Stress assisted oxidative failure of Inconel 601 for thermal energy storage

Madjid Sarvghad, Stuart Bell, Ralf Raud, Theodore A. Steinberg, Geoffrey Will

Publisher page

Abstract

Degradation of an Inconel 601 superalloy subjected to a eutectic mixture of carbonate salt at 450 °C was studied using advanced microscopy and microanalysis techniques. On the outside of the vessel, long term exposure to elevated temperature led to intergranular stress corrosion cracking via a stress assisted oxidation process. Elemental analysis verified diffusion controlled de-alloying of Ni and Cr from grain boundaries. Transmission electron microscopy showed that a (CrFeNiAl)3O4 oxide phase was formed at grain boundaries as a result of oxygen penetration. Intergranular cracking appeared due to the presence of residual stresses and microstructural heterogeneities facilitated the crack branching.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Chemical Looping and Thermochemical Processes · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. 1 - Introduction to concentrating solar power (CSP) technology
2. Gomez · 2011
3. High-temperature phase change materials for thermal energy storage10.1016/j.rser.2009.11.011 ↗
4. Thermal energy storage technologies and systems for concentrating solar power plants10.1016/j.pecs.2013.02.001 ↗
5. Lithium in thermal energy storage: a state-of-the-art review10.1016/j.rser.2014.10.096 ↗
6. 20 - High-Temperature Molten Salts for Solar Power Application
7. 2 - Fundamental principles of concentrating solar power (CSP) systems
8. Intergranular corrosion of high temperature alloys in molten fluoride salts10.3184/096034010X12743509428336 ↗
9. 12 - Corrosion in Molten Salts
10. Olson · 2009
11. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
12. 7 - Stress corrosion cracking (SCC) of nickel-based alloys
13. Environmentally assisted cracking of nickel alloys —a review
14. Numerical Simulation of the Simultaneous Precipitation of δ and γ′ Phases in the Ni-Base Superalloy ATI Allvac®718Plus™
15. Microstructure evolution during dynamic recrystallisation in polycrystalline nickel superalloys10.1016/j.msea.2015.03.121 ↗
16. The effect of structural evolution in INCONEL 601 on intergranular corrosion10.1016/S0254-0584(98)00149-7 ↗
17. Infrared brazing Inconel 601 and 422 stainless steel using the 70Au-22Ni-8Pd braze alloy10.1007/s10853-005-0446-9 ↗
18. Pitting characteristics of alloy 600 and alloy 601 in a chloride-containing acidic environment10.5006/1.3290372 ↗
19. Role of grain boundary carbides in cracking behavior of ni base alloys10.5516/NET.07.2012.013 ↗
20. Precipitation Reactions in Inconel Alloy 600 and Their Effect on Corrosion Behavior10.5006/0010-9312-32.10.401 ↗
21. The IGSCC, sensitization, and microstructure study of Alloys 600 and 69010.1016/0029-5493(93)90040-G ↗
22. Effects of grain boundary carbides on the mechanical properties of Inconel 60010.1016/S0254-0584(00)00484-3 ↗
23. Tensile deformation behavior and microstructure evolution of Ni-based superalloy 61710.1016/j.jnucmat.2014.08.003 ↗
24. Ground-state properties and relative stability between the L 1 2 and DO a phases of Ni 3 Al by Nb substitution10.1103/PhysRevB.53.1129 ↗
25. Influence of Portevin–Le Chatelier effect on rupture mode of alloy 718 specimens10.1016/j.jnucmat.2007.10.009 ↗
26. Oxidation induced intergranular cracking and Portevin–Le Chatelier effect in nickel base superalloy 71810.1016/S0921-5093(01)01224-2 ↗
27. Oxygen-induced intergranular cracking of a Ni-base alloy at elevated temperatures—an example of dynamic embrittlement10.1016/S1359-6454(01)00005-2 ↗
28. Surface enrichment and grain boundary segregation of niobium in inconel 718 single- and poly-crystals10.1016/0956-716X(94)90294-1 ↗
29. Environmental enhancement of creep crack growth in inconel 718 by oxygen and water vapor10.1016/0956-716X(94)90257-7 ↗
30. W. Carpenter, B. Kang, K. Chang, SAGBO Mechanism on high temperature cracking behavior of Ni-base Superalloys, Superalloys 718, 625, 706 and Various Derivatives, (1997) pp.679–688.
31. Oxidation assisted intergranular cracking under loading at dynamic strain aging temperatures in Inconel 718 superalloy10.1016/j.jallcom.2014.12.279 ↗
32. Tensile-hold effects on high-temperature fatigue-crack growth in nickel-based HASTELLOY® X alloy10.1016/j.msea.2006.06.069 ↗
33. The effect of grain-boundary-engineering-type processing on oxygen-induced cracking of IN71810.1016/S0921-5093(02)00753-0 ↗
34. Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM10.1016/j.corsci.2013.10.039 ↗
35. Thermodynamics of Corrosion: Pourbaix Diagrams
36. Microstructure and corrosion characterization of the interfacial region in dissimilar friction stir welded AA5083 to AA702310.1016/j.corsci.2016.02.027 ↗
37. 23 - Recovery and Recrystallization: phenomena, Physics, Models, Simulation
38. 1 - Mechanistic and fractographic aspects of stress-corrosion cracking (SCC)
39. The residual stress distribution in the wall of a deep-drawn and ironed cup determined experimentally and by FEM10.1016/S0007-8506(07)62206-9 ↗
40. A synchrotron study of residual stresses in a Al6022 deep drawn cup10.1016/j.msea.2003.08.059 ↗
41. Microfractographic aspects of stress corrosion cracking of Inconel 600 in a pressurized water reactor environment10.1016/0921-5093(94)90503-7 ↗
42. Gaune-Escard · 2012
43. The effect of sheet processing on the microstructure, tensile, and creep behavior of INCONEL alloy 71810.1007/s11661-006-0149-0 ↗
44. Relationship between ferromagnetic properties and grain size of Inconel alloy 60010.1016/j.jmmm.2014.12.041 ↗
45. X-ray spectrum and Mössbauer study of nickel ferrites excited by aluminum and chromium ions10.1007/BF00791810 ↗
46. Isothermal reduction kinetics at 900–1100°C of NiFe2O4 sintered at 1000–1200°C10.1016/j.jaap.2005.01.002 ↗
47. Preparation of composite nickel–iron oxide as highly reactive oxygen carrier for chemical-looping combustion process10.1016/j.jtice.2013.06.014 ↗
48. Hydrogen embrittlement of ultra high strength 300 grade maraging steel10.1016/j.corsci.2015.06.022 ↗
49. Hosford · 2010
50. J. Pokluda, Brittle and Ductile Fracture, in: Micromechanisms of Fracture and Fatigue, Springer London, 2010, pp. 69–123.10.1007/978-1-84996-266-7_3 ↗
51. The crystallography of stress corrosion cracking in face centered cubic single crystals10.1016/0010-938X(84)90123-9 ↗