Abstract

The effect of silicon, germanium, tin (X), and aluminum on the structure, physicochemical and mechanical properties of Ti-B-X and Ti-Al-B (5 and 7.5 at.% B) ternary and Ti-Al-B-X and Ti-Zr-Al-B (9 at.% Al and 5 at.% B; 8.5 at.% Al and 7.5 at.% B) quaternary alloys is studied by metallography, scanning electron microscopy (SEM), X-ray diffraction, differential thermal analysis (DTA), microhardness measurements, Vickers hardness measurements (from room temperature to 900°C), bending tests (room temperature), and compression tests (from room temperature to 700°C). The alloys are melted in an arc furnace from pure materials. Doping with p-elements (Al, Si, Ge, and Sn) does not change the specific titanium-boride eutectic structure in the two-phase (Ti) + TiB field. The doping additions hardly change the chemical composition of the eutectic and only decrease the boron content by 1–2 at.%. The Al, Si, Ge, and Sn (p-elements) are not soluble in TiB titanium borides and completely concentrate in the metal matrix in two-phase (Ti) + TiB alloys. The temperature of incipient sharp softening is shown to be exclusively connected with the matrix composition. It is determined that p-elements increase the hardness and strength of titanium-boride eutectic alloys in the entire temperature range of interest and increase the temperature of incipient sharp softening from 500 to 600-650°C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. T. V. Massalski, P. R. Subramanian, H. Okomoto, et al., Binary Alloy Phase Diagrams: Handbook, in 3 Vols., 2nd ed., ASM International, Materials Park, Ohio (1990), p. 3589.
2. J. L. Murray, P. K. Liao, and K. E. Spear, “The B-Ti (boron-titanium) system,” Bull. Alloy Phase Equilib., 7, No. 6, 550–555 (1986).10.1007/BF02869864 ↗
3. J. L. Murray, P. K. Liao, and K. E. Spear, “The B-Ti (boron-titanium) system,” in: J. L. Murray, Phase Diagrams of Binary Titanium Alloys, ASM International, Materials Park, Ohio (1987), pp. 33–38.
4. M. de Graef, J. P. A. Löfvander, C. McCollough, et al., “The evolution of metastable Bf borides in a Ti-Al- B alloy,” Acta Metall. Mater., 40, No. 12, 3395–3406 (1992).10.1016/0956-7151(92)90053-H ↗
5. J. Braun and M. Ellner, “On the partial atomic volume of aluminum in the titanium-rich phases of the binary system Ti-Al,” Z. Metallkd., 91, No. 5, 389–392 (2000).
6. J. Braun and M. Ellner, “Phase equilibria investigations on the aluminum rich part of the binary system Ti-Al,” Metall. Mater. Trans. A, 32A, 1037–1048 (2001).10.1007/s11661-001-0114-x ↗
7. P. Villars and L. D. Calvert (eds.), Pearson’s Handbook of Crystallographic Data for Intermetallic Phases, in 4 Vols., 2nd ed., ASM International, Materials Park, Ohio (1991).
8. J. J. Williams, M. J. Kramer, M. Akinc, et al., “Effects of interstitial additions on the structure of Ti5Si3,” J. Mater. Res., 15, No. 8, 1773–1779 (2000).10.1557/JMR.2000.0256 ↗
9. J. J. Williams, M. J. Kramer, and S. K. Akinc, “Thermal expansion of Ti5Si3 with Ge, B, C, N, or O additions,” J. Mater. Res., 15, No. 8, 1780 (2000).10.1557/JMR.2000.0257 ↗
10. J. J. Williams, Y. Y. Ye, M. J. Kramer, et al., “Theoretical calculations and experimental measurements of the structure of Ti5Si3 with interstitial additions,” Intermetallics, 8, 937–943 (2000).10.1016/S0966-9795(00)00064-9 ↗
11. A. S. Ramos, C. A. Nunes, G. Rodrigues, et al., “Ti6S12B, a new ternary phase in the Ti-Si-B system,” Intermetallics, 12, No. 5, 487–491 (2004).10.1016/j.intermet.2004.01.001 ↗
12. T. Ya. Velikanova, A. A. Bondar, L. V. Artyukh, et al., “Titanium-boride composites: Influence of alloying on constitution and properties of titanium-boride eutectic alloys,” in: O. N. Senkov, D. B. Miracle, and S. O. Firstov (eds.), Metallic Materials with High Structural Efficiency, Kluwer Academic Publishers, Dordrecht−Boston−London (2004), pp. 259–268.10.1007/1-4020-2112-7_27 ↗
13. G. Rodrigues, C. A. Nunes, P. A. Suzuki, et al., “Thermal expansion of the Ti5Si3 and Ti6Si2B phases investigated by high-temperature X-ray diffraction,” Intermetallics, 14, No. 3, 236–240 (2006).10.1016/j.intermet.2005.05.007 ↗
14. J. L. Murray (ed.), “The Ge-Ti (germanium-titanium) system,” in: Phase Diagrams of Binary Titanium Alloys, ASM International, Materials Park, Ohio (1987), pp. 118–122.
