journal article·2018-05

Shrinkage characteristics of heat-treated ultra-high performance concrete and its mitigation using superabsorbent polymer based internal curing method

Sung-Hoon Kang, Sung-Gul Hong, Juhyuk Moon

Publisher page

Abstract

Abstract The shrinkage and cracking risk of heat-treated ultra-high performance concrete (UHPC) can be mitigated by using the superabsorbent polymer (SAP)-based internal curing method. The heat treatment (HT) accelerates the hydration reaction and resulting self-desiccation of UHPC; consequently, the UHPC experiences severe shrinkage during the HT. This study experimentally demonstrates that the shrinkage is effectively resolved by adopting the SAP-based internal curing method during the HT period as well as early-ages. This method also reduces the strain rate resulting from dimensional change, without showing an increase in drying shrinkage. The accurately conducted experiments herein can help to better understand the shrinkage characteristics of heat-treated UHPC and broaden the application of various internal curing agents.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Association Française de Génie Civil (AFGC) · 2013
2. Japan Society of Civil Engineers (JSCE) · 2004
3. Korea Concrete Institute (KCI) · 2012
4. NF P18-470 · 2016
5. The newly enforced French standard for UHPFRC specification, performance, production, and conformity
6. Effect of curing temperature at an early age on the long-term strength development of UHPC
7. Creep of UHPC in tension and compression: effect of thermal treatment10.1016/j.cemconcomp.2011.12.002 ↗
8. Effect of heat treatment method on the properties of UHPC
9. Phase composition and strength of thermally treated UHPC
10. Composition of reactive powder concretes10.1016/0008-8846(95)00144-2 ↗
11. Effects of nano-silica and nano-limestone on flowability and mechanical properties of ultra-high-performance concrete matrix10.1016/j.conbuildmat.2015.05.137 ↗
12. Influence of nanolimestone on the hydration, mechanical strength, and autogenous shrinkage of ultrahigh-performance concrete
13. National Precast Concrete Association (NPCA) · 2013
14. Delayed ettringite formation10.1016/S0008-8846(01)00466-5 ↗
15. Heat treatment and the risk of DEF delayed ettringite formation in UHPC
16. Effect of water-to-cementitious materials ratio and silica fume on the autogenous shrinkage of concrete10.1016/S0008-8846(03)00149-2 ↗
17. Vande Voort · 2008
18. Autogenous deformation and change of the relative humidity in silica fume-modified cement paste
19. Autogenous shrinkage in high-performance cement paste: an evaluation of basic mechanisms10.1016/S0008-8846(02)00890-6 ↗
20. Mitigation strategies for autogenous shrinkage cracking10.1016/S0958-9465(03)00045-3 ↗
21. A new approach to determine autogenous shrinkage of mortar at an early age considering temperature history10.1016/S0008-8846(00)00241-6 ↗
22. Autogenous deformations of cement pastes: Part I. Temperature effects at early age and micro–macro correlations10.1016/j.cemconres.2004.10.019 ↗
23. Temperature dependence of autogenous shrinkage of silica fume cement pastes with a very low water–binder ratio10.1016/j.cemconres.2013.03.017 ↗
24. Autogenous shrinkage of high performance concrete containing mineral admixtures under different curing temperatures10.1016/j.conbuildmat.2014.03.023 ↗
25. Effect of curing temperature and type of cement on early-age shrinkage of high-performance concrete10.1016/S0008-8846(01)00601-9 ↗
26. The influence of superabsorbent polymers on the autogenous shrinkage properties of cement pastes with supplementary cementitious materials10.1016/j.cemconres.2015.03.020 ↗
27. Material property characterization of ultra-high performance concrete
28. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
29. Effectiveness of shrinkage-reducing admixture in reducing autogenous shrinkage stress of ultra-high-performance fiber-reinforced concrete10.1016/j.cemconcomp.2015.09.005 ↗
30. Shrinkage and cracking of restrained ultra-high-performance fiber-reinforced concrete slabs at early age10.1016/j.conbuildmat.2014.09.097 ↗
31. Internal curing by superabsorbent polymers in ultra-high performance concrete10.1016/j.cemconres.2015.05.005 ↗
32. Autogenous shrinkage strain of ultra-high-performance concrete (UHPC)
33. Early-age shrinkage development of ultra-high-performance concrete under heat curing treatment10.1016/j.conbuildmat.2016.11.024 ↗
