Structure and properties of thin ceramic coatings in the system AlN-TiCrB2
Source abstract
Abstract
The structure, composition and properties of coatings on Si, Al2O3 and GaAs single crystals prepared by radio-frequency magnetron sputtering of a AlN-TiCrB2 target prepared by powder metallurgy are studied. Coating phase composition is different from that of the target material due to oxidation of aluminum nitride and its dissociation under ion bombardment conditions. The coatings have a very fine structure and marked resistance to high-temperature oxidation due to formation of solid solutions in the systems Al2O3-TiO2-Cr2O3 and Al2O3-B2O3. The increase in mass of the target material at 1300°C is 1.4 mg/cm2. After high-temperature oxidation the reinforced fine structure of the coating forms as interwoven Al2O3 fibers. Coatings of (AlN-TiCrB2)-Al2O3 and (AlN-TiCrB2)-GaAs are thermally stable up to 900°C and have a high microhardness (H µ) and crack resistance (KIc = 4.7–3.3 MN/m3/2). With an increase in annealing temperature (T ≥ 1000°C) coating mechanical properties worsen, but their adhesive strength increases. The AlN-TiCrB2 target material may be recommended for preparing wear-and corrosion-resistant coatings on tools, and also on critical components operating under extreme conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Y. Tanaka, T. M. Gur, M. Kelly, et al., “Propertires of (Ti1−x Alx)N coatings for cutting tools prepared by the cathodic arc ion plating method,” J. Vac. Sci. Technol. A, 10, No. 4, Part 2, 1749–1756 (1992).10.1116/1.577742 ↗
2. Harte, “Schichten Zahlen Sich Aus,” Techn. Report, 19, No. 5, 44 (1992).
3. J. Y. Rauch, C. Rousselot, N. Martin, et al., “Characterization of (Ti1− xAlx)N films prepared by radio-frequency reactive magnetron sputtering,” Europ. Ceram. Soc., 20, 795–799 (2000).10.1016/S0955-2219(99)00200-9 ↗
4. A. Ravikiran, “Effect of interphase layers formed during dry sliding of zirconia toughened alumina against steel,” Wear, 171, 129–134 (1994).10.1016/0043-1648(94)90345-X ↗
5. B. R. lawn, Fracture of Brittle Solids, 2nd Ed., Cambridge Univ. Press, Cambridge (1993).10.1017/CBO9780511623127 ↗
6. V. A. Lavrenko, A. D. Panasyuk, M. Desmaison-Brut, and J. Desmaison, “Development of AlN-(TiCr)B2 ceramics and study of their corrosion resistance in air up to 1550°C,” Key Eng. Mat., 206-213, 1069–1072 (2002).
7. A. D. Verkhoturov, I. A. Podchernyaeva, and F. F. Egorov, Electrode Materials for Electric-Arc Alloying [in Russian], Nauka, Moscow (1988).
8. R. A. Andrievskii, V. A. Lavrenko, J. Desmaison, et al., “High-temperature oxidation of films based on aluminum nitride,” Dokl. RAN, 373, No. 1, 60–62 (2000).