Abstract

The high-temperature (to 1450°C) oxidation of AlN-ZrB2-ZrSi2 powders and compact ceramic materials with different contents of ZrB2-ZrSi2 solid solution in air is examined using scanning electron microscopy and differential thermal, thermogravimetric, x-ray phase, and x-ray spectrum microanalyses. It is established that the hot-pressed (practically porousless) ceramic materials have high corrosion resistance up to 1350–1400°C when scale components (individual oxides) interact with each other to form solid solutions based on aluminum oxide, zirconium oxide, and aluminum borate. These phases become sintered in the presence of the liquid B2O3 phase, self-reinforced scale being formed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Yu. G. Gogotsi and V. A. Lavrenko, Corrosion of High-Performance Ceramics, Springer-Verlag, Berlin (1992), p. 181.10.1007/978-3-642-77390-7 ↗
2. Yu. G. Gogotsi, J. Desmaison, R. A. Andrievski, et al., “AlN-based ceramics —an alternative to Si3N4 and SiC in high-temperature applications,” Key Eng. Mat., 132–136, 1600–1603 (1997).10.4028/www.scientific.net/KEM.132-136.1600 ↗
3. V. A. Lavrenko, T. V. Mosina, O. N. Grigor’ev, et al., “High-temperature oxidation of TiN-AlN powders and composites,” Dokl. AN Ukrainy, No. 12, 139–143 (1997).
4. V. A. Lavrenko, M. Desmaison-Brut, A. D. Panasyuk, and J. Desmaison, “Features of corrosion resistance of AlN-SiC ceramics in air up to 1600°C,” J. Europ. Ceram. Soc., 18, 2339–2343 (1998).10.1016/S0955-2219(98)00240-4 ↗
5. V. A. Lavrenko, “Reaction of composite ceramic materials with corrosionally active media,” Powder Metall. Met. Ceram., 39, No. 7–8, 369–380 (2000).10.1023/A:1026665523478 ↗
6. V. A. Lavrenko, J. Desmaison, A. D. Panasyuk, and M. Desmaison-Brut, “Oxidation resistance of AlN-(TiB2-TiSi2) ceramics in air up to 1450°C,” J. Europ. Ceram. Soc., 23, 357–369 (2003).10.1016/S0955-2219(02)00181-4 ↗
7. A. D. Panasyuk, V. A. Lavrenko, M. Desmaison-Brut, and J. Desmaison, “Development of AlN-(Ti, Cr)B2 composite ceramics and study of their corrosion resistance in air up to 1550°C,” Key Eng. Mat., 206-213, 1069–1072 (2002).10.4028/www.scientific.net/KEM.206-213.1069 ↗
8. R. A. Andrievskii, V. A. Lavrenko, J. Desmaison, et al., “High-temperature oxidation of films based on aluminum nitride,” Dokl. RAN, 373, No. 1, 60–62 (2000).
9. V. A. Lavrenko, D. Baxter, A. D. Panasyuk, and M. Desmaison-Brut, “Corrosion of ceramic composites in the AlN-SiC system in air and in combustion products of kerosene and diesel fuel,” Powder Metall. Met. Ceram., 43, No. 3–4, 179–186 (2004).10.1023/B:PMMC.0000035707.58363.f5 ↗
10. V. A. Lavrenko, A. D. Panasyuk, M. Desmaison-Brut, et al., “Corrosion of ceramic composites in the AlN-SiC-TiB2 system in air and in combustion products of kerosene and diesel fuel,” Powder Metall. Met. Ceram., 43, No. 5–6, 295–304.10.1023/B:PMMC.0000042466.23104.b9 ↗
11. S. V. Schneider, M. Desmaison-Brut, Yu. G. Gogotsi, and J. Desmaison, “Oxidation behavior of hot isostatically pressed TiB2-AlN composite,” Key Eng. Mat., 113, 49–58 (1996).10.4028/www.scientific.net/KEM.113.49 ↗