journal article·2022-06

Effect of dynamic conditions on high-temperature corrosion of ternary carbonate salt for thermal energy storage applications

Luis González-Fernández, Mikel Intxaurtieta-Carcedo, Oleksandr Bondarchuk, Yaroslav Grosu

Publisher page

Abstract

Li 2CO 3–Na 2CO 3–K 2CO 3 salt is one of the candidates for 3 rd generation concentrated solar power (CSP) plants, aiming to increase the operational temperature. This rise of temperature significantly increases the corrosion issue of molten salts. However, there is a lack of studies focused on the effect of salt flow on the corrosion kinetic for this ternary carbonate salt. In this work, corrosion experiments under static and dynamic conditions are compared for SS310 subjected to ternary carbonate salt at 600 °C. A complete characterization of the corrosion layer, surface and cross-section, was carried out by means of SEM-EDX and XRD, while the molten salts after the corrosion tests were analysed by ICP-OES and XPS. The dynamic experiment exhibited an enlarged spallation of the corrosion layer, leading to a thinner and less homogeneous scale. This feature exposed the chromium containing phase and considerably increased the extent of its dissolution into the salt. The obtained results remark that the detrimental effect of dynamic conditions on the corrosivity of molten carbonate salt cannot be neglected and must be taken into account in the design of 3 rd generation CSP plants.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Solar Thermal and Photovoltaic Systems · Adsorption and Cooling Systems

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. A comprehensive review of state-of-the-art concentrating solar power (CSP) technologies: current status and research trends10.1016/j.rser.2018.04.097 ↗
2. Zarza-Moya · 2018
3. Solar power technology for electricity generation: a critical review10.1002/ese3.239 ↗
4. Kost · 2018
5. Review on concentrating solar power plants and new developments in high temperature thermal energy storage technologies10.1016/j.rser.2015.09.026 ↗
6. Policies to keep and expand the option of concentrating solar power for dispatchable renewable electricity10.1016/j.enpol.2018.02.014 ↗
7. Thermal energy storage: recent developments and practical aspects10.1016/j.pecs.2015.10.003 ↗
8. Mainstreaming commercial CSP systems: a technology review10.1016/j.renene.2019.03.049 ↗
9. Thermal convection loop study of the corrosion of incoloy 800 in molten NaNO3-KNO310.5006/1.3583131 ↗
10. Kruizenga · 2013
11. Kruizenga · 2013
12. High temperature molten salt corrosion behavior of aluminide and nickel-aluminide coatings for heat storage in concentrated solar power plants10.1016/j.surfcoat.2018.05.081 ↗
13. Impact of Solar Salt aging on corrosion of martensitic and austenitic steel for concentrating solar power plants10.1016/j.solmat.2019.110162 ↗
14. High-temperature corrosion performance of austenitic stainless steels type AISI 316L and AISI 321H, in molten Solar Salt10.1016/j.solener.2018.11.019 ↗
15. Molten salt corrosion mechanisms of nitrate based thermal energy storage materials for concentrated solar power plants: a review10.1016/j.solmat.2019.02.012 ↗
16. Concentrating solar power Gen3 demonstration roadmap
17. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review10.1007/s11705-018-1720-0 ↗
18. Molten chloride technology pathway to meet the U.S. DOE sunshot initiative with Gen3 CSP10.1063/1.5117601 ↗
19. Molten chloride salts for next generation CSP plants: electrolytical salt purification for reducing corrosive impurity level10.1016/j.solmat.2019.04.021 ↗
20. The thermal stability of molten lithium-sodium-potassium carbonate and the influence of additives on the melting point
21. Determination and evaluation of the thermophysical properties of an alkali carbonate eutectic molten salt10.1039/C5FD00236B ↗
22. A critical review of eutectic salt property prediction for latent heat energy storage systems10.1016/j.rser.2016.11.274 ↗
23. Carbonate molten salt solar thermal pilot facility: plant design, commissioning and operation up to 700 °C10.1016/j.renene.2019.11.045 ↗
24. Effects of temperature and partial pressure of CO2/O2 on corrosion behaviour of stainless-steel in molten Li/Na carbonate salt10.1016/S0378-7753(00)00376-1 ↗
25. The role of temperature on the corrosion and passivation of type 310S stainless steel in eutectic (LiþK) carbonate melt10.1016/j.jpowsour.2006.04.068 ↗
26. Corrosion behavior of Fe- Cr alloys in Li2CO3-K2CO3 molten carbonate10.1149/1.1955168 ↗
27. Corrosion resistance of HR3C to a carbonate molten salt for energy storage applications in CSP plants10.1016/j.solmat.2016.08.014 ↗
28. Corrosion of 304 stainless steel in carbonates melt– a state of enhanced dissolution of corrosion products10.1016/j.corsci.2020.108535 ↗
29. Corrosion evaluation of alumina-forming alloys in carbonate molten salt for CSP plants10.1016/j.renene.2019.03.087 ↗
30. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
31. Corrosion of steel alloys in eutectic NaCl + Na2CO3 at 700 °C and Li2CO3 + K2CO3 + Na2CO3 at 450 °C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
32. On the effect of cold-rolling on the corrosion of SS316L alloy in a molten carbonate salt10.1016/j.solmat.2019.110136 ↗
33. Comparative interaction of cold-worked versus annealed inconel 601 with molten carbonate salt at 450 °C10.1016/j.corsci.2017.01.004 ↗
34. Corrosion behavior of SS316L in ternary Li2CO3–Na2CO3–K2CO3 eutectic mixture salt for concentrated solar power plants10.1016/j.solmat.2020.110679 ↗
35. Nanofluids based on molten carbonate salts for high-temperature thermal energy storage: thermophysical properties, stability, compatibility and life cycle analysis10.1016/j.solmat.2020.110838 ↗
36. Inhibiting hot corrosion of molten Li2CO3-Na2CO3-K2CO3 salt through graphitization of construction materials for concentrated solar power10.1016/j.solmat.2020.110650 ↗
37. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
38. Compatibility of container materials for Concentrated Solar Power with a solar salt and alumina based nanofluid: a study under dynamic conditions10.1016/j.renene.2019.06.145 ↗
39. Experimental research of high temperature dynamic corrosion characteristic of stainless steels in nitrate eutectic molten salt10.1016/j.solener.2020.09.034 ↗
40. Investigation on static and dynamic corrosion behaviors of thermal energy transfer and storage system materials by molten salts in concentrating solar power plants10.1002/maco.201810362 ↗
41. Corrosion behavior research on austenitic stainless steel in dynamic molten salt
42. Dynamic corrosion testing of metals in solar salt for concentrated solar power10.1016/j.solmat.2021.111331 ↗
43. Dynamic corrosion test using LiNO3 containing molten salt for CSP applications10.3390/app10124305 ↗
44. Dynamic corrosion behavior of 316L stainless steel in quaternary nitrate-nitrite salts under different flow rates10.1016/j.solmat.2020.110821 ↗
45. High temperature corrosion beneath carbonate melts of aluminide coatings for CSP application10.1016/j.solmat.2020.110514 ↗
46. An improved technique for molten salt corrosion sample preparation10.1016/j.solmat.2021.111057 ↗