrogenation of dislocation clusters and boron-oxygen defects in silicon solar cells
43. Bhushan · 2011
44. Comprehensive simulation study of industrially relevant silicon solar cell architectures for an optimal material parameter choice10.1002/pip.2790 ↗
45. Stretched-exponential relaxation arising from dispersive diffusion of hydrogen in amorphous silicon
46. Studies of photodegradation in hydrogenated amorphous silicon
47. Stretched-exponential a-si:h/c-si interface recombination decay10.1063/1.2956668 ↗
48. Light induced changes in the amorphous-crystalline silicon heterointerface
49. Is light-induced degradation of a-si:h/c-si interfaces reversible?