Abstract
A high-temperature Al–8Cr–1.5Fe alloy has been developed for applications in the range from room temperature to 300°C. The billets are obtained in two ways: using gas-atomized and water-atomized powders. Structural analysis shows that particles of the second phase in the water-atomized powders are finer and their number in the aluminum matrix is greater than that in the gas-atomized powders. The rods extruded from the water-atomized powders have much higher hardness, ultimate strength, and yield stress than those from the gas-atomized powders, plasticity being acceptable at all temperatures (20, 190, and 300°C). An additional powder metallurgy operation—pulsed hot pressing—does not increase the strength of billets from either the water-atomized or gas-atomized powders. The alloy based on the water-atomized 0–63 μm powder shows the maximum strength: 483, 332, and 261 MPa at 20, 190, and 300°C, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. V. I. Dobatkin, V. I. Elagin, and V. M. Fedorov, Rapidly Solidified Aluminum Alloys [in Russian], VILS, Moscow (1995), p. 360.
2. P. Y. Li , S. L. Dai, C. Y. Li, and B. C. Liu, “Some developments in rapidly solidified aluminum alloys for elevated temperature applications,” Acta Metall. Sinica, 12, No. 4, 452–461 (1999).
3. A. Ziani and G. Michot, “Preparation and characterization of centrifugally atomized Al–Cr–Fe alloy powders,” Int. J. Rapid Solidif., 9, No. 4, 305–321 (1996).
4. T. Sheppard and E. K. Ioannidis, “Powder metallurgy aluminum alloys: characteristics of an Al–Cr–Fe rapidly solidified alloy,” J. Mater. Sci., 25, No. 9, 3965–3975 (1990).10.1007/BF00582468 ↗
5. T. S. Srivatsan, S. Givens, Meslet Al-Hajri, et al., “The quasistatic fracture behavior of a bulk Al–Cr–Fe alloy made by consolidating micron- and nanosized powders,” J. Metastable Nanocryst. Mater., 23, 255–258 (2005).10.4028/www.scientific.net/JMNM.23.255 ↗
6. Osamu Kido, Mami Kurumada, Katsuya Kamitsuji, et al., “Synthesis of Al–Cr decagonal quasicrystal nanoparticles and their temperature of phase transformation to stable crystal phase. Original research article,” Physica E: Low-Dimens. Syst. Nanostruct., 31, No. 2, 169–173 (2006).10.1016/j.physe.2005.11.002 ↗
7. R. Garder, “Vapor deposition aluminum alloys,” Mater. Des., 10, No. 6, 274–279 (1989).10.1016/0261-3069(89)90001-0 ↗
8. A. W. Bowen and C. J. Gilmore, “Texture development in a hot-rolled rapidly-quenched Al–Cr–Fe alloy,” Text. Microstruct., 14–18, 1049–1054 (1991).10.1155/TSM.14-18.1049 ↗
9. O. D. Neikov, A. V. Krainikov, Yu. V. Mil’man, et al., Method of Producing Blanks from Aluminum Alloys [in Russian], Russian Federation Patent 2238172, IPC B 22 F 9/06, 3/115, No. 2003123486/02; applied July 29, 2003; publ. October 20 (2004), p. 23.
10. R. K. Ivashchenko, Yu. V. Mil’man, and Ya. S. Shchepanskii, “Effect of temperature and structural state on the strain hardening of molybdenum,” Fiz. Met. Metalloved., 48, 158–163 (1979).
11. Y. V. Milman, D. V. Lotsko, O. D. Neikov, et al., “Processing, structure and mechanical behavior of rapidly solidified aluminum alloys containing quasicrystalline particles,” Mater. Sci. Forum, 396–402, 723–728 (2002).10.4028/www.scientific.net/MSF.396-402.723 ↗
12. Y. V. Milman, A. I. Sirko, M. O. Iefimov, et al., “High strength aluminum alloys reinforced by nanosize quasicrystalline particles for elevated temperature application,” High Temp. Mater. Proc., 25, No. 1–2, 19–29 (2006).10.1515/HTMP.2006.25.1-2.19 ↗
13. A. V. Krainikov, “Effect of the structure and chemical inhomogeneity of rapidly solidified powders on the properties of aluminum alloys,” Powder Metall. Met. Ceram., 49, No. 7–8, 397–409 (2010).10.1007/s11106-010-9250-4 ↗
14. Yu. V. Mil’man, O. D. Neikov, A. I. Sirko, et al., “Structure and properties of Al–Mg alloys depending on scandium and zirconium additions and production methods,” Powder Metall. Met. Ceram., 49, No. 7–8, 430–437 (2010).10.1007/s11106-010-9254-0 ↗
15. V. F. Moiseev, “Effective indicator of metal strain hardening,” Metallofiz. Noveish. Tekhnol., 23, No. 7, 387–399 (2001).