journal article·2019-07

Formation of Phases in the FePt/Au/FePt Films and their Magnetic Properties

P. V. Makushko, M. Yu. Verbytska, M. N. Shamis, A. P. Burmak, Ya. A. Berezniak, K. A. Graivoronska, T. I. Verbytska, Yu. N. Makogon

Powder Metallurgy and Metal Ceramics· Volume 58· Issue 3-4
Publisher page

Abstract

The effect of annealing atmosphere (vacuum, hydrogen) and intermediate Au layer thickness on the formation of a magnetically hard L10 phase and the magnetic properties of Fe50Pt50(15 nm)/Au(7.5, 30 nm)/Fe50Pt50(15 nm) films deposited by magnetron sputtering onto SiO2(100 nm)/Si(001) substrates was studied. Samples were heat-treated in a hydrogen atmosphere at 100 kPa. The disordered A1-FePt phase formed in the as-deposited films. The ordered L10-FePt phase appeared in the film with an intermediate Au (7.5 nm) layer during vacuum annealing at 650°C. Increase in the intermediate Au layer thickness to 30 nm reduces the ordering temperature to 600°C. This is promoted by higher compressive stresses in the as-deposited Fe50Pt50 layers with a thicker Au interlayer. In hydrogen annealing, the A1 → L10-FePt phase transition in the Fe50Pt50(15 nm)/Au(7.5, 30 nm)/Fe50Pt50(15 nm) films starts at 500°C regardless of the intermediate Au layer thickness. The Au and FePt axial (111) textures are observed in the films annealed in hydrogen. This is more evident in the films with a thicker Au (30 nm) interlayer. The film with an intermediate Au (30 nm) layer shows 27.3 kOe coercivity after vacuum annealing at 900°C. The same coercivity can be achieved by hydrogen annealing at 700°C, which is 200°C lower than after vacuum annealing due to the introduction of hydrogen into voids of the L10-FePt lattice and increase of stresses.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic properties of thin films · Magnetic Properties and Applications · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. D. Weller, A. Moser, L. Folks, M.E. Best, W. Lee, M.F. Toney, M. Schickert, J.-U. Thiele, and M.F. Doemer, “High Ku materials approach to 100 Gbits = in2,” IEEE Trans. Magn., 36, 10–15 (2000).10.1109/20.824418 ↗
2. A.T. McCallum, P. Krone, F. Springer, C. Brombacher, M. Albrecht, E. Dobisz, M. Grobis, D. Weller, and O. Hellwig, “L10 FePt based exchange coupled composite bit patterned films,” Appl. Phys. Lett., 98, 242503 (2011), DOI: https://doi.org/10.1063/1.3599573 .10.1063/1.3599573 ↗
3. D. Weller, O. Mosendz, G. Parker, S. Pisana, and T.S. Santos, “L10 FePtX–Y media for heat-assisted magnetic recording,” Phys. Status Solidi A, 210, 1245 (2013), DOI: https://doi.org/10.1002/pssa.201329106 .10.1002/pssa.201329106 ↗
4. D. Weller, G. Parker, O. Mosendz, A. Lyberatos, D. Mitin, N.Y. Safonova, and M. Albrecht, “Review article: FePt heat assisted magnetic recording media,” J. Vac. Sci. Technol., B34, 060801 (2016), DOI: https://doi.org/10.1116/1.4965980 .10.1116/1.4965980 ↗
5. I.A. Vladymyrskyi, O.P. Pavlova, T.I. Verbitska, S.I. Sidorenko, G.L. Katona, D.L. Beke, and Iu.M. Makogon, “Influence of intermediate Ag layer on the structure and magnetic properties of Pt/Ag/Fe thin films,” Vacuum, 101, 33 (2014), DOI: https://doi.org/10.1016/j.vacuum.2013.07.018 .10.1016/j.vacuum.2013.07.018 ↗
