Abstract

Two important aspects for the success of the porous silicon-based layer transfer method in producing kerfless thin (<50 µm) silicon foils for future silicon solar modules are addressed in this work: achieving high detachment yield and high minority carrier diffusion lengths. The detachment characteristics of the porous silicon-based lift-off process is studied using finite element modeling as well as experiments. It is shown that for easy detachment and high detachment yield, a low density of thin silicon pillars must be attained in the high porosity detachment layer (HP-DL) after high temperature sintering. This is elegantly achieved by increasing the thickness of the low porosity template layer (LP-TL) which acts as the vacancy supply to increase the post-anneal porosity of the HP-DL. In this way, near 100% detachment yield has been achieved. However, a thicker LP-TL results in a poorer quality epitaxial growth surface. To circumvent this trade-off, novel triple and quadruple layer porous silicon stacks are introduced which decouple the function of the LP-TL that acts as both the template for epitaxy and as the vacancy supply for the HP-DL. In these new stacks, a surface zone of very low void size and density (nearly void-free) is created which allows high quality epitaxy on easily-detachable porous silicon stacks. Minority carrier lifetime measurements on epitaxial foils grown on such a triple layer stack has resulted in an effective lifetime of ~350 µs at the injection level of 10 15 cm −3 which corresponds to a minimum minority carrier diffusion length of ~670 µm (> 16 times the silicon thickness). With such high quality epitaxial foils combined with high detachment yield, very high efficiency solar devices on thin silicon substrates would be a reality in the near future.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence · Nanowire Synthesis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. SEMI, International Technology Roadmap for Photovoltaic ( ITRPV ) results 2012. 〈http://www.itrpv.net〉, 2013.
2. H. Tayanaka, K. Yamauchi, T. Matsushita, Thin-film crystalline silicon solar cells obtained by separation of a porous silicon sacrificial layer, in: 2nd World Conference and Exhibition on Photovoltaic Solar Energy Conversion, 6–10 July, Vienna, Austria, 1998, 1272–1277.
3. Review of layer transfer processes for crystalline thin-film silicon solar cells10.1143/JJAP.40.4431 ↗
4. 19%-efficient and 43 µm-thick crystalline Si solar cell from layer transfer using porous silicon10.1002/pip.1129 ↗
5. M. Moslehi, World-record 20%+efficiency 156 mm × 156 mm full square solar cells using low-cost kerfless ultrathin epitaxial silicon and porous silicon lift-off technology for industry-leading high performance smart PV modules, in: PV Asia Pacific Conference, Singapore, 2012.
6. Ravi · 2011
7. A. Lochtefeld, L. Wang, M. Carroll, J. Han, D. Stryker, S. Bengtson, et al., 15%, 20 μm Thin, Silicon Solar Cells on Steel, in: Proceedings of the 39th IEEE Photovoltaic Specialists Conference, 2013. 10.1002/pip.2221 (accessed 10.01.14).10.1002/pip.2221 ↗
8. Structural changes in porous silicon during annealing10.1002/pssa.200306474 ↗
9. K. Van Nieuwenhuysen, V. Depauw, R. Martini, J. Govaerts, M. Debucquoy, H. Sivaramakrishnan Radhakrishnan, et al., High quality epitaxial foils, obtained by a porous silicon based layer transfer process, for integration in back contacted solar cells, in: 27th European Photovoltaic Solar Energy Conference and Exhibition, 2012: 2471–2474.10.1109/PVSC.2012.6317950 ↗
10. Improving the quality of epitaxial foils produced using a porous silicon-based layer transfer process for high-efficiency thin-film crystalline silicon solar cells10.1109/JPHOTOV.2013.2282740 ↗
11. N. Ott, M. Nerding, G. Mu¨ller, R. Brendel, H.P. Strunk, Evolution of the microstructure during annealing of porous silicon multilayers, J. Appl. Phys. 95 (2004) 497–503. 〈http://link.aip.org/link/?JAP/95/497/1&Agg=doi〉, (accessed 27.09.13).10.1063/1.1633657 ↗
