Photoluminescence spectroscopy of highly oriented Y2O3:Tb crystalline whiskers
Source abstract
Abstract
AbstractThe crystalline state of terbium-containing yttria is one of the important candidates for uses to ultraviolet- and electron-excited green phosphors. To increase the intensity of green emission, structural design of the polycrystalline Y2O3:Tb was carried out using a chemical-vapor-deposition technique operated under atmospheric pressure. The green luminescence intensity was strongly dependent upon the concentration of Tb. The intensity of the photoluminescence at 542 nm obtained from ȥ100Ɂ oriented Y2O3:Tb whiskers was higher than that obtained from the uniform Y2O3:Tb polycrystalline film with random orientation.Key words: Y2O3:TbCVDOrientationWhiskerPhosphorPolycrystalPhotoluminescence
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 10.1557/JMR.1990.157310.1557/JMR.1990.1573 ↗
2. 10.1063/1.12032910.1063/1.120329 ↗
3. 10.1016/S0022-2313(96)00237-210.1016/S0022-2313(96)00237-2 ↗
4. 10.1143/JJAP.38.L58610.1143/JJAP.38.L586 ↗
5. 10.1143/JJAP.38.687310.1143/JJAP.38.6873 ↗
6. 10.1143/JJAP.40.701310.1143/JJAP.40.7013 ↗
7. 10.1143/JJAP.39.L16910.1143/JJAP.39.L169 ↗
8. N. Tanaka · J. Ceram. Soc. Jpn · 1997 · 105 · 55110.2109/jcersj.105.551 ↗
9. H. Saitoh · Initial growth process of epitaxially chemical-vapor-deposited titanium dioxide crystalline films · 1998 · 165
10. H. Saitoh · J. Ceram. Soc. Jpn. · 1998 · 106 · 105110.2109/jcersj.106.1051 ↗
11. 10.1143/JJAP.41.L125310.1143/JJAP.41.L1253 ↗
12. 10.1143/JJAP.40.602410.1143/JJAP.40.6024 ↗