Interaction of Ground SmCo4.8Zr0.2 Alloy with Hydrogen
Source abstract
Abstract
The hydrogen pressure and reaction time were studied during disproportionation of the ground SmCo4.8Zr0.2 alloy. The alloy ground at ν = 100 rpm for τ = 24 h disproportionates at 0.5 MPa hydrogen pressure within 15–30 min, the alloy ground at ν = 200 rpm for τ = 6 and 12 h disproportionates at 0.5 MPa hydrogen pressure, and the alloy ground at ν = 300 rpm for τ = 6 h disproportionates into SmHx and ht-Co below 0.1 MPa hydrogen pressure. Residues of the CaCu5–type ferromagnetic phase were found among the disproportionation products.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Rare-earth and actinide compounds · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. J. P. Liu, E. Fullerton, O. Gutfleisch, and D. J. Sellmyer, Nanoscale Magnetic Materials and Applications, Springer, London (2009), p. 731.10.1007/978-0-387-85600-1 ↗
2. N. Poudyal and J. P. Liu, “Advances in nanostructured permanent magnets research,” J. Phys. D: Appl. Phys., 46, 1–23 (2013).
3. O. Gutfleisch, M. A. Willard, E. Brück, et al., “Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient,” J. Adv. Mater., 23, 821–842 (2011).10.1002/adma.201002180 ↗
4. N. Cannesan and I. R. Harris, “Aspects of NdFeB HDDR powders: fundamentals and processing,” in: G. C. Hadjipanayis (ed.), Bonded Magnets, NATO Science Series: II. Mathematics, Physics and Chemistry (2002), Vol. 118, pp. 13–36.
5. I. I. Bulik and V. V. Panasyuk, “Hydrogen as a process environment to form nanostructure in ferromagnetic Sm–Co alloys,” Fiz. Khim. Mekh. Mater., 48, No. 1, 9–18 (2012).
6. I. I. Bulyk and V. V. Burkhovetsky, “Variation in microstructure of ground SmCo5 alloy during disproportionation in hydrogen and recombination,” Powder Metall. Met. Ceram., 54, No. 9–10, 614–623 (2015).10.1007/s11106-016-9755-6 ↗
7. I. I. Bulyk, V. N. Varyukhin, V. Yu. Tarenkov, et al., “Effect of hydrogen treatment on the microstructure and magnetic properties of KS37 alloys (SmCo5—substrate),” Fiz. Tekh. Vys. Davl., 23, No. 4, 67–82 (2013).
8. K. Suresh, R. Gopalan, G. Bhikshamaiah, et al., “Phase formation, microstructure and magnetic properties investigation in Cu and Fe substituted SmCo5 melt-spun ribbons,” J. Alloys Compd., 463, 73–77 (2008).10.1016/j.jallcom.2007.09.062 ↗
9. K. Suresh, R. Gopalan, D. V. Sridhara Rao, et al., “Microstructure and coercivity variation in melt-spun Sm–Co–Fe–Zr ribbons,” Intermetallics, 18, 2244–2249 (2010).10.1016/j.intermet.2010.07.010 ↗
10. H. Zaigham and F. A. Khalid, “Characterization of Sm–Co–Sn alloys,” Mater. Charact., 61, 1274–1280 (2010).10.1016/j.matchar.2010.09.002 ↗
11. R. Gopalan, T. Ohkubo, and K. Hono, “Platelet microstructure and magnetic properties in rapidly solidified Sm20.8Co63.4Fe7.9Cu2.4Zr1.6B4 ribbons,” Scr. Mater., 53, 367–371 (2005).10.1016/j.scriptamat.2005.03.050 ↗
12. K. Suresh, R. Gopalan, A. K. Singh, et al., “Coercivity of Sm(Co0.9Cu0.1)4.8 melt-spun ribbons,” J. Alloys Compd., 436, 358–363 (2007).10.1016/j.jallcom.2006.07.052 ↗
13. X. B. Liu and Z. Altounian, “Magnetic moments and exchange interaction in Sm(Co, Fe)5 from firstprinciples,” Comput. Mater. Sci., 50, 841–846 (2011).10.1016/j.commatsci.2010.10.019 ↗
14. Y. Zhang, A. Gabay, Y. Wang, and G. C. Hadjipanayis, “Microstructure, microchemistry, and coercivity in Sm–Co–Cu and Pr–Co–Cu 1:5 alloys,” J. Magn. Magn. Mater., 272–276, e1899–e1900 (2004).10.1016/j.jmmm.2003.12.899 ↗
15. R. F. Sabirianov, A. Kashyap, R. Skomski, et al., “First principles study of transition-metal substitutions in Sm–Co permanent magnets,” J. Appl. Phys. Lett., 85, No. 12, 2286–2288 (2008).10.1063/1.1792791 ↗
16. A. A. Kündig, R. Gopalan, T. Ohkubo, and K. Hono, “Coercivity enhancement in melt-spun SmCo5 by Sn addition,” Scr. Mater., 54, 2047–2051 (2006).10.1016/j.scriptamat.2006.03.007 ↗
17. Z. Yao, Q. Xu, and C. Jiang, “Structural and magnetic properties of SmCo5.6Ti0.4 alloy,” J. Magn. Magn. Mater., 320, 1717–1721 (2008).10.1016/j.jmmm.2008.01.042 ↗
18. T. Saito and D. Nishio-Hamane, “Magnetic properties of SmCo5–xFe x (x = 0–4) melt-spun ribbon,” J. Alloys Compd., 585, 423–427 (2014).10.1016/j.jallcom.2013.09.183 ↗
19. J. Zhou, R. Skomski, and D. J. Sellmyer, “Coercivity of titanium-substituted high-temperature permanent magnets,” J. IEEE Trans. Magn., 37, 2518–2520 (2001).10.1109/20.951221 ↗
20. R. S. K. Valiveti, A. Ingmire, C. Baudot, and J. E. Shield, “Microstructural selection in conventionally and rapidly solidified Sm–Co–T alloys,” J. Alloys Compd., 493, 95–98 (2010).10.1016/j.jallcom.2009.12.069 ↗
21. A. Handstein, M. Kubis, O. Gutfleisch, et al., “HDDR of Sm–Co alloys using high hydrogen pressures,” J. Magn. Magn. Mater., 192, 73–76 (1999).10.1016/S0304-8853(98)00379-5 ↗
22. I. I. Bulyk, A. M. Trostyanchyn, and V. I. Markovich, “Phase transformations in SmCo5-based alloy initiated by hydrogen at 650 kPa pressure,” Fiz. Khim. Mekh. Mater., No. 1, 94–98 (2007).