6. O.P. Pavlova, T.I. Verbitska, I.A. Vladymyrskyi, S.I. Sidorenko, G.L. Katona, D.L. Beke, G. Beddies, M. Albrecht, and I.M. Makogon, “Structural and magnetic properties of annealed FePt/Ag/FePt thin films,” Appl. Surf. Sci., 266, 100 (2013), DOI: https://doi.org/10.1016/ j.apsusc.2012.11.102.
7. T. Maeda, T. Kai, A. Kikitsu, T. Nagase, and J. Akiyama, “Reduction of ordering temperature of a FePtordered alloy by addition of Cu,” Appl. Phys. Lett., 80, No. 12, 2147–2149 (2002), DOI: https://doi.org/10.1063/1.1463213 .10.1063/1.1463213 ↗
8. C. Feng, Q. Zhan, B. Li, J. Teng, M. Li, Y. Jiang, and G. Yu, “Magnetic properties and microstructure of FePt/Au multilayers with high perpendicular magnetocrystalline anisotropy,” Appl. Phys. Lett., 93, 152513 (2008), DOI: https://doi.org/10.1063/1.3001801 .10.1063/1.3001801 ↗
9. C. Feng, B.-H. Li, Y. Liu, J. Teng, M.-H. Li, Y. Jiang, and G.-H. Ya, “Improvement of magnetic property of L10-FePt film by FePt/Au multilayer structure,” J. Appl. Phys., 103, 023916 (2008), DOI: https://doi.org/10.1063/1.2828148 .10.1063/1.2828148 ↗
10. Y.S. Yu, H.-B. Li, W.L. Li, M. Liu, and W.D. Fei, “Structure and magnetic properties of magnetron sputtered [(Fe/Pt/Fe)/Au] n multilayer films,” J. Magn. Magn. Mater., 322, 1770 (2010), DOI: https://doi.org/10.1016/j.jmmm.2009.12.027 .10.1016/j.jmmm.2009.12.027 ↗
11. W.Y. Zhang, H. Shima, F. Takano, H. Akinaga, X.Z. Yu, T. Hara, W.Z. Zhang, K. Kimoto, Y. Matsui, and S. Nimori, “Enhancement in ordering of Fe50Pt50 film caused by Cr and Cu additives,” J. Appl. Phys., 106, 033907 (2009), DOI: https://doi.org/10.1063/1.3194313 .10.1063/1.3194313 ↗
12. C.L. Platt, K.W. Wierman, E.B. Svedberg, R. van de Veerdonk, J.K. Howard, A.G. Roy, and D.E. Laughlin, “L10 ordering and microstructure of FePt thin films with Cu, Ag and Au additive,” J. Appl. Phys., 92, No. 10, 6104–6108 (2002), DOI: https://doi.org/10.1063/1.1516870 .10.1063/1.1516870 ↗
13. Y.F. Ding, J.S. Chen, and E. Liu, “Epitaxial L10 FePt films on SrTiO3(100) by sputtering,” J. Cryst. Growth, 276, 111 (2005), DOI: https://doi.org/10.1016/j.jcrysgro.2004.10.154 .10.1016/j.jcrysgro.2004.10.154 ↗
14. M. Albrecht and C. Brombacher, “Rapid thermal annealing of FePt thin films,” Phys. Status Solidi A, 210, 1272 (2013), DOI: https://doi.org/10.1002/pssa.201228718 .10.1002/pssa.201228718 ↗
15. C.L. Zha, S.H. He, B. Ma, Z.Z. Zhang, F.X. Gan, and Q.Y. Jin, “Dependence of ordering kinetics of FePt thin films on different substrates,” IEEE Trans. Magn., 44, No. 11, 3539–3542 (2008), DOI: https://doi.org/10.1109/TMAG.2008.2001609 .10.1109/TMAG.2008.2001609 ↗
16. K.W. Wierman, C.L. Platt, J.K. Howard, and F.E. Spada, “Evolution of stress with L10 ordering in FePt and FeCuPt thin films,” J. Appl. Phys., 93, No. 10, 7160–7162 (2003), DOI: https://doi.org/10.1063/1.1555893 .10.1063/1.1555893 ↗
17. S.N. Hsiao, S.K. Chen, T.S. Chin, Y.W. Hsu, H.W. Huang, F.T. Yuan, H.Y. Lee, and W.M. Liao, “Earlystage ordering in in-situ annealed Fe51Pt49 films,” J. Magn. Magn. Mater., 321, 2459–2466 (2009), DOI: https://doi.org/10.1016/j.jmmm.2009.03.018 .10.1016/j.jmmm.2009.03.018 ↗
18. S.N. Hsiao, F.T. Yuan, H.W. Chang, H.W. Huang, S.K. Chen, and H.Y. Lee, “Effect of initial stress/strain state on order-disorder transformation of FePt thin films,” Appl. Phys. Lett., 94, 232505 (2009), DOI: https://doi.org/10.1063/1.3153513 .10.1063/1.3153513 ↗