15. S. Gorsse and D. B. Miracle, “Mechanical properties of Ti-6Al-4 V/TiB composites with randomly oriented and aligned TiB reinforcements,” Acta Mater., 51, No. 9, 2427–2442 (2003).10.1016/S1359-6454(02)00510-4 ↗
16. S. Gorsse, Y. Le Petitcorps, S. Matar, et al., “Investigation of the Young’s modulus of TiB needles in situ produced in titanium matrix composite,” Mater. Sci. Eng. A, A340, 80–87 (2003).10.1016/S0921-5093(02)00188-0 ↗
17. S. S. Sahay, K. S. Ravichandran, and R. Atri, “Evolution of microstructure and phases in in situ processed Ti-TiB composites containing high volume fractions of TiB whickers,” J. Mater. Res., 14, No. 11, 4214-4223 (1999).10.1557/JMR.1999.0571 ↗
18. M. Kobayashi, K. Funami, S. Suzuki, et al., “Manufacturing process and mechanical properties of fine TiB dispersed Ti-6Al-4 V alloy composites obtained by reaction sintering,” Mater. Sci. Eng. A, A243, 279–284 (1998).10.1016/S0921-5093(97)00814-9 ↗
19. Z. Fan, H. J. Niu, A. P. Miodownik, et al., “Microstructure and mechanical properties of in situ Ti/TiB MMCs produced by a blended elemental powder metallurgy method,” Key Eng. Mater., 127–131, 423–430 (1997).10.4028/www.scientific.net/KEM.127-131.423 ↗
20. T. Saito, T. Furuta, and T. Yamaguchi, “Development of low cost titanium matrix composite,” in: P. A. Blenkinsop, W. J. Evans, and H. M. Flower (eds.), Titanium‘95 Science and Technology, Vol. 3, The Institute of Materials, London (1996), pp. 2859–2870.
21. T. Saito, T. Furuta, and T. Yamaguchi, “Development of low cost titanium matrix composite,” in: Recent Advances in Titanium Metal Matrix Composites, The Minerals Metals & Materials Society, Warrendale, Pennsylvania, USA (1995), pp. 33–44.
22. W. O. Soboyejo, R. J. Lederich, and S. M. L. Sastry, “Recent advances in the development of damage tolerant in-situ titanium matrix composites,” in: Proc. Conf. Advanced Metal Matrix Composites for Elevated Temperatures, Cincinnati, Ohio (1991), pp. 85–93.
23. Z. Fan and A. P. Miodownik, “The Young’s moduli of in-situ Ti/TiB composites obtained by rapid solidification processing,” J. Mater. Sci., 29, 1127–1134 (1994).10.1007/BF00351442 ↗
24. W. O. Soboyejo, R. J. Lederich, and S. M. L. Sastry, “Mechanical behavior of damage tolerant TiB whisker-reinforced in situ titanium matrix composites,” Acta Metall. Mater., 42, No. 8, 2579–2591 (1994).10.1016/0956-7151(94)90199-6 ↗
25. T. M. T. Godfrey, A. Wisbey, P. S. Godwin, et al., “Microstructure and tensile properties of mechanically alloyed Ti-6Al-4 V with boron additions,” Mater. Sci. Eng. A, A282, 240–250 (2000).10.1016/S0921-5093(99)00699-1 ↗
26. T. Yamamoto, A. Otsuki, K. Ishihara, et al., “Synthesis of near net shape high density TiB/Ti composite,” Mater. Sci. Eng. A, 239–240, 647–651 (1997).10.1016/S0921-5093(97)00643-6 ↗
27. R. Banerjee, P. C. Collins, A. Genc, et al., “Direct laser deposition of in situ Ti-6Al-4 V-TiB composites,” Mater. Sci. Eng. A, A358, 343–349 (2003).10.1016/S0921-5093(03)00299-5 ↗
28. T. S. Srivatsan, W. O. Soboyejo, and R. J. Lederich, “Tensile deformation and fracture behavior of a titanium-alloy metal-matrix composite,” Composites Part A. Appl. Sci. Manuf., 28A, No. 4, 365–376 (1997).10.1016/S1359-835X(96)00136-4 ↗
29. O. N. Senkov, D. B. Miracle, and S. O. Firstov (eds.), “The main tendencies in elaboration of materials with high specific strength,” in: Metallic Materials with High Structural Efficiency, Kluwer Academic Publishers, Dordrecht (2004), pp. 33–44.