23. I. I. Bulyk, V. I. Markovich, and A. M. Trostyanchyn, “Features of solid HDDR in SmCo5-based alloys in low-pressure hydrogen,” Fiz. Khim. Mekh. Mater., No. 4, 121–126 (2008).
24. I. I. Bulyk, V. V. Burkhovetsky, and A. M. Trostyanchyn, “Change in phase and structural state of SmCo5-based alloy in solid HDDR in low-pressure hydrogen,” Metallofiz. Noveish. Tekhnol., No. 2, 169–184 (2015).
25. I. I. Bulyk, A. M. Trostyanchyn, and P. Ya. Lyuty, “Effect from the length of interaction between SmCo5-based alloy and low-pressure hydrogen on the phase composition,” Fiz. Khim. Mekh. Mater., No. 3, 53–58 (2012).
26. I. I. Bulyk, V. I. Markovich, A. M. Trostyanchyn, and V. A. Chervatyuk, “Hydrogen-initiated phase transformations in Sm–Co alloy under the action of ultrasound,” Fiz. Khim. Mekh. Mater., No. 5, 71–75 (2007).
27. I. I. Bulyk and A. M. Trostyanchyn, “Dependence of the phase composition of disproportionated SmCo5-based alloy on temperature and length of recombination,” Metallofiz. Noveish. Tekhnol., 38, No. 4, 511–519 (2016).10.15407/mfint.38.04.0509 ↗
28. I. I. Bulyk, A. M. Trostyanchyn, P. Ya. Lyuty, and V. V. Burkhovetsky, “Interaction between hydrogen and ground SmCo5 alloy,” Powder Metall. Met. Ceram., 52, No. 9–10, 530–538 (2013).10.1007/s11106-014-9556-8 ↗
29. N. Poudyal and J. P. Liu, “Advances in nanostructured permanent magnets research,” J. Phys. D: Appl. Phys., 46, 1–23 (2013).
30. V. A. Goltsov, S. B. Rybalka, D. Fruchart, and V. Didus, “Kinetics and same general features of hydrogen induced diffusive phase transformations in Nd2Fe14B type alloys,” in: V. A. Goltsov (ed.), Progress in Hydrogen Treatment of Materials, Kassiopeya, Donetsk–Coral Gables (2001), pp. 368–390.
31. I. I. Bulyk, I. V. Borukh, and A. M. Trostyanchyn, “Effect of grinding in hydrogen on the phase composition and anisotropy of SmCo4.8Zr0.2 alloy,” Fiz. Khim. Mekh. Mater., No. 4, 41–45 (2015).
32. I. I. Bulyk, R. V. Denis, V. V. Panasyuk, et al., “HDDR process and hydrogen-sorption properties of didymium–aluminum–iron–boron (Dd12.3Al1.2Fe79.4B6) alloy,” Fiz. Khim. Mekh. Mater., No. 4, 15–20 (2001).
33. I. I. Bulyk, Yu. B. Basaraba, A. M. Trostyanchyn, and V. M. Davidov, “Disproportionation in hydrogen and recombination of Laves phases of zirconium and chromium,” Fiz. Khim. Mekh. Mater., No. 3, 101–108 (2005).
34. CCP14, access mode: http://www.ccp14.ac.uk .
35. FullProf Suite, access mode: http://www.ill.eu/sites/fullprof .
36. O. Gutfleisch and I. R. Harris, “Fundamental and practical aspects of the hydrogenation, disproportionation, desorption and recombination process,” J. Phys. D: Appl. Phys., 29, 2255–2265 (1996).10.1088/0022-3727/29/9/006 ↗
37. D. L. Leslie-Pelecky and R. L. Schalek, “Effect of disorder on the magnetic properties of SmCo5,” J. Phys. Rev. B, 59, 457–462 (1999).10.1103/PhysRevB.59.457 ↗