19. F.T. Yuan, S.H. Liu, W.M. Liao, S.N. Hsiao, S.K. Chen, and H.Y. Lee, “Ordering transformation of FePt thin films by initial stress/strain control,” IEEE Trans. Magn., 48, No. 3, 1139–1142 (2012), DOI: https://doi.org/10.1109/TMAG.2011.217366010.1109/TMAG.2011.2173660 ↗
20. S.N. Hsiao, S.H. Liu, S.K. Chen, F.T. Yuan, and H.Y. Lee, “Effect of intrinsic tensile stress on (001) orientation in L10 FePt thin films on glass substrates,” J. Appl. Phys., 111, 07A702 (2012), DOI: https://doi.org/10.1063/1.3670515 .10.1063/1.3670515 ↗
21. C.H. Lai, C.H. Yang, C.C. Chiang, T. Balaji, and T.K. Tseng, “Dynamic stress-induced low-temperature ordering of FePt,” Appl. Phys. Lett., 85, 4430 (2004), DOI: https://doi.org/10.1063/1.1819985 .10.1063/1.1819985 ↗
22. S.N. Hsiao, S.K. Chen, S.H. Liu, C.J. Liao, F.T. Yuan, and H.Y. Lee, “Effect of annealing process on residual strain/stress behaviors in FePt thin films,” IEEE Trans. Magn., 47, No. 10, 3637–3640 (2011), DOI: https://doi.org/10.1109/TMAG.2011.2147291 .10.1109/TMAG.2011.2147291 ↗
23. S.N. Hsiao, S.H. Liu, S.K. Chen, T.S. Chin, and H.Y. Lee, “Direct evidence for stress-induced (001) anisotropy of rapid-annealed FePt thin films,” Appl. Phys. Lett., 100, 261909 (2012), DOI: https://doi.org/10.1063/1.4730963 .10.1063/1.4730963 ↗
24. J.-S. Kim, Y.-M. Koo, and N. Shin, “The effect of residual strain on (001) texture evolution in FePt thin films,” J. Appl. Phys., 100, 093909 (2006), DOI: https://doi.org/10.1063/1.2364051 .10.1063/1.2364051 ↗
25. J.-S. Kim, Y.-M. Koo, B.-J. Lee, and S.-R. Lee, “The origin of (001) texture evolution in FePt thin films on amorphous substrates,” J. Appl. Phys., 99, 053906 (2006), DOI: https://doi.org/10.1063/1.2176088 .10.1063/1.2176088 ↗
26. W. Hsu, S.K. Chen, W.M. Liao, F.T. Yuan, W.C. Chang, and J.L. Tsai, “Effect of Pt underlayer on the coercivity of FePt sputtered film,” J. Alloys Compd., 449, 52–55 (2008), DOI: https://doi.org/10.1016/j.jallcom.2006.01.113 .10.1016/j.jallcom.2006.01.113 ↗
27. T. Kamiki and S. Nagawa, “Fabrication of FePt ordered alloy films by annealing in hydrogen atmosphere,” J. Magn. Soc. Jpn., 28, No. 3, 330–334 (2004).10.3379/jmsjmag.28.330 ↗
28. T. Kitagawa, J. Ikemoto, T. Kamiki, and S. Nakagawa, “Effect of hydrogen to attain (001) oriented FePt ordered alloy films from Pt/Fe bilayers,” in: IEEE Int. Magn. Conference 2006, INTERMAG, San Diego, California (2006), pp. 476–476.
29. M. Yamauchi, K. Okubo, T. Tsukuda, K. Kato, M. Takata, and S. Takeda, “Hydrogen-induced structural transformation of AuCu nanoalloys probed by synchrotron X-ray diffraction techniques,” Nanoscale, 6, No. 8, 4067–4071 (2014).10.1039/C3NR06327E ↗
30. I.A. Vladymyrskyi, M.V. Karpets, F. Ganss, G.L. Katona, D.L. Beke, S.I. Sidorenko, T. Nagata, T. Nabatame, T. Chikyow, G. Beddies, M. Albrecht, and Iu.M. Makogon, “Influence of the annealingatmosphere on the structural properties of FePt thin films,” J. Appl. Phys., 114, 164314 (2013), DOI: https://doi.org/10.1063/1.4827202 .10.1063/1.4827202 ↗
31. M.Yu. Verbitska, M.N. Shamis, P.V. Makushko, Ya.O. Bereznyak, K.O. Graivoronska, T. I. Verbitska, and Iu.M. Makogon, “Formation of ordered L10-FePt phase in Fe50Pt50/Au/Fe50Pt50 films in hydrogen annealing,” Metallofiz. Noveish. Tekhnol., 40, No. 8, 1069–1079 (2018).10.15407/mfint.40.08.1069 ↗
32. V.E. Antonov, T.E. Antonova, I.T. Belash, A.E. Gorodetskii, and E.G. Ponyatovskii, “Production of gold hydrides at high hydrogen pressure,” Dokl. Akald. Nauk SSSR, 266, No. 2, 376–380 (1982).