30. N. P. Lyakishev (ed.), Phase Diagrams of Binary Systems: Handbook [in Russian], in 3 Vols., Vol. 1, Mashinostroenie, Moscow (1996), p. 992.
31. V. T. Witusiewicz, A. A. Bondar, U. Hecht, et al., “The Al-B-Nb-Ti system. II. Thermodynamic description of the constituent ternary system B-Nb-Ti,” J. Alloys Compd., 456, 143–150 (2008).10.1016/j.jallcom.2007.02.030 ↗
32. V. T. Witusiewicz, A. A. Bondar, U. Hecht, et al., “The Al-B-Nb-Ti system. V. Thermodynamic description of the ternary system Al-B-Ti,” J. Alloys Compd., 474, No. 1–2, 86–104 (2009).10.1016/j.jallcom.2008.06.128 ↗
33. A. Bondar, T. Velikanova, and G. Effenberg, “Boron-silicon-titanium,” in: Landolt-Börnstein, Numerical Data and Functional Relationships in Science and Technology, W. Martinsen (ed.), New Series. Group IV: Physical Chemistry, G. Effenberg and S. Ilyenko (eds.), Ternary Alloy Systems, Phase Diagrams, Crystallographic and Thermodynamic Data Critically Evaluated by MSIT, Vol. 11E2, Springer-Verlag, Berlin, Heidelberg (2010), pp. 179–193.
34. D. B. Borisov, O. S. Fomichev, A. A. Bondar, et al., “Phase equilibria in the Ti-Ge-B system in the range of the Ti6Ge2B ternary phase,” in: V. V. Skorokhod (ed.), Current Issues of Materials Physics. Ser. Physicochemical Fundamentals of Powder Material Technology [in Russian], Inst. Probl. Materialoved. NAN Ukrainy, Kiev (2005), pp. 42–46.
35. D. B. Borisov, L. V. Artyukh, A. A. Bondar, et al., “Titanium-boride eutectic materials: Structure of titanium-rich Ti-Ge-B alloys and phase equilibria at crystallization temperatures,” Powder Metall. Met. Ceram., 46, No. 3–4, 153–162 (2007).10.1007/s11106-007-0025-5 ↗
36. A. A. Bondar, T. Ya. Velikanova, D. B. Borysov, et al.,“Titanium-boride eutectic materials: Phase equilibria and properties of alloys in the Ti-rich portion of the Ti-Sn-B system,” J. Alloys Compd., 400, No. 1–2, 202–208 (2005).10.1016/j.jallcom.2005.04.010 ↗
37. V. I. Trefilov, Yu. V. Mil’man, and S. A. Firstov, Physical Fundamentals of Strength of Refractory Metals [in Russian], Naukova Dumka, Kiev (1975), p. 315.
38. V. A. Borisenko, “General trends of temperature dependence of mechanical properties of refractory materials,” Probl. Prochn., No. 8, 58–63 (1975).
39. R. Hill, The Mathematical Theory of Plasticity, Oxford University Press Inc., New York (1998), p. 355.10.1093/oso/9780198503675.001.0001 ↗
40. V. A. Borisenko, Hardness and Strength of Refractory Materials at High Temperatures [in Russian], Naukova Dumka, Kiev (1984), p. 211.
41. O. O. Bilous, N. I. Tsyganenko, M. P. Burka, et al.,“Titanium-boride eutectic materials: effects of vanadium and niobium on high-temperature strength,” High Temp. Mater. Processes, 83–96 (2005).
42. O. M. Ivasishin, V. I. Bondarchuk, I. V. Moiseeva, et al., “Temperature dependence of activation energy of deformation of near-α, (α + β) and near-β titanium alloys,” Metallofiz. Noveish. Tekhnol., 21, No. 2, 117-121 (1999).
43. O. M. Ivasishin, V. I. Bondarchuk, I. V. Moiseeva, et al., “Temperature dependence of activation energy of deformation of near-α, (α + β) and near-β titanium alloys,” Mater. Phys. Adv. Tech., 19, 397–404 (2001).