Abstract

Measures to improve the cycling performance and stability of bulk-type all-solid-state batteries (SSBs) are currently being developed with the goal of substituting conventional lithium-ion battery (LIB) technology. As known from liquid electrolyte-based LIBs, layered oxide cathode materials undergo volume changes upon (de)lithiation, causing mechanical degradation because of particle fracture, among others. Unlike solid electrolytes, liquid electrolytes are somewhat capable of accommodating morphological changes. In SSBs, the rigidity of the materials used typically leads to adverse contact loss at the interfaces of cathode material and solid electrolyte during cycling. Hence, designing zero- or low-strain electrode materials for application in next-generation SSBs is desirable. In the present work, we report on novel Co-rich NCMs, NCM361 (60% Co) and NCM271 (70% Co), showing minor volume changes up to 4.5 V versus Li+/Li, as determined by operando X-ray diffraction and pressure measurements of LIB pouch and pelletized SSB cells, respectively. Both cathode materials exhibit good cycling performance when incorporated into SSB cells using argyrodite Li6PS5Cl solid electrolyte, albeit their morphology and secondary particle size have not yet been optimized.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Battery and Electrochemistry Laboratory, Institute of Nanotechnology, Karlsruhe Institute of Technology (KIT), Hermann-von-Helmholtz-Platz 1, 76344 Eggenstein-Leopoldshafen, Germany

Institute of Physical Chemistry & Center for Materials Science, Justus-Liebig-University Giessen, Heinrich-Buff-Ring 17, 35392 Giessen, Germany

BASF SE, Carl-Bosch-Strasse 38, 67056 Ludwigshafen, Germany

Funding

BASF International Network for Batteries and Electrochemistry

References (22)

Show source-provided references
1. 10.1038/nenergy.2016.14110.1038/nenergy.2016.141 ↗
2. 10.1149/2.1571707jes10.1149/2.1571707jes ↗
3. 10.1021/acsenergylett.6b0059410.1021/acsenergylett.6b00594 ↗
4. 10.1002/anie.20181247210.1002/anie.201812472 ↗
5. 10.1021/acsenergylett.9b0065210.1021/acsenergylett.9b00652 ↗
6. 10.1021/acs.jpcc.7b0636310.1021/acs.jpcc.7b06363 ↗
7. 10.1021/acs.jpcc.6b1288510.1021/acs.jpcc.6b12885 ↗
8. 10.1038/srep3966910.1038/srep39669 ↗
9. 10.1016/j.ssi.2016.01.00910.1016/j.ssi.2016.01.009 ↗
10. 10.1021/acs.chemmater.7b0526910.1021/acs.chemmater.7b05269 ↗
11. 10.1021/acs.chemmater.7b0093110.1021/acs.chemmater.7b00931 ↗
12. 10.1039/C8EE00907D10.1039/C8EE00907D ↗
13. Rosciano, F.; Christensen, M.; Eyert, V.; Mavromaras, A.; Wimmer, E. Reduced Strain Cathode Materials for Solid State Lithium Ion Batteries. International Patent No. WO/2014/191018, 2014.
14. 10.1021/acs.jpcc.7b0659810.1021/acs.jpcc.7b06598 ↗
15. 10.1021/cm504753410.1021/cm5047534 ↗
16. 10.1107/S056773947600155110.1107/S0567739476001551 ↗
17. 10.1021/acs.chemmater.5b0494010.1021/acs.chemmater.5b04940 ↗
18. 10.1021/acsenergylett.8b0027510.1021/acsenergylett.8b00275 ↗
19. 10.1039/C9CC04453A10.1039/C9CC04453A ↗
20. 10.1038/s41598-019-41767-010.1038/s41598-019-41767-0 ↗
21. 10.1021/acs.chemmater.9b0077010.1021/acs.chemmater.9b00770 ↗
22. 10.1021/acs.chemmater.6b0499010.1021/acs.chemmater.6b04990 ↗