34. Water-entrained cement-based materials: I. Principles and theoretical background10.1016/S0008-8846(01)00463-X ↗
35. Water-entrained cement-based materials: II. Experimental observations10.1016/S0008-8846(02)00737-8 ↗
36. Absorption kinetics of superabsorbent polymers (SAP) in various cement-based solutions10.1016/j.cemconres.2017.03.009 ↗
37. Importance of monovalent ions on water retention capacity of superabsorbent polymer in cement based solutions10.1016/j.cemconcomp.2018.01.015 ↗
38. Microstructural investigation of heat-treated ultra-high performance concrete for optimum production10.3390/ma10091106 ↗
39. Influence of internal curing by superabsorbent polymer on mechanical properties of ultra high performance concrete
40. Effect of water-entraining admixtures on the hydro-mechanical properties of ultra-high performance concrete
41. Relation between the molecular structure and the efficiency of superabsorbent polymers (SAP) as concrete admixture to mitigate autogenous shrinkage10.1016/j.cemconres.2012.03.011 ↗
42. A review of characterisation methods for superabsorbent polymer (SAP) samples to be used in cement-based construction materials: report of the RILEM TC 260-RSC10.1617/s11527-017-1060-4 ↗
43. Autogenous shrinkage of high-strength concrete containing silica fume under drying at early ages10.1016/j.cemconres.2004.06.006 ↗
44. Ultrasonic monitoring of setting and hardening of cement mortar-a new device10.1007/BF02480539 ↗
45. Ultrasonic in-situ monitoring of setting process of high-performance concrete10.1016/j.cemconres.2003.10.012 ↗
46. Monitoring the setting process of mortars by ultrasonic P and S-wave transmission velocity measurement10.1016/j.conbuildmat.2015.06.054 ↗
47. Mehta · 2006
48. Effect of water-retaining lightweight aggregate on the reduction of thermal expansion coefficient in mortar subject to temperature histories10.1016/j.cemconcomp.2012.08.003 ↗
49. Controlling the coefficient of thermal expansion of cementitious materials – a new application for superabsorbent polymers10.1016/j.cemconcomp.2012.08.010 ↗
50. Influence of superabsorbent polymers on hydration of cement pastes with low water-to-binder ratio10.1007/s10973-013-3359-x ↗
51. Phase development in normal and ultra high performance cementitious systems by quantitative X-ray analysis and thermoanalytical methods10.1016/j.cemconres.2008.11.003 ↗
52. Performance of silica fume-calcium hydroxide mixture as a repair material10.1016/S0958-9465(00)00075-5 ↗
53. Investigation of hydration and pozzolanic reaction in reactive powder concrete (RPC) using 29 Si NMR10.1016/0008-8846(95)00197-2 ↗
54. Microstructural investigation of innovative UHPC10.1016/S0008-8846(98)00225-7 ↗
55. Acceleration of intended pozzolanic reaction under initial thermal treatment for developing cementless fly ash based mortar10.3390/ma10030225 ↗
56. Intensified pozzolanic reaction on kaolinite clay-based mortar10.3390/app7050522 ↗
57. Water consumption of the early-age paste and the determination of “time-zero” of self-desiccation shrinkage10.1016/j.cemconres.2007.08.005 ↗
58. Effect of mineral filler type on autogenous shrinkage of self-compacting concrete10.1016/j.cemconres.2010.01.014 ↗
59. Effect of fly ash on autogenous shrinkage10.1016/j.cemconres.2004.07.010 ↗
60. Hydration kinetics, change of relative humidity, and autogenous shrinkage of ultra-high-strength concrete10.1016/S0008-8846(99)00022-8 ↗
61. Autogenous deformation and RH-change in perspective10.1016/S0008-8846(01)00501-4 ↗
62. Thermal dilation and internal relative humidity of hardened cement paste10.1617/s11527-006-9108-x ↗
63. Delayed thermal dilatations of cement paste and concrete due to mass transport10.1016/0029-5493(70)90108-1 ↗
64. Immediate and delayed thermal expansion of hardened cement paste10.1016/0008-8846(82)90007-2 ↗
65. Short-term tensile creep and shrinkage of ultra-high performance concrete10.1016/j.cemconcomp.2009.01.002 ↗
66. Powers · 1948
67. Micro-computed tomography study on the pore structure of ultra-high performance concrete containing water-entraining admixture
68. The use of superabsorbent polymers to reduce cracking of bonded mortar overlays10.1016/j.cemconcomp.2014.03.009 ↗
69. Neville · 1981
70. Effects of SAP on the properties and pore structure of high performance cement-based materials10.1016/j.conbuildmat.2016.11.090 ↗