New structural unidirectional-fiber material
Source abstract
Abstract
Structural basaltic materials are analyzed to establish the relationship of their structure to strength and fracture resistance. It is shown that their strength is determined by the size of initial crack-like defects, and fracture resistance by the amount and extent of weak boundaries that are perpendicular to the growing main crack. Samples of one-component unidirectional basalt fiber material of channel structure were produced by hot pressing. It is shown how temperature and time under pressure influence the structure and fracture behavior of the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Geotechnical and Geomechanical Engineering · Powder Metallurgy Techniques and Materials · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Pelikan, Fused Stones [Russian translation], Metallurgizdat, Moscow (1959).
2. G. F. Gorbachev, S. G. Ivanitskii, and V. P. Sergeev, “Studying the thermophysical and mechanical properties of basalt fibers used as reinforcement of structural materials,” Promyshl. Teplotekhn., 23, No. 4– 5, 146–148 (2001).
3. Bykov and M. M. Krasnoshchekov, “Influence of the structure of stonecast materials on bending strength,” Steklo Keram., No. 7, 316–319 (1991).
4. F. Beloivan, I. I. Bykov, and A. N. Pilyankevich, “Effect of scale and temperature dependence of the strength of basalt stone castings,” Strength Mater., 1, No. 5, 519–522 (1969).10.1007/BF01802436 ↗
5. J.-S. Wang, J.-D. Kim, and H.-J. Yoon, “Mechanical characteristics of fused cast basalt tube encased in steel pipe for protecting steel surface,” Trans. Nonferrous Met. Soc. China, 19, 935–940 (2009).10.1016/S1003-6326(08)60381-7 ↗
6. V. P. Sergeev, Yu. N. Chuvashov, O. V. Galushchak, et al., “Basalt fibers—A reinforcing filler for composites,” Powder Metal. Met. Ceram., 33, No. 9–10, 555–557 (1995).10.1007/BF00559548 ↗
7. ASTM. Standard Methods of Fire Test of Building Construction and Materials, ASTM E119-05a, American Society for Testing and Materials, West Conshohocken, PA (2005).
8. CAN/ULC. Standard Methods of Fire Endurance Tests of Building Construction and Materials, CAN/ULC S101-04, Underwriters’ Laboratories of Canada Scarborough, ON (2004).
9. ASCE. Manuals and Reports on Engineering Practice No. 78: Structural Fire Protection, American Society of Civil Engineers, New York (1992).
10. R. Akisanya, A. C. F. Cocks, and N. A. Fleck, “Hydrostatic compaction of cylindrical particles,” J. Mech. Phys. Sol., 42, No. 7, 1067–1085 (1994).10.1016/0022-5096(94)90060-4 ↗
11. V. G. Borovik, “Modeling the formation of internal boundaries in an unidirectional fiber strand compacted in plastic state,” Powder Metal. Met. Ceram., 48, No. 7–8, 388–395 (2009).10.1007/s11106-009-9154-3 ↗
12. V. G. Borovik, “Morphological characteristics of contacts between fibers obtained by modeling their plastic pressing with allowance for friction,” in: Mathematical Models and Computational Experiments in Materials Science [in Russian], Issue 11, Inst. Probl. Materialoved. NAN Ukrainy, Kyiv (2009), pp. 55–64.
13. V. G. Borovik, “Modeling the effective elastic properties of materials pressed from a unidirectional hexagonal fiber strand,” Powder Metal. Met. Ceram., 49, No. 1–2, 8–16 (2010).10.1007/s11106-010-9195-7 ↗
14. V. G. Borovik, “Local stress intensity factors for cracks in a material with parallel channels of various cross-section,” in: Mathematical Models and Computational Experiments in Materials Science [in Russian], Issue 12, Inst. Probl. Materialoved. NAN Ukrainy, Kyiv (2010), pp. 48–57.
15. T. Ishikawa, S. Kajii, K. Matsunaga, et al., “Tough, thermally conductive silicon carbide composite with high strength up to 1600°C in air,” Science, 282, No. 5392, 1295–1297 (1998).10.1126/science.282.5392.1295 ↗