Corrosion behavior of SS316L in ternary Li2CO3–Na2CO3–K2CO3 eutectic mixture salt for concentrated solar power plants
Source abstract
Abstract
Abstract This paper elaborates the compatibility of SS316L alloy with LiNaK carbonate for concentrated solar power plant applications. In this study, corrosion behavior and corrosion mechanism of SS316L in the eutectic LiNaK carbonate molten salt, at 600 °C and 700 °C, were investigated in detail. The results revealed that the corrosion process of stainless steel 316L in the LiNaK carbonate molten salt is mainly divided into four successive steps: (i) selective oxidation process of metals → (ii) lithiation reaction of the oxide → (iii) formation of a dual-structured corrosion scale → (iv) separation and spalling of corrosion products. Moreover, increasing temperature to 700 °C results in a severe corrosion of SS316L in the molten carbonate salt. Therefore, it is imperative to explore a suitable protective coating for SS316L to use it as a structural material in concentrated solar power plant.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Phase Change Materials Research · Solar Thermal and Photovoltaic Systems · Solar Energy Systems and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Prospects and problems of concentrating solar power technologies for power generation in the desert regions10.1016/j.rser.2015.09.015 ↗
2. Comparative environmental assessment of two materials suited to central tower CSP technology10.1016/j.solener.2018.01.036 ↗
3. A comprehensive review of state-of-the-art concentrating solar power (CSP) technologies: current status and research trends10.1016/j.rser.2018.04.097 ↗
4. Solar power technology for electricity generation: a critical review10.1002/ese3.239 ↗
5. Review on concentrating solar power plants and new developments in high temperature thermal energy storage technologies10.1016/j.rser.2015.09.026 ↗
6. Advanced heat transfer fluids for direct molten salt line-focusing CSP plants10.1016/j.pecs.2018.02.002 ↗
7. Concentrating solar power Gen3 demonstration roadmap
8. Heat transfer fluids for concentrating solar power systems – a review10.1016/j.apenergy.2015.01.125 ↗
9. Protective coatings for high temperature molten salt heat storage systems in solar concentration power plants
10. Thermal energy storage using chloride salts and their eutectics10.1016/j.applthermaleng.2016.07.046 ↗
11. Experimental study on optimized composition of mixed carbonate salt for sensible heat storage in solar thermal power plant10.1016/j.solener.2011.05.004 ↗
12. Experimental verification of theoretically estimated composition and enthalpy of fusion of eutectic salt mixtures10.1016/j.solmat.2017.09.033 ↗
13. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
14. Sensible energy storage options for concentrating solar power plants operating above 600 degrees C10.1016/j.rser.2019.01.062 ↗
15. HIGH-TEMPERATURE heat content and related properties for LI2CO3, NA2CO3, K2CO3, and ternary eutectic mixture10.1039/tf9635900841 ↗
16. A critical review of eutectic salt property prediction for latent heat energy storage systems10.1016/j.rser.2016.11.274 ↗
17. Review on storage materials and thermal performance enhancement techniques for high temperature phase change thermal storage systems10.1016/j.rser.2012.01.020 ↗
18. The thermal stability of molten lithium-sodium-potassium carbonate and the influence of additives on the melting point10.1115/1.4006895 ↗
19. Technical challenges and opportunities for concentrating solar power with thermal energy storage
20. Bradshaw · 2010
21. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
22. Corrosion of stainless steels and low-Cr steel in molten Ca(NO3)(2)-NaNO3-KNO3 eutectic salt for direct energy storage in CSP plants10.1016/j.solmat.2015.05.004 ↗
23. Molten salt corrosion of stainless steels and low-Cr steel in CSP plants10.1007/s11085-012-9310-x ↗
24. Corrosion of alumina-forming austenitic steel in molten nitrate salts by gravimetric analysis and impedance spectroscopy10.1002/maco.201307422 ↗
25. High-temperature and corrosion behavior of nitrate nitrite molten salt mixtures regarding their application in concentrating solar power plants
