Abstract

The formation and decomposition of LaNi5H6, TiFeH2, Ti2NiH, TiNiH2, Ti2CuH2.7, TiCuH, Ti3AlH3, Mg2NiH4, Mg2CuH3, and ZrMn2.8H4 intermetallic hydrides are thermodynamically analyzed in identical conditions. These reactions are competitive and the interface between them is determined by boundary composition $ {{\text{A}}_x}{{\text{B}}_y}{{\text{H}}_{{n_{\text{b}}}}} $ . For LaNi5, TiFe, Mg2Ni, and ZrMn2.8, intermetallides, ranges of stable hydrogenation are equal to 17, 27, 5, and 17% of the maximum hydrogen capacity, and the others are ranges of metastable hydrides, over which decomposition reactions are limited kinetically. The improvement in kinetics of intermetallide hydrogenation prevents the decomposition of intermetallic hydrides. This is promoted by mechanical or catalytic activation of hydrogenation and by the use of heat-conducting nonvolatile metal matrix composites based on intermetallides.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Materials Characterization Techniques · Catalytic Processes in Materials Science · Catalysis and Oxidation Reactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. M. Kh. Karapet’yants and M. L. Karapet’yants, Basic Thermodynamic Constants of Inorganic and Organic Substances [in Russian], Khimiya, Moscow (1968), p. 546.
2. M. Kh. Karapet’yants and M. L. Karapet’yants, Tables of Some Thermodynamic Properties of Different Substances [in Russian], Khim. Tekhnol. Inst., Moscow (1961), Issue 34, p. 166.
3. V. P. Glushko (ed.), Thermal Constants of Substances [in Russian], VINITI, Moscow (1972), Issue 7, P. 1, p. 370.
4. V. P. Glushko (ed.), Thermal Constants of Substances [in Russian], VINITI, Moscow (1974), Issue 6, P. 1, p. 344.
5. B. A. Kolachev, R. E. Shalin, and A. A. Il’in, Hydrogen-Accumulating Alloys: Handbook [in Russian], Metallurgiya, Moscow (1995), p. 384.
6. B. A. Kolachev, A. A. Il’in, V. A. Lavrenko, and Yu. V. Levinskii, Hydride Systems: Handbook [in Russian], Metallurgiya, Moscow (1992), p. 350.
7. T. I. Bratanich, V. V. Skorokhod, L. I. Kopylova, et al., “Destruction hydrogenation and recombination of α2-Ti3Al alloy: production of solid nanocomposites and coatings with improved properties. I. Mechanism of destructive hydrogenation of Ti3Al,” Powder Metall. Met. Ceram., 49, No. 7–8, 484–494 (2010).10.1007/s11106-010-9263-z ↗
8. T. I. Bratanich, V. V. Skorokhod, O. V. Kucheryavyi, et al., “Phase transformations in Ti2Cu under destructive hydrogenation and recombination,” Powder Metall. Met. Ceram., 49, No. 3–4, 220–226 (2010).10.1007/s11106-010-9225-5 ↗
9. T. I. Bratanich, S. M. Solonin, and V. V. Skorokhod, “Mechanical activation of the reaction of hydrogen with the intermetallics LaNi5 and TiFe in powder systems,” Int. J. Hydrogen Energy, 20, No. 5, 353–355 (1995).10.1016/0360-3199(94)00062-5 ↗
10. T. I. Bratanich, S. M. Solonin, and V. V. Skorokhod, “Hydrogen sorption peculiarities of mechanical activated intermetallic compound TiFe and TiFe–MmNi5(LaNi5) mixtures,” Int. J. Hydrogen Energy, 21, No. 11–12, 1049–1051 (1996).10.1016/S0360-3199(96)00042-0 ↗
11. T. I. Bratanich and S. M. Solonin, “Research into the rate of interaction between hydrogen and TiFe–Ni powder composites,” in: Current Problems of Physical Materials Science (Collected Scientific Papers) [in Russian], Kiev (2008), Issue 17, pp. 175–180.