Study of the Process of Destructive Hydrogenation of Powder Intermetallic Systems. Part 2. Rate of the First Destructive Hydrogenation of the Intermetallic TiNi

Tatyana I. Bratanich, Valerii V. Skorokhod

Powder Metallurgy and Metal Ceramics· Volume 44· Issue 1-2
Publisher page

Abstract

We have studied the rate of the first destructive hydrogenation of the as-poured bulk powder and compacts of TiNi. We have established that it is determined on the whole by the rate of processes that occur on the surface of the particles and are connected with formation of catalytic sites for dissociation of hydrogen, and by the rate of processes within the volume of the particles that is controlled by the rate of hydrogen diffusion and decomposition of TiNi. The first destructive hydrogenation of bulk TiNi powders is a lengthy process that can take tens of hours. Its rate increases as the temperature and hydrogen pressure increase. The effect of particle size is nonmonotonic because of the competing action of oxygen on the particle surface. Pressing TiNi powders made it possible to shorten the time required for the first destructive hydrogenation ten-fold (down to a few hours). This is connected with formation during pressing of fresh catalytic surfaces in closed cracks and on interparticle contacts. The rate of the first destructive hydrogenation of TiNi compacts increases as the temperature rises, and does not depend on particle size.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Powder Metallurgy Techniques and Materials · Material Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. K. N. Semenenko, V. N. Verbetskii, and M. I. Ioffe, “Hydrogenolysis of the intermetallic compounds LaNi5 and LaCo5 at high pressures and temperatures,” Vest. Mosk. Gos. Univ., No. 6, 560–563 (1979).
2. K. N. Semenenko, V. N. Verbetskii, and V. S. Zontov, “Reaction of Ti2Ni with hydrogen,” Zhurn. Neorg. Khim., 26, No.10, 2603–2605 (1981).
3. K. N. Semenenko, V. N. Verbetskii, V. S. Zontov, et al., “Reaction of intermetallic compounds of titanium with hydrogen,” Zhurn. Neorg. Khim., 27, No.6, 1359–1362 (1982).
4. K. N. Semenenko, V. N. Verbetskii, T. Kh. Kurbanov, et al., “Reaction with hydrogen of rare-earth-aluminum intermetallic compounds,” Zhurn. Neorg. Khim., 30, No.5, 1133–1137 (1985).
5. E. A. Movlaev, S. P. Sirotinkin, and V. N. Verbetskii, “Hydrogenolysis of ZrNiH3 under high pressure conditions,” Vest. Mosk. Gos. Univ., Ser. 2. Khimiya, 35, No.3, 197–200 (1994).
6. V. N. Verbetskii and E. A. Movlaev, “Conversion of hydrides of ZrCo and Zr2Co under high pressure conditions,” Vest. Mosk. Gos. Univ., Ser. 2. Khimiya, 37, No.1, 91–92 (1996).
7. I. R. Harris, A. J. Williams, and V. A. Yartys, “Recent developments in the HDDR process,” in: Seventh International Conference on Hydrogen Materials Science and Chemistry of Metal Hydrides (September 16–22, 2001, Alushta, Crimea, Ukraine), Kiev (2001), pp. 40–41.
8. A. B. Ryabov, V. A. Yartys’, R. V. Denis, and V. V. Panasyuk, “Homogenization of Pr-Fe-Al(Ga)-B cast alloy by HDDR treatment,” in: Seventh International Conference on Hydrogen Materials Science and Chemistry of Metal Hydrides (September 16–22, 2001, Alushta, Crimea, Ukraine), Kiev (2001), pp. 102–105.
9. A. B. Ryabov and I. Yu. Zavalii, “Modification of compounds based on rare-earth metals to design hydrogen sorbents that are resistant to disproportionation,” in: Seventh International Conference on Hydrogen Materials Science and Chemistry of Metal Hydrides (September 16–22, 2001, Alushta, Crimea, Ukraine), Kiev (2001), pp. 136–139.
10. I. Yu. Zavalii, V. A. Yartys’, and I. R. Harris, “Further studies of HDDR processes for Zr-based oxygen-stabilized compounds,” in: Seventh International Conference on Hydrogen Materials Science and Chemistry of Metal Hydrides (September 16–22, 2001, Alushta, Crimea, Ukraine), Kiev (2001), pp. 334–337.
11. T. I. Bratanich, S. M. Solonin, and V. V. Skorokhod, “Characteristic features of the process for activation of reaction between hydrogen and the intermetallics LaNi5, TiFe, and composites based on them. I. Compacts made from LaNi5 powder,” Poroshk. Metall., No. 5, 55–59 (1993).
12. T. I. Bratanich, S. M. Solonin, and V. V. Skorokhod, “Characteristic features of the process for activation of reaction between hydrogen and the intermetallics LaNi5, TiFe, and composites based on them. II. Compacts made from powders of TiFe and LaNi5, TiFe-metal mixtures,” Poroshk. Metall., No. 7, 91–94 (1993).