12. Lift-off of free-standing layers in the Kerfless porous silicon process10.1016/j.egypro.2013.07.365 ↗
13. H. Sivaramakrishnan Radhakrishnan, M. Debucquoy, F. Korsós, K. Van Nieuwenhuysen, V. Depauw, I. Gordon, et al., Lifetime measurements on attached epilayers and detached epifoils grown on reorganised porous silicon showing a bulk lifetime exceeding 100μs, Energ. Procedia. 38 (2013) 950–958. 10.1016/j.egypro.2013.07.369.10.1016/j.egypro.2013.07.369 ↗
14. Layer transfer process assisted by laser scribing for thin film solar cells based on epitaxial foils, Phys10.1002/pssa.201200955 ↗
15. Plasma–silicone interaction during a-Si:H deposition on solar cell wafers bonded to glass10.1016/j.solmat.2014.01.035 ↗
16. Qualification of encapsulation materials for module-level-processing10.1016/j.solmat.2013.06.012 ↗
17. Development of a-Si:H/c-Si heterojunctions for the i2-module concept: low-temperature passivation and emitter formation on wafers bonded to glass10.1016/j.solmat.2013.01.029 ↗
18. R.A. Sinton, A. Cuevas, M. Stuckings, Quasi-steady-state photoconductance, a new method for solar cell material and device characterization, in: Conference Rec. 25th IEEE Photovoltaic Specialists Conference, IEEE, Washington D.C., USA, 1996, 457–460. doi:10.1109/PVSC.1996.564042.10.1109/PVSC.1996.564042 ↗
19. K.R. McIntosh, J.N. Cotsell, J.S. Cumpston, A.W. Norris, N.E. Powell, B.M. Ketola, An optical comparison of silicone and EVA encapsulants for conventional silicon PV modules: A ray-tracing study, in: 34th IEEE Photovoltaic Specialists Conference IEEE, Philadelphia, Pennsylvania, USA, n.d. 000544–000549. doi:10.1109/PVSC.2009.5411624.10.1109/PVSC.2009.5411624 ↗
20. In situ study of size and temperature dependent brittle-to-ductile transition in single crystal silicon10.1002/adfm.201201992 ↗
21. Brittle-to-ductile transition in uniaxial compression of silicon pillars at room temperature10.1002/adfm.200900418 ↗
22. Evaluation of size effect on mechanical properties of single crystal silicon by nanoscale bending test using AFM10.1109/84.896765 ↗
23. Measurement of the bending strength of vapor-liquid-solid grown silicon nanowires10.1021/nl052223z ↗
24. P. Ferret, Size effects in mechanical deformation and fracture of cantilevered silicon nanowires10.1021/nl802556d ↗
25. Development of AFM-based techniques to measure mechanical properties of nanoscale structures10.1016/S0924-4247(02)00268-6 ↗
26. Size and temperature effects on the fracture mechanisms of silicon nanowires: molecular dynamics simulations10.1016/j.ijplas.2010.02.001 ↗
27. Low-temperature in situ large-strain plasticity of silicon nanowires10.1002/adma.200602705 ↗
28. Mechanical properties of vapor-liquid-solid synthesized silicon nanowires10.1021/nl902132w ↗
29. The brittle–ductile transition in Silicon. I. Experiments10.1098/rspa.1989.0001 ↗
30. Mechanical properties of Si nanowires as revealed by in situ transmission electron microscopy and molecular dynamics simulations10.1021/nl204282y ↗
31. Fracture toughness of silicon
32. L. James, W. Mills, Review and synthesis of stress intensity factor solutions applicable to cracks in bolts, Eng. Fract. Mech. 30 (1988) 641–654. 〈http://www.sciencedirect.com/science/article/pii/0013794488901567〉, (accessed 28.07.14).10.1016/0013-7944(88)90156-7 ↗
33. Stress intensity factor solutions for a cracked bolt under tension, bending and residual stress loading10.1016/0013-7944(91)90050-B ↗
34. Erosion evolution in mono-crystalline silicon surfaces caused by acoustic cavitation bubbles10.1063/1.4791582 ↗
35. Nucleation threshold and deactivation mechanisms of nanoscopic cavitation nuclei10.1063/1.3249602 ↗
36. Disruptive bubble behaviour leading to microstructure damage in an ultrasonic field10.1017/jfm.2014.267 ↗
37. Heat treatment effect on porous silicon10.1016/0040-6090(86)90200-2 ↗
38. Sensitivity of state-of-the-art and high efficiency crystalline silicon solar cells to metal impurities10.1002/pip.2195 ↗
39. Effective lifetimes exceeding 300 μs in gettered p-type epitaxial kerfless silicon for photovoltaics10.1063/1.4844915 ↗