Thermal activation of hydrogen for defect passivation in poly-Si based passivating contacts
Source abstract
Abstract
Abstract Hydrogenation of poly-Si based passivating contacts (TOPCon) is an essential process to achieve a very high level of surface passivation, especially on textured surface. This contribution is dedicated to improve the understanding of the hydrogenation mechanism. We compare different hydrogen sources with regard to their ability to chemically passivate defects at the Si/SiOx interface and presumably in the doped poly-Si layer as well as their thermal stability in a low and high temperature range. To this end, hotplate annealing series were performed on textured n-type TOPCon structures and Al2O3/SiNx multi-layer stacks were exposed to fast-firing processes. Very distinct activation characteristics were detected. It was also observed that the Al2O3 capping layers enable a higher level of surface passivation and higher thermal stability compared to SiNx. When implemented in multi-layer stacks, Al2O3 acts as a hydrogen diffusion barrier und prevents effusion from the TOPCon structure that deteriorates the passivation quality irreversibly.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. SiO2 surface passivation layers – a key technology for silicon solar cells10.1016/j.solmat.2018.04.029 ↗
2. Hydrogenation of phosphorus-doped polycrystalline silicon films for passivating contact solar cells10.1021/acsami.8b19989 ↗
3. Dielectric surface passivation for silicon solar cells: a review10.1002/pssa.201700293 ↗
4. Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristics10.1016/j.solmat.2013.09.017 ↗
5. On the hydrogenation of Poly-Si passivating contacts by Al2O3 and SiN thin films10.1016/j.solmat.2020.110592 ↗
6. Stodolny · 2018 · 414
7. Study on the interfacial oxide in passivating contacts10.1063/1.5123843 ↗
8. A passivating contact for silicon solar cells formed during a single firing thermal annealing10.1038/s41560-018-0239-4 ↗
9. C.R. Helms, E.H. Poindexter, The silicon-silicon dioxide system: its microstructure and imperfections, Rep. Prog. Phys. 57 791.10.1088/0034-4885/57/8/002 ↗
10. Interaction of Pb defects at the (111)Si/SiO2 interface with molecular hydrogen: simultaneous action of passivation and dissociation10.1063/1.373684 ↗
11. Hydrogen passivation of poly-Si/SiO x contacts for Si solar cells using Al 2 O 3 studied with deuterium10.1063/1.5031118 ↗
12. Analysis of hydrogen distribution and migration in fired passivating contacts (FPC)10.1016/j.solmat.2019.110018 ↗
13. Density of gap states of silicon grain boundaries determined by optical absorption10.1063/1.94278 ↗
14. Passivation of grain boundaries in polycrystalline silicon10.1063/1.90779 ↗
15. Degradation and regeneration of n+ -doped poly-Si surface passivation on p -type and n -type Cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
16. Long-term stability study of the passivation quality of polysilicon-based passivation layers for silicon solar cells10.1016/j.solmat.2020.110691 ↗
17. Lindekugel · 2008 · 2232
18. Improved passivation of n-type poly-Si based passivating contacts by the application of hydrogen-rich transparent conductive oxides
19. Interplay of annealing temperature and doping in hole selective rear contacts based on silicon-rich silicon-carbide thin films10.1016/j.solmat.2017.06.039 ↗
20. On the influence of the SiN x composition on the firing stability of poly‐Si/SiN x stacks10.1002/pssa.202000333 ↗
21. Hydrogenation mechanisms of poly‐Si/SiO x passivating contacts by different capping layers10.1002/solr.201900476 ↗
22. Polycrystalline silicon passivated tunneling contacts for high efficiency silicon solar cells10.1557/jmr.2016.77 ↗
23. Surface passivation of crystalline silicon solar cells: present and future10.1016/j.solmat.2018.06.047 ↗
24. Influence of annealing and Al 2 O 3 properties on the hydrogen-induced passivation of the Si/SiO 2 interface10.1063/1.4709729 ↗
25. Reaction kinetics during the thermal activation of the silicon surface passivation with atomic layer deposited Al 2 O 310.1063/1.4865901 ↗
26. Carrier-diffusion corrected J0-analysis of charge carrier lifetime measurements for increased consistency10.1016/j.solmat.2015.06.043 ↗
27. Laser-powered Co-firing process for highly efficient Si solar cells10.1109/JPHOTOV.2020.3043856 ↗
28. VCSEL arrays expanding the range of high-power laser systems and applications
29. Thermal activation energy for the passivation of the n-type crystalline silicon surface by hydrogenated amorphous silicon10.1063/1.3120765 ↗
30. Correlation between midgap interface state density and thickness‐averaged oxide stress and strain at Si/SiO 2 interfaces formed by thermal oxidation of Si10.1063/1.103228 ↗
31. Investigation of the strain relaxation mechanism in the Si–SiO2 system during the process of its formation10.1002/pssa.200306611 ↗
32. Electronic structure of silicon nitride10.1080/01418639108224430 ↗
33. Defects and hydrogen in amorphous silicon nitride10.1080/01418639408240111 ↗
34. Modelling of hydrogen transport in silicon solar cell structures under equilibrium conditions10.1063/1.5016854 ↗
35. Hydrogenation of Si from SiNx(H) films: Characterization of H introduced into the Si10.1063/1.1598643 ↗
36. Hot-wire chemical vapor deposition of high hydrogen content silicon nitride for solar cell passivation and anti-reflection coating applications10.1016/S0040-6090(03)00131-7 ↗
37. Hydrogen induced passivation of Si interfaces by Al2O3 films and SiO2/Al2O3 stacks10.1063/1.3497014 ↗
38. Energetics and diffusion of hydrogen in SiO210.1103/PhysRevB.61.4417 ↗
39. Time-resolved thermal annealing of interface traps in aluminium gate-silicon oxide-silicon devices10.1109/23.7507 ↗
40. Richter · 2014
41. Activation energy of negative fixed charges in thermal ALD Al2O310.1063/1.4960097 ↗
42. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon10.1002/pip.3240 ↗
43. Controlling light- and elevated-temperature-induced degradation with thin film barrier layers10.1109/JPHOTOV.2019.2945199 ↗
44. Atomic‐layer‐deposited Al 2 O 3 as effective barrier against the diffusion of hydrogen from SiN x :H layers into crystalline silicon during rapid thermal annealing10.1002/pssr.202000367 ↗
45. Kang · 2020 · 188