Structure and properties of WC-Co alloys in solid-phase sintering. II. Mechanical properties of samples
Source abstract
Abstract
The mechanical properties of hard WC-Co alloys produced by solid-phase sintering at various temperatures are discussed. It is shown that the bending strength and hardness of these alloys may be the same as those achieved in liquid-phase sintering. The difference between solid-phase and liquid-phase sintering is only in the time it takes to achieve the dense state. Excellent mechanical properties at rather low temperatures (1150–1200 °C) can be obtained by sintering under pressure. High hardness can be achieved at 1000–1100 °C by hot isostatic pressing of nanoscale powders. The excellent mechanical properties of solid-phase-sintered hard WC-Co alloys indicate that strong interphase and intercarbide boundaries occur earlier than the liquid phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. A. V. Laptev, “Structure and properties of WC-Co alloys in solid-phase sintering. I. Geometrical evolution,” Powder Metall. Met. Ceram., 46, No. 9–10, 415–422 (2007).10.1007/s11106-007-0065-x ↗
2. A. V. Laptev, “Densification of WC-Co alloys in solid-phase sintering (review),” Powder Metall. Met. Ceram., 46, No. 7–8, 317–324 (2007).10.1007/s11106-007-0051-3 ↗
3. I. N. Chaporova and K. S. Chernyavskii, Structure of Sintered Hard Alloys [in Russian], Metallurgiya, Moscow (1975).
4. M. M. Babich, Carbon Inhomogeneity of Hard Alloys and Its Elimination [in Russian], Naukova Dumka, Kiev (1975).
5. R. F. Snowball and D. R. Milner, “Densification processes in the tungsten carbide-cobalt system,” Powder Metall., 11, No. 21, 23–40 (1968).10.1179/pom.1968.11.21.002 ↗
6. C. Colin, L. Durant, N. Favrot, et al., “Comparative study of the densification and properties of WC-Co cermets processed by Liquid phase sintering and solid state sintering,” in: H. Bildstein and R. Eck (eds.), Proc. 13th Int. Plansee Seminar, Metallwerk Plansee, Reutte, Vol. 2, 505–521 (1993).
7. I. L. Chermant and F. J. Osterstock, “Fracture toughness and fracture of WC-Co composites,” J. Mat. Sci., 11, No. 2, 1939–1951 (1976).10.1007/BF00708272 ↗
8. M. G. Loshak, Strength and Life of Hard Alloys [in Russian], Naukova Dumka, Kiev (1984).
9. N. Tsuchiya, M. Fukuda, T. Nakai, and H. Suzuki, “Some properties of WC-Co alloy prepared by solid-phase sintering,” J. Jap. Soc. Powd. Powd. Metallurgy, 37, No. 8, 1177–1180 (1990).10.2497/jjspm.37.1177 ↗
10. J. Azcona, A. Ordonez, L. Dominguez, et al., “Hot isostatic pressing of nanosized WC-Co hardmetals,” in: Proc. 15th Int. Plansee Seminar, Reutte, Vol. 2 (2001), pp. 35–49.
11. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Structural features and properties of alloy 84% WC-16% Co, obtained by hot pressing in the solid and liquid phases. Part 2. Influence of the temperature at which the specimens are made on their physicomechanical properties,” Powder Metall. Met. Ceram., 40, No. 1–2, 77–83 (2001).10.1023/A:1011368124481 ↗
12. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Solid phase consolidation fine grained WC-16 wt.% Co hard metals,” J. Adv. Mat., 33, No. 3, 42–51 (2001).
13. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Study of possibility of solid phase producing poreless WC-26% Co hard metal at high energy pressing,” in: Proc. EURO PM’99 Conf. on Advances in Hard Materials Production (November 8–10, 1999, Turin, Italy), Turin (1999), pp. 205–212.
14. A. V. Laptev, “Potential of the high-energy hot compaction in a vacuum for creating materials with an ultrafine structure and high strength,” Powder Metall. Met. Ceram., 40, No. 3–4, 103–111 (2001).10.1023/A:1011963019060 ↗
15. G. A. Bovkun and A. V. Laptev, “Relationship between erosion and mechanical characteristics of fine-grained hard alloy WC-16% Co obtained by solid-phase and liquid-phase consolidation. Part 1. Erosion resistance,” Powder Metall. Met. Ceram., 43, No. 5–6, 265–272 (2004).10.1023/B:PMMC.0000042461.02431.22 ↗
16. S. S. Gorelik, V. P. Elyutin, E. I. Mozzhuhin, et al., “Radiographic study of processes of recrystallization boridov the titan, zirconium and molybdenum and carbides of the titan and tungsten,” Izv. VUZov, Tsvetn. Metallurgiya, No. 4, 143–148 (1962).
17. S. Roure and J.-M. Missiaen, “Macroscopic and microstructural evolution of WC-Co compacts during solid state sintering,” in: Proc. EURO PM’96, Stockholm (1986), pp. 77–84.
18. O. Lavergne, F. Hodaj, and C. H. Allibert, “Solid state dissolution behavior of WC in Co binder,” in: Proc. EURO PM’96, Stockholm (1986), pp. 153–158.
19. T. V. Gorbachova and I. N. Chaporova, “Influence of cobalt on the fine structure of the WC-phase formed in an alloy,” Sb. Tr. VNIITS, No. 18, 51–54 (1978).
20. I. N. Chaporova, T. B. Gorbachova, V. A. Ivensen, et al., “Change of the fine structure of the WC phase in sintering of tungsten-cobalt alloys,” Sb. Tr. VNIITS, No. 16, 163–172 (1976).
21. V. V. Skorokhod and S. M. Solonin, Physical and Metallurgical Fundamentals of Powder Sintering [in Russian], Metallurgiya, Moscow (1984).
22. V. V. Panichkina, V. V. Skorokhod, and A. F. Khrienko, “Activated sintering of tungsten and molybdenum powders,” Powder Metall. Met. Ceram., 6, No. 7, 558–560 (1967).10.1007/BF00774073 ↗