Promising long-term stability of encapsulated ITO-free bulk-heterojunction organic solar cells under different aging conditions
Source abstract
Abstract
Abstract This paper reports on the stability of encapsulated ITO-free bulk heterojunction organic solar cells (BHJ-OSC) with the layer sequence of Cr/Al/Cr/photoactive layer (PAL)/poly (3, 4-ethylenedioxythiophene) poly (styrenesulfonate) (PEDOT:PSS)/metal-grid under different aging conditions. The PAL consisted of poly (3-hexylthiophene) (P3HT) as donor and (6,6)-phenyl-C 60 butyric acid methyl ester (PCBM) as acceptor. Completely flexible devices (encapsulated between two flexible barrier films) were able to maintain >95% of their initial device performance after 1000 h of aging under damp heat condition (85 °C/85% relative humidity) according to standard IEC 61646. Suns– V OC measurements reveal that there is a slight increase in both the transport resistance of the photoactive layer as well as the series resistance of the PEDOT:PSS electrode. Devices encapsulated between two glass plates were able to retain more than 90% of their initial device performance after ca. 1800 h of aging under damp heat condition. Similar devices encapsulated between two glass plates and between a glass plate and flexible barrier film showed almost no degradation after ca. 10,000 h under thermal stress of 85 °C (dark and ambient air). Further, remarkable stability of more than 12,000 h with less than 10% reduction in the device performance was achieved under continuous illumination of 1000 W/m 2 (similar to AM1.5G spectrum but with lower UV content).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Polymer photovoltaic cells: enhanced efficiencies via a network of internal donor–acceptor heterojunctions10.1126/science.270.5243.1789 ↗
2. Conjugated polymer-based organic solar cells10.1021/cr050149z ↗
3. Plastic solar cells10.1002/1616-3028(200102)11:1<15::AID-ADFM15>3.0.CO;2-A ↗
4. Photovoltaic and photophysical properties of a novel bis-3-hexylthiophene substituted quinoxaline derivative10.1016/j.solmat.2008.04.004 ↗
5. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
6. Solar cell efficiency tables (version 41)10.1002/pip.2452 ↗
7. A polymer tandem solar cell with 10.6% power conversion efficiency10.1038/ncomms2411 ↗
8. High efficiency polymer solar cells with long operating lifetimes10.1002/aenm.201100138 ↗
9. Long-term operational lifetime and degradation analysis of P3HT:PCBM photovoltaic cells10.1016/j.solmat.2010.09.007 ↗
10. Upscaling of polymer solar cell fabrication using full roll-to-roll processing10.1039/b9nr00430k ↗
11. Polymer-fullerene bulk-heterojunction solar cells10.1002/adma.200801283 ↗
12. Business, market and intellectual property analysis of polymer solar cells10.1016/j.solmat.2010.04.074 ↗
13. Photodegradation and photo-oxidation of synthetic polymers10.1016/0165-2370(89)85037-5 ↗
14. Infrared spectroscopic detection of sulphone groups in doped polybenzo[c]thiophenes10.1016/0584-8539(91)80082-T ↗
15. Photoimaging of electronically conducting polymeric networks10.1021/cm00018a009 ↗
16. Mechanisms of photodegradation of poly( 3-alkylthiophenes) in solution10.1021/ma00063a047 ↗
17. Solid-state photochemistry of π conjugated poly(3-alkylthiophenes)10.1139/v95-234 ↗
18. Photochemical transformation of C60 and C70 films10.1016/0040-6090(94)05704-4 ↗
19. Oxygen and methylene adducts of C60 and C7010.1021/ja00015a080 ↗
20. Synthesis and characterization of C60O, the first fullerene epoxide10.1021/ja00029a058 ↗
21. Defect quenching of conjugated polymer luminescence10.1103/PhysRevLett.73.744 ↗
22. Photo-oxidation of polymers used in electroluminescent devices10.1016/0379-6779(95)80015-8 ↗
23. Light-induced degradation of the active layer of polymer-based solar cells10.1016/j.polymdegradstab.2009.11.021 ↗
24. Photochemical stability of π-conjugated polymers for polymer solar cells: a rule of thumb10.1039/c0jm03105d ↗
25. Effects of photo-oxidation on the performance of poly[2-methoxy-5-(3′,7′-dimethyloctyloxy)-1,4-phenylene vinylene]:[6,6]-phenyl C61-butyric acid methyl ester solar cells10.1002/adfm.200500714 ↗