26. Molten nitrate salts at 600 and 680 degrees C: thermophysical property changes and corrosion of high-temperature nickel alloys10.1016/j.solener.2014.01.028 ↗
27. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 degrees C10.1016/j.solmat.2015.08.011 ↗
28. Corrosion behavior of Incoloy 800 in molten nitrate salt
29. Electrochemical performance of Ni20Cr coatings applied by combustion powder spray in ZnCl2-KCl molten salts10.1016/S1452-3981(23)13401-8 ↗
30. Molten chloride salts for next generation concentrated solar power plants: mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
31. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
32. Corrosion of selected alloys in eutectic lithium-sodium-potassium carbonate at 900C
33. Corrosion behavior of Fe-Cr alloys in Li2CO3-K2CO3 molten carbonate10.1149/1.1955168 ↗
34. Corrosion resistance of HR3C to a carbonate molten salt for energy storage applications in CSP plants10.1016/j.solmat.2016.08.014 ↗
35. Corrosion evaluation of alumina-forming alloys in carbonate molten salt for CSP plants10.1016/j.renene.2019.03.087 ↗
36. On the effect of cold-rolling on the corrosion of SS316L alloy in a molten carbonate salt
37. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
38. Comparative interaction of cold-worked versus annealed inconel 601 with molten carbonate salt at 450 degrees C10.1016/j.corsci.2017.01.004 ↗
39. Stress assisted oxidative failure of Inconel 601 for thermal energy storage10.1016/j.solmat.2016.10.008 ↗
40. Effects of temperature and partial pressure of CO2/O-2 on corrosion behaviour of stainless-steel in molten Li/Na carbonate salt10.1016/S0378-7753(00)00376-1 ↗
41. The role of temperature on the corrosion and passivation of type 310S stainless steel in eutectic (Li+K) carbonate melt10.1016/j.jpowsour.2006.04.068 ↗
42. A simple method for the inhibition of the corrosion of carbon steel by molten nitrate salt for thermal storage in concentrating solar power applications
43. Corrosion evaluation of alloys and MCrAlX coatings in molten carbonates for thermal solar applications10.1016/j.solmat.2016.07.029 ↗
44. Corrosion resistance of protective coatings against molten nitrate salts for thermal energy storage and their environmental impact in CSP technology10.1016/j.solener.2018.10.083 ↗
45. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
46. Corrosion of steel alloys in eutectic NaCl + Na2CO3 at 700 C-omicron and Li2CO3 + K2CO3 + Na2CO3 at 450 C-omicron for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
47. Corrosion of alloys in high temperature molten-salt heat transfer fluids with air as the cover gas10.1016/j.solener.2019.09.015 ↗
48. Hot corrosion of different alloys in chloride and carbonate molten-salt mixtures under argon atmosphere10.1016/j.solener.2019.07.065 ↗
49. High-temperature phase change materials for thermal energy storage10.1016/j.rser.2009.11.011 ↗
50. A comparative study of the corrosion behavior of three stainless steels in an eutectic (Li,Na,K)(2)CO3 melt with and without (Na,K)Cl additives at 973K in air10.1515/htmp.2011.024 ↗
51. 2CRO4 IN molten alkali carbonates at 650-DEGREES-C10.1149/1.2100840 ↗
52. Corrosion monitoring and mitigation techniques on advanced thermal energy storage materials for CSP plants10.1016/j.solmat.2018.12.028 ↗
53. Acids" and "bases" in molten mass. The determination of oxygen ions concentrations10.1002/bbpc.19390450405 ↗
54. The acidic and basic properties OF oxides10.3891/acta.chem.scand.01-0592 ↗
55. The solubility and electrochemistry OF alkali-metal oxides IN the molten eutectic mixture OF lithium-carbonate sodium-carbonate potassium carbonate10.1007/BF01007939 ↗
56. Lide · 2004
57. Electrochemistry OF molten-salt corrosion10.1016/0921-5093(91)90265-O ↗
58. Corrosion behavior of AISI 316L stainless steel and ODS FeAl aluminide in eutectic Li2CO3-K2CO3 molten carbonates under flowing CO2-O-2 gas mixtures10.1023/A:1004538931676 ↗
59. High temperature corrosion of low and high alloy steels under molten carbonate fuel cell conditions10.1002/maco.19970480803 ↗
60. The corrosion behavior of Fe‐Cr alloys containing Co, Mn, and/or Ni and of a Co‐base alloy in the presence of molten (Li, K)‐carbonate10.1002/maco.19970481103 ↗