Improving the corrosion resistance of ferritic-martensitic steels at 600 °C in molten solar salt via diffusion coatings
Source abstract
Abstract
Abstract Molten salt corrosion in the receiver's piping system and storage tanks is still one of the major drawbacks of concentrated solar power (CSP) plants and is currently covered by using expensive high-alloyed steels or Ni-base alloys. The employment of cheaper structural materials combined with protective coatings is an attractive alternative to increase cost-efficiency. The present study investigates the corrosion resistance of three different coatings (a pure Ni, a Cr and a combined Ni + Cr coating) deposited on ferritic-martensitic X20CrMoV12-1 steel during isothermal immersion in molten solar salt in comparison to uncoated Ni-base alloy Haynes 230. Exposure tests were conducted at 600 °C for up to 1000 h. To identify the individual role of the main elements, exposure tests of pure Fe, Ni and Cr were undertaken as well. In addition to the cross-sectional investigations via light-optical microscopy and EPMA, X-ray diffraction measurements were conducted to identify the corrosion products. These were complemented by weight change measurements and chemical analysis of the salts after the exposure tests. The study reveals differences between the corrosion behaviour of the different coating approaches, which is discussed as a function of coating composition and degradation mechanisms. Whereas pure Cr or pure Ni coatings offer hardly any improved protection of the uncoated X20CrMoV12-1 substrate, the combined Ni + Cr coating performs very well and improves the scaling behaviour of X20CrMoV12-1 significantly. The outcome highlights the correlation between the solubility of the pure metals Fe, Ni and Cr in molten solar salt and the corrosion resistance of the investigated coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solar Thermal and Photovoltaic Systems · Phase Change Materials Research · Heat Transfer Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (77)
Show source-provided references
1. Review of commercial thermal energy storage in concentrated solar power plants: steam vs. molten salts10.1016/j.rser.2017.05.084 ↗
2. Advanced heat transfer fluids for direct molten salt line-focusing CSP plants10.1016/j.pecs.2018.02.002 ↗
3. Power cycles integration in concentrated solar power plants with energy storage based on calcium looping10.1016/j.enconman.2017.03.029 ↗
4. Future directions in the field of high-temperature corrosion research10.1007/s11085-017-9719-3 ↗
5. Comprehensive comparison of efficiency and CO2 emissions between biomass energy conversion technologies—position of supercritical water gasification in biomass technologies10.1016/S0961-9534(03)00016-3 ↗
6. Concentrating solar power technology: present status and outlook10.1515/nleng-2017-0171 ↗
7. An overview of drivers and barriers to concentrated solar power in the European Union10.1016/j.rser.2017.06.038 ↗
8. Carbon emission and mitigation cost comparisons between fossil fuels, nuclear and renewable energy resources for electricity generation10.1016/S0301-4215(02)00192-1 ↗
9. Durability of solar absorber coatings and their cost-effectiveness10.1016/j.solmat.2017.03.010 ↗
10. Solar selective coatings for concentrating solar power central receivers
11. Accelerated aging of absorber coatings for CSP receivers under real high solar flux - evolution of their optical properties10.1016/j.solmat.2018.12.030 ↗
12. Heat transfer fluids for concentrating solar power systems: a review10.1016/j.apenergy.2015.01.125 ↗
13. Molten salt power towers operating at 600–650 °C: salt selection and cost benefits10.1016/j.solener.2018.01.063 ↗
14. Mehos · 2017
15. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
16. Impact of Solar Salt aging on corrosion of martensitic and austenitic steel for concentrating solar power plants10.1016/j.solmat.2019.110162 ↗
17. Nitrate/nitrite chemistry in sodium nitrate-potassium nitrate melts10.1021/ic00147a004 ↗
18. A review of the chemical and physical properties of molten alkali nitrate salts and their effect on materials used for solar central receivers
19. High temperature corrosion beneath nitrate melts10.1002/maco.201307076 ↗
20. Corrosion behavior of structural materials for potential use in nitrate salts based solar thermal power plants10.1149/2.0501708jes ↗
21. High chromium martensitic steels - microstructure, properties and potential for further development
22. Microstructure control for high strength 9Cr ferritic–martensitic steels10.1016/j.jnucmat.2011.12.011 ↗
23. Creep and corrosion testing of aluminide coatings on ferritic–martensitic substrates10.1016/j.surfcoat.2006.07.258 ↗
24. Effect of tungsten on primary creep deformation and minimum creep rate of reduced activation ferritic-martensitic steel10.1007/s11661-014-2472-1 ↗
25. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600°C10.1016/j.solmat.2015.08.011 ↗
26. Review of the solubility, monitoring, and purification of impurities in molten salts for energy storage in concentrated solar power plants10.1016/j.rser.2020.110006 ↗
27. Solar Salt - pushing an old material for energy storage to a new limit10.1016/j.apenergy.2020.114535 ↗
28. Graphitization as efficient inhibitor of the carbon steel corrosion by molten binary nitrate salt for thermal energy storage at concentrated solar power10.1016/j.solmat.2019.110172 ↗
29. Protective coatings for high temperature molten salt heat storage systems in solar concentration power Plants10.1063/1.5067095 ↗
30. High temperature molten salt corrosion behavior of aluminide and nickel-aluminide coatings for heat storage in concentrated solar power plants10.1016/j.surfcoat.2018.05.081 ↗
31. scale formation and degradation of diffusion coatings deposited on 9% Cr steel in molten solar salt10.3390/coatings9100687 ↗
32. Slurry aluminizing: a solution for molten nitrate salt corrosion in concentrated solar power plants10.1016/j.solmat.2015.11.024 ↗
33. P.F. Tortorelli, P.S. Bishop, J.R. DiStefano, Selection of Corrosion-Resistant Materials for Use in Molten Nitrate Salts, Oak Ridge National Lab., TN (USA).
