journal article·2019-12

Graphitization as efficient inhibitor of the carbon steel corrosion by molten binary nitrate salt for thermal energy storage at concentrated solar power

Mikel Gonzalez, Udayashankar Nithiyanantham, Enrique Carbó-Argibay, Oleksandr Bondarchuk, Yaroslav Grosu, Abdessamad Faik

Publisher page

Abstract

Abstract Hot corrosion by molten salts has detrimental effect on various industrial and infrastructural systems particularly on the Concentrated Solar Power (CSP) plants. To enhance durability of the CSP plants′ components, while decreasing the production cost of electricity, the graphitization anticorrosion method for carbon steel in contact with molten binary nitrate salt is proposed in this work. To shed some light on the corrosion mechanisms and quantify corrosion rates a combination of advanced material characterization techniques like Focused Ion Beam, SEM, EDX, XPS depth profiling, XRD was applied. It has been demonstrated that the surface spray-coating by graphite reduces the corrosion rate at least by factor of 6 and stabilizes the corrosion scale by iron carbide crystals at 390 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solar Thermal and Photovoltaic Systems · Phase Change Materials Research · Radiative Heat Transfer Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Zarza-Moya · 2018
2. Thermal energy storage: recent developments and practical aspects10.1016/j.pecs.2015.10.003 ↗
3. Policies to keep and expand the option of concentrating solar power for dispatchable renewable electricity10.1016/j.enpol.2018.02.014 ↗
4. Thermal energy storage technologies and systems for concentrating solar power plants10.1016/j.pecs.2013.02.001 ↗
5. System-level performance optimization of molten-salt packed-bed thermal energy storage for concentrating solar power10.1016/j.apenergy.2018.05.081 ↗
6. A versatile one-dimensional numerical model for packed-bed heat storage systems10.1016/j.renene.2018.10.012 ↗
7. Two-tank molten salts thermal energy storage system for solar power plants at pilot plant scale: lessons learnt and recommendations for its design, start-up and operation10.1016/j.renene.2018.01.026 ↗
8. Dynamic simulation of two-tank indirect thermal energy storage system with molten salt10.1016/j.renene.2017.06.024 ↗
9. Parametric simulation and economic estimation of thermal energy storage in solar power tower
10. A comprehensive review of state-of-the-art concentrating solar power (CSP) technologies: current status and research trends10.1016/j.rser.2018.04.097 ↗
11. Corrosion of stainless steels and low-Cr steel in molten Ca(NO3)2–NaNO3–KNO3 eutectic salt for direct energy storage in CSP plants10.1016/j.solmat.2015.05.004 ↗
12. High-temperature and corrosion behavior of nitrate nitrite molten salt mixtures regarding their application in concentrating solar power plants10.1016/j.egypro.2015.03.071 ↗
13. High temperature corrosion in molten solar salt: the role of chloride impurities
14. Corrosion behavior and mechanism of austenitic stainless steels in a new quaternary molten salt for concentrating solar power10.1016/j.solmat.2019.01.024 ↗
15. Corrosion testing device for in-situ corrosion characterization in operational molten salts storage tanks: a516 Gr70 carbon steel performance under molten salts exposure10.1016/j.solmat.2016.06.005 ↗
16. High-temperature corrosion of Cr-Mo steel in molten LiNO3-NaNO3-KNO3 eutectic salt for thermal energy storage10.1016/j.solmat.2014.10.007 ↗
17. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗
18. Investigation on static and dynamic corrosion behaviors of thermal energy transfer and storage system materials by molten salts in concentrating solar power plants10.1002/maco.201810362 ↗
19. Electrochemical impedance spectroscopy (EIS): an efficient technique for monitoring corrosion processes in molten salt environments in CSP applications10.1016/j.solmat.2018.11.007 ↗
20. High-temperature corrosion performance of austenitic stainless steels type AISI 316L and AISI 321H, in molten Solar Salt10.1016/j.solener.2018.11.019 ↗
21. Corrosion in molten nitrate-nitrite salts
22. Corrosion monitoring of ferritic-martensitic steels in molten salt environments for CSP applications10.1063/1.5117552 ↗
23. Corrosion resistance of HR3C to a carbonate molten salt for energy storage applications in CSP plants10.1016/j.solmat.2016.08.014 ↗