26. The mechanism of photo- and thermooxidation of poly(3-hexylthiophene) (P3HT) reconsidered10.1016/j.polymdegradstab.2009.03.005 ↗
27. Photo- and thermo-oxidation of poly(p-phenylene-vinylene) and phenylene-vinylene oligomer10.1016/j.polymdegradstab.2011.02.002 ↗
28. Morphology and thermal stability of the active layer in poly(p-phenylenevinylene)/methanofullerene plastic photovoltaic devices10.1021/ma035620+ ↗
29. Relating the morphology of poly(p-phenylene vinylene)/methanofullerene blends to solar cell performance10.1002/adfm.200305049 ↗
30. Impact of contact evolution on the shelf life of organic solar cells10.1039/b910213b ↗
31. Observation of degradation processes of Al electrodes in organic electroluminescence devices by electroluminescence microscopy, atomic force microscopy, scanning electron microscopy, and Auger electron spectroscopy10.1063/1.357224 ↗
32. Analysis of the degradation mechanism of ITO-free organic solar cells under UV radiation10.1016/j.solmat.2013.10.021 ↗
33. Water vapor and oxygen degradation mechanisms in organic light emitting diodes10.1002/1616-3028(200104)11:2<116::AID-ADFM116>3.0.CO;2-B ↗
34. Degradation of organic light-emitting diodes under different environment at high drive conditions10.1016/j.orgel.2006.10.005 ↗
35. Influence of the hole-transport layer on the initial behavior and lifetime of inverted organic photovoltaics10.1016/j.solmat.2010.12.036 ↗
36. Flexible, conjugated polymer-fullerene-based bulk-heterojunction solar cells: basics, encapsulation, and integration10.1557/jmr.2005.0399 ↗
37. A new encapsulation solution for flexible organic solar cells10.1016/j.tsf.2005.12.091 ↗
38. Stability and photodegradation mechanisms of conjugated polymer/fullerene plastic solar cells10.1016/S0927-0248(99)00094-X ↗
39. Flexible long-lived large-area organic solar cells10.1016/j.solmat.2006.10.013 ↗
40. Nanoscale morphology of high-performance polymer solar cells10.1021/nl048120i ↗
41. Flexible organic P3HT:PCBM bulk-heterojunction modules with more than 1 year outdoor lifetime10.1016/j.solmat.2008.01.004 ↗
42. Large-area organic photovoltaic module-fabrication and performance10.1016/j.solmat.2008.11.018 ↗
43. Semitransparent OPV modules pass environmental chamber test requirements10.1016/j.solmat.2012.09.031 ↗
44. Longterm stability of efficient inverted P3HT:PCBM solar cells10.1016/j.solmat.2008.12.022 ↗
45. The mechanism of burn-in loss in a high efficiency polymer solar cell10.1002/adma.201103010 ↗
46. V.L. Dalal, R. Mayer, J. Bhattacharya, M. Samiee, Stability of organic solar cells, in: Proceedings of the Reliability Physics Symposium (IRPS), IEEE International, 2012, pp. 4A.5.1–4A.5.4.10.1109/IRPS.2012.6241829 ↗
47. P.C. Yang, S.Y. Ma, C.H. Shia, Y.M. Shen, C.P. Chen, C.F. Lin, Inverted low-band gap polymer solar cells with long-term stability, in: Proceedings of the 37th IEEE Photovoltaic Specialists Conference (PVSC), 2011, pp. 001203–001205.10.1109/PVSC.2011.6186172 ↗
48. Air-stable inverted flexible polymer solar cells using zinc oxide nanoparticles as an electron selective layer10.1063/1.2945281 ↗
49. The ISOS-3 inter-laboratory collaboration focused on the stability of a variety of organic photovoltaic devices10.1039/C1RA00686J ↗
50. Ultra-high barriers for encapsulation of flexible organic electronic devices
51. ITO-free laminated concept for flexible organic solar cells10.1016/j.solmat.2013.09.024 ↗
52. ITO-free organic solar cells with roll-to-roll coated organic functional layers from non-halogenated solvents10.1016/j.solmat.2014.02.001 ↗
53. R.A. Sinton, A. Cuevas, A quasi-steady-state open-circuit voltage method for solar cell characterization, in: Proceedings of the 16th European Photovoltaic Solar Energy Conference, Glasgow, 2000, pp. 1152–1155.
54. Applicability of the Suns-Voc method on organic solar cells10.1109/JPHOTOV.2013.2288527 ↗
55. Determination of the intrinsic and the injection dependent charge carrier density in organic solar cells using the Suns-Voc method10.1063/1.4862960 ↗
56. The stability of PEDOT:PSS films monitored by electron spin resonance10.3938/jkps.52.621 ↗
57. Influence of photo-induced degradation on the optoelectronic properties of regioregular poly(3-hexylthiophene)10.1016/j.solmat.2008.01.002 ↗