34. Room-temperature mechanical behavior of FeAl: effects of stoichiometry, environment, and boron addition10.1016/S1359-6454(98)00254-7 ↗
35. Thermal expansion of binary CoAl, FeAl and NiAl alloys
36. Touloukian · 1970
37. Innovative heat treatment and novel non-harmful slurries for "in situ" aluminization or Co-deposition of elements on steels for corrosion protection at high temperatures
38. Creep behavior of pack cementation aluminide coatings on Grade 91 ferritic–martensitic alloy10.1016/j.surfcoat.2013.12.008 ↗
39. Steam oxidation and mechanical performance of a ferritic–martensitic steel with slurry aluminide coating10.1002/maco.202011554 ↗
40. Corrosion in molten nitrate-nitrite salts
41. The hot corrosion of metals by molten salts
42. Protective coatings for high temperature materials: chemical vapour deposition and pack cementation processes
43. Protective coatings for high temperature alloys: state of technology
44. Pack cementation processes10.1179/mst.1986.2.3.201 ↗
45. ISO 17245: Corrosion of Metals and Alloys - Test Method for High Temperature Corrosion Testing of Metallic Materials by Immersing in Molten Salt or Other Liquids under Static Conditions, ISO TC156 WG 13 (High Temperature Corrosion).
46. Influence of different atmospheres on molten salt chemistry and its effect on steel corrosion
47. On the formation of carbide coatings by chromizing carbon steels10.1007/BF02649834 ↗
48. Cr diffusion coatings on a ferritic-martensitic steel for corrosion protection in KCl-rich biomass co-firing environments10.1016/j.corsci.2019.108343 ↗
49. High-temperature stability of nitrate/nitrite molten salt mixtures under different atmospheres10.1016/j.apenergy.2018.05.101 ↗
50. Molten lithium-potassium nitrate eutectic: the reactions of some compounds of chromium10.1016/S0020-1693(00)93183-9 ↗
51. Molten sodium nitrite-potassium nitrite eutectic: the reactions of some compounds of chromium10.1016/S0020-1693(00)92574-X ↗
52. Bradshaw · 2001
53. Chemistry and electrochemistry of hot corrosion of metals
54. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
55. Standard electrode potentials in molten chlorides10.1016/0013-4686(68)85016-9 ↗
56. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part I: NaCl–KCl binary system10.1016/j.solmat.2020.110659 ↗
57. Corrosion testing of diffusion-coated steel in molten salt for concentrated solar power tower systems10.1016/j.surfcoat.2018.08.097 ↗
58. Molten nitrate salts at 600 and 680°C: thermophysical property changes and corrosion of high-temperature nickel alloys10.1016/j.solener.2014.01.028 ↗
59. Hot corrosion behavior of Inconel 625 superalloy in eutectic molten nitrate salts10.1007/s11085-017-9830-5 ↗
60. A. Solimani, T.M. Meißner, C. Oskay, M.C. Galetz, Electroless Ni-P Coatings on Low-Cr Steels: A Cost-Efficient Solution for Solar Thermal Applications?, Submitted to: Solar Energy Materials and Solar Cells 09/2020.10.1016/j.solmat.2021.111312 ↗
61. Aging behaviour of 25Cr-17Mn high nitrogen duplex stainless steel10.2355/isijinternational.40.719 ↗
62. Martensitic–austenitic 9–12% Cr steels—alloy design, microstructural stability and mechanical properties10.1016/j.msea.2007.04.093 ↗
63. Characterization of sodium nitrate as phase change material10.1007/s10765-011-1113-9 ↗
64. The kinetics of the thermal decomposition of potassium nitrate and of the reaction between potassium nitrite and oxygen 1a10.1021/ja01561a015 ↗
65. Equilibrium in melts of the nitrates and nitrites of sodium potassium
66. Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
67. Fähsing · 2016
68. Inhibiting hot corrosion of molten Li2CO3-Na2CO3-K2CO3 salt through graphitization of construction materials for concentrated solar power10.1016/j.solmat.2020.110650 ↗
69. Molten salt corrosion of stainless steels and low-Cr steel in CSP plants10.1007/s11085-012-9310-x ↗
70. The effect of NaCl addition on the corrosion of mild steel in NaNO3 melt10.1016/0010-938X(93)90045-I ↗
71. Oxidation behavior of electroless Ni–P, Ni–B and Ni–W–B coatings deposited on steel substrates10.1016/j.surfcoat.2015.01.064 ↗
72. High-temperature oxidation of iron covered by electroless Ni-P coating: a GDOS depth profiling study10.1002/sia.740180910 ↗
73. Oxidation of Ni films electroplated on steel10.1007/BF03027489 ↗
74. Interdiffusion of the electroless Ni-P deposit with the steel substrate10.1149/1.2086702 ↗
75. Bürgel · 2011
76. Galvanic corrosion of pure metals in molten fluorides10.1016/j.jfluchem.2014.05.010 ↗
77. Constitution diagram for stainless steel weld metal