24. The effect of humidity, impurities and initial state on the corrosion of carbon and stainless steels in molten HitecXL salt for CSP application10.1016/j.solmat.2017.08.026 ↗
25. A.M. Kruizenga, D.D. Gill, M.E. LaFord, G. McConohy, reportCorrosion of High Temperature Alloys in Solar Salt at 400, 500, and 680oC, SANDIA REPORT, SAND 2013-8256 California 2013.10.2172/1104752 ↗
26. Electrochemical study on the corrosion behaviors of 316 SS in HITEC molten salt at different temperatures10.1016/j.solmat.2018.06.044 ↗
27. Unexpected effect of nanoparticles doping on the corrosivity of molten nitrate salt for thermal energy storage10.1016/j.solmat.2018.01.002 ↗
28. High temperature corrosion behavior on molten nitrate salt-based nanofluids for CSP plants10.1016/j.renene.2018.07.018 ↗
29. Protective coatings for high temperature molten salt heat storage systems in solar concentration power plants
30. A simple method for the inhibition of the corrosion of carbon steel by molten nitrate salt for thermal storage in concentrating solar power applications10.1038/s41529-018-0055-0 ↗
31. Corrosion resistance of protective coatings against molten nitrate salts for thermal energy storage and their environmental impact in CSP technology10.1016/j.solener.2018.10.083 ↗
32. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
33. Molten salt corrosion mechanisms of nitrate based thermal energy storage materials for concentrated solar power plants: a review10.1016/j.solmat.2019.02.012 ↗
34. Thermo-economic analysis of high-temperature sensible thermal storage with different ternary eutectic alkali and alkaline earth metal chlorides10.1016/j.solener.2018.10.008 ↗
35. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
36. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
37. Corrosion behavior of Ni-based alloys in molten NaCl-CaCl2-MgCl2 eutectic salt for concentrating solar power10.1016/j.solmat.2017.05.050 ↗
38. Electrochemical measurement of corrosive impurities in molten chlorides for thermal energy storage10.1016/j.est.2017.12.007 ↗
39. Corrosion resistance of Hastelloys in molten metal-chloride heat-transfer fluids for concentrating solar power applications10.1016/j.solener.2014.02.002 ↗
40. Vapor pressure and corrosivity of ternary metal-chloride molten-salt based heat transfer fluids for use in concentrating solar power systems10.1016/j.apenergy.2015.08.131 ↗
41. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
42. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
43. Electrochemical performance of Ni20Cr coatings applied by combustion powder spry in ZnCl2-KCl molten salts10.1016/S1452-3981(23)13401-8 ↗
44. Dimensionless analysis for predicting Fe-Ni-Cr alloy corrosion in molten salt systems for concentrated solar power systems10.5006/1865 ↗
45. Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: pre-oxidation treatment and isothermal corrosion tests10.1016/j.solmat.2017.02.019 ↗
46. Corrosion resistance of MCrAlX coatings in a molten chloride for thermal storage in concentrating solar power applications
47. Molten chloride salts for next generation concentrated solar power plants: mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
48. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants - a review10.1007/s11705-018-1720-0 ↗
49. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
50. Molten chloride salts for next generation CSP plants: electrolytical saltpurification for reducing corrosive impurity level10.1016/j.solmat.2019.04.021 ↗
51. Corrosion evaluation of alumina-forming alloys in carbonate molten salt for CSP plants10.1016/j.renene.2019.03.087 ↗
52. Hot corrosion of different alloys in chloride and carbonate molten-salt mixtures under argon atmosphere10.1016/j.solener.2019.07.065 ↗
53. Corrosion monitoring and mitigation techniques on advanced thermal energy storage materials for CSP plants10.1016/j.solmat.2018.12.028 ↗
54. Magnesium salt decomposition and morphological development during evaporative decomposition of solutions10.1016/0040-6031(84)87128-2 ↗
55. Thermodynamics of stable and metastable structures in Fe–C system10.1016/j.calphad.2014.03.004 ↗
56. Equilibria in the systems Fe2C—Fe—CH4—H2 and Fe3C—Fe—CH4—H2110.1021/ja01165a108 ↗
57. Thermodynamic properties of minerals and related substances at 298.15 K (25 C) and one atmosphere (1.013 bars) pressure and at higher temperatures