journal article·2003-11

Hard Alloy WC – 24% Ni Obtained in the Solid Phase from Ultrafine WC, NiO, and C Powders. Part 1. Density and Structure of Specimens

Anatolii V. Laptev, Alexander I. Tolochin, Larisa F. Ochkas

Powder Metallurgy and Metal Ceramics· Volume 42· Issue 11-12
Publisher page

Abstract

We have studied the density and structure of specimens of the alloy WC – 24 mass% Ni, obtained by combining into one step the processes of synthesis of the metallic phase and compaction of the ultrafine mixture of WC – Ni powders by high-energy pressing and sintering. We have established that reduction of nickel monoxide by carbon occurs at temperatures of 650-750°C and does not affect the shrinkage process which in the case of sintering begins only at a temperature of 1050°C. High-energy pressing of briquettes sintered at the indicated temperature reduces their porosity from 30-25% down to 8-4%. Specimens of porosity <1% can be obtained by pressing at 1150°C or 1050°C in the case of triple pressing. Raising the temperature at which the briquettes are heated is accompanied by enlargement of the pores together with a decrease in the total porosity, but at temperatures of 1300°C (sintering) and 1250°C (pressing), the pore dimensions are sharply reduced. The high density of the specimens pressed at low temperature does not provide low electrical resistance, which suggests the presence of weakly connected boundaries. When the specimens are sintered and pressed in the solid phase, we observe the growth of tungsten carbide particles. It is most rapid at 1150-1250°C, while at 1050°C the particle growth process slows down. Reduction of the metal oxide when the powders are heated promotes formation of structure in the higher temperature range.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. W. D. Schubert, H. Neumeister, G. Kinger, and B. Lux, “Hardness to toughness relationship of fine-grained WC-Co hard metals,” in: Proceedings of the Fourteenth International Plansee Seminar (May 12-16, 1997, Reutte, Tirol, Austria), Reutte, Tirol (1997), Vol. 4, pp. 249-264.
2. K. Jia, T. E. Fischer, and B. Gallois, “Microstructure, hardness and toughness of nanostructured and conventional WC-Co composites,” Nanostructured Mat., 10, No. 5, 875-891 (1998).10.1016/S0965-9773(98)00123-8 ↗
3. G. Gille, B. Szesny, K. Dreyer, H. Van Den Berg, et al., “Submicron and ultrafine grained hardmetal for microdrills and metal cutting insert,” in: Proceedings of the Fifteenth International Plansee Seminar (May 27-June 1, 2001, Reutte, Tirol, Austria), Reutte, Tirol (2001), Vol. 2, pp. 782-816.
4. S. I. Cha, S. H. Hong, G. H. Ha, and B. K. Kim, “Microstructure and mechanical properties of ultrafine WC-10 Co hardmetals,” in: Proceedings of the Fifteenth International Plansee Seminar (May 27-June 1, 2001, Reutte, Tirol, Austria), Reutte, Tirol (2001), Vol. 2, pp. 119-130.
5. M. T. Laugier, “The distribution of WC grain size and cobalt spacing in some WC-Co composites,” J. Mat. Sci. Lett., No. 5, 168-170 (1986).10.1007/BF01672037 ↗
6. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Characteristic features of the structure and properties of the alloy WC-16% Co obtained by hot pressing in solid and liquid phases. I. Effect of the temperature at which the specimens are obtained on their density and structure,” Poroshk. Metall., Nos. 11-12, 103-116 (2000).
7. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Characteristic features of the structure and properties of the alloy WC-16% Co obtained by hot pressing in solid and liquid phases. II. Effect of the temperature at which the specimens are obtained on their physical and mechanical properties,” Poroshk. Metall., Nos. 1-2, 100-109 (2001).
8. A. V. Laptev and S. S. Ponomarev, “Features of structure and mechanical properties of hard metal produced by low-temperature pressing of submicron WC-Ni powder,” in: Proceedings of the1998 Powder Metallurgy World Congress and Exhibition (October 18-22, 1998, Granada, Spain), Granada (1998), Vol. 4, pp. 223-228.
9. A. V. Laptev and S. S. Ponomarev, “Behavior of ultrafine powders of iron-block metals produced by salt pyrolysis during low-temperature pressing,” in: Proceedings of the1998 Powder Metallurgy World Congress and Exhibition (October 18-22, 1998, Granada, Spain), Granada (1998), Vol. 1, pp. 602-608.
10. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Study of possibility of solid phase producing poreless WC-26% Co hard metal at high energy pressing,” in: Proceedings, EURO PM'99 Conference on Advances in Hard Materials Production (November 8-10, 1999, Turin, Italy), Turin (1999), pp. 205-212.
11. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Solid phase consolidation fine grained WC-16 wt.% Co hard metals,” J. Adv. Mat., 33, No. 3, 42-51 (2001).
12. A. V. Laptev, “Possibilities of the method of high-energy hot pressing under vacuum for creating materials with ultrafine structure and high porosity,” Poroshk. Metall., Nos. 3-4, 8-19 (2001).
13. Production of Sintered Alloys, Pat. 520139 German, Publ. March 30 (1932).
14. Nobuhiro Kuribayashi, Koji Ueda, Keniti Wakana, et al., Method for Obtaining a Hard Alloy Based on Nickel Binder, Pat. Appl. 91-197627 Jpn., Publ. August 29 (1991).
15. M. E. Shaffer and E. R. Kimmerl, Method for Preparation of WC-Ni Grade Powder, Pat. 5057147 US, Publ. October 15 (1991).
16. U. Kuniaki, F. Koichi, and O. J. Takeo, “Characteristics of WC-Co alloys made from directly carburized powders of (WO3-C-Co3O4) mixtures,” Jpn. Inst. Metals, 43, No. 10, 895-900 (1979).10.2320/jinstmet1952.43.10_895 ↗
17. U. Kuniaki and F. J. Koichi, “Behavior of C on the formation process of WC from the mixed powder of WO3, Co3O4 and C,” Jpn. Inst. Metals, 43, No. 10, 890-895 (1979).10.2320/jinstmet1952.43.10_890 ↗
18. V. V. Sverdel, A. V. Shatov, N. A. Yurchuk, and O. V. Bakun, “Finely dispersed hard WC-Ni alloys. I. Mechanical properties,” Poroshk. Metall., Nos. 1-2, 73-76 (1994).
19. M. S. Koval'chenko, A. V. Laptev, V. V. Sverdel, and N. A. Yurchuk, “Effect of geometric parameters of the structure on the strength properties of hard alloys based on titanium carbide,” Poroshk. Metall., Nos. 3-4, 83-85 (1995).
20. A. V. Laptev and L. F. Ochkas, “Study of solid-phase consolidation of ultrafine grained WC-26% Ni hardmetal during high-energy hot pressing,” in: Proceedings of the European Congress PM2001 (October 21-23, 2001, Nice, France), Nice (2001), Vol. 1, pp. 187-193.
21. A. K. Ashin, S. T. Rostovtsev, and O. L. Kostelov, “Reduction of nickel monoxide by carbon,” in: Reductive Processes in Ferroalloy Production [in Russian], Nauka, Moscow (1977), pp. 178-182.
22. M. G. Zhuravleva and G. I. Chufarov, “Reduction of nickel monoxide and cobalt monoxide by graphite,” Tr. Inst. Metallurgii Ural. Fil. Akad. Nauk SSSR, No. 3, 63-66 (1959).