Abstract
Abstract We have conducted a series of accelerated exposure test (AET) studies for various samples of crystalline-Si (c-Si) and amorphous-Si (a-Si) cells that were encapsulated with different superstrates, pottants, and substrates. Transmittance, fluorescence, color indices, impedance spectroscopy, laser optical beam induced current (OBIC), and light and dark current–voltage ( I – V ) measurements were used to characterize the samples. Nonuniform browning patterns of ethylene vinyl acetate (EVA) pottants were observed for glass/EVA/glass-encapsulated c-Si cell samples under solar simulator exposures at elevated temperatures. The EVA discolored gradually into a yellow–brown color when exposed under ∼7.5 ultraviolet (UV) suns at a black panel temperature (BPT) of ∼85°C, and very rapidly into a dark brown color when exposed under ∼9.0 UV suns at a BPT of ∼145°C. The latter conditions also caused extensive delamination of a polyolefin-based thermoplastic pottant laminated between two borosilicate plates. No visible color change of EVA could be observed for the c-Si cell samples heated in an oven at 85°C or exposed under ∼1.2 UV suns at BPT=60–65°C or 80–85°C. Under ∼1.2 UV suns exposure at a BPT of 60–65°C, the thin layers of EVA or silicone in the lightweight c-Si cell samples, which were laminated in a polymer/solar cell/polymer configuration with Tedlar or Tefzel films, did not discolor because of photobleaching reactions. In comparison, the polyester or nylon superstrate films turned yellow on laminates of polymer/a-Si/polymer minimodules, and significant delamination was observed for the polyester/EVA layers. For all c-Si cell samples tested, irregular changes in the I – V parameters were observed that could not be attributed only to transmittance changes of the superstrate/pottant layers. Under UV-transmitting polymer superstrate films, current/efficiency losses were greater for the c-Si and a-Si cells that were laminated with silicone-type adhesives than with EVA or polyethylene pottants.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Czanderna · Solar Energy Mater. Solar Cells · 1996 · 43 · 10110.1016/0927-0248(95)00150-6 ↗
2. C.E. Witt, M. Al-Jassim, J.M. Gee (Eds.), AIP Conference Proceedings No. 394 for the 14th NREL/SNL PV Program Review Meeting, November 1996, Lakewood, CO, American Institute of Physics, Woodbury, NY, 1997.10.1063/1.52894 ↗
3. Kroposki · 1997 · 285
4. von Roedern · 1997 · 313
5. Durand · 1997 · 323
6. King · 1997 · 347
7. N.G. Dhere (Ed.), Proceeding of PV Module Durability and Long-Term Exposure Symposium, Cocoa, FL, February 17–18, 1998, sponsored by Sandia National Laboratories.
8. S. Durand, A. Rosenthal, Long-term effects on roof-mounted photovoltaic modules, in: K.A. Summers (Coordinator), NREL Photovoltaic Program FY 1994 Annual Report, NREL/TP-410-7993, June 1995, pp. 349–352.
9. Rosenthal · 1999 · 655
10. Berman · Solar Energy Mater. Solar Cells · 1995 · 36 · 42110.1016/0927-0248(94)00198-7 ↗
11. Berman · Solar Energy Mater. Solar Cells · 1997 · 45 · 40110.1016/S0927-0248(96)00087-6 ↗
12. Berman · Solar Energy Mater. Solar Cells · 1999 · 58 · 25310.1016/S0927-0248(99)00002-1 ↗
13. Pern · 1999 · 559
14. F.J. Pern, Proceedings of the PV Performance and Reliability Workshop, September 16–18, 1992, Golden, CO, pp. 327–344.
15. Meier · 1999 · 661
16. M.J. Nowlan, J.C. Maglitta, T.R. Lamp, Proceedings of 33rd Intersociety Engineering Conference on Energy Conversion, IECEC-98-1253, Colorado Springs, CO, August 2–6, 1998, pp. 1253.
17. I.E. Eisgruber, Role of nonuniformity in thin film polycrystalline module characterization, a Ph.D. Dissertation, Department of Physics, Colorado State University, Fort Collins, CO, 1996, pp. 15–19 and references cited therein.
18. F.J. Pern, I. Eisgruber, R.H. Micheels, Proceedings of 25th IEEE PVSC, May 13–17, 1996, Washington D.C., pp. 1255–1258.10.1109/PVSC.1996.564360 ↗
19. Pern · Polym. Deg. and Stab. · 1993 · 41 · 12510.1016/0141-3910(93)90035-H ↗
20. Pern · Solar Energy Mater. Solar Cells · 1996 · 41/42 · 58710.1016/0927-0248(95)00128-X ↗
21. Pickett · Polym. Deg. and Stab. · 1993 · 42 · 23110.1016/0141-3910(93)90219-9 ↗
22. F.J. Pern, Proceedings of 6th PV Performance and Reliability Workshop, September 21–23, 1994, Lakewood, CO, pp. 329–347.
23. Klemchuk · Polym. Deg. and Stab. · 1997 · 55 · 34710.1016/S0141-3910(96)00162-0 ↗
24. Klemchuk · Polym. Deg. Stab. · 1991 · 34 · 33310.1016/0141-3910(91)90127-D ↗
25. Pern · 1997 · 811
26. D.L. King, B.R. Hansen, J.A. Kratochvil, M.A. Quintana, Proceedings of 26th IEEE PVSC, IEEE, 1997, pp. 1125–1128.
27. Green · 1992
28. J.I. Hanoka, Proceedings of 2nd WCPSEC/27th IEEE PVSC, Vienna, Austria, July 6–10, 1998, Vol. II, pp. 1974–1977.