Effect of Chromium Diboride Additives in Intermetallic Matrix on the Corrosion Resistance of NiAl–CrB2 Composites in Sea Water
Source abstract
Abstract
The effect of the amount of chromium diboride additives in the NiAl intermetallic alloy on the corrosion resistance of composites in a 3 % NaCl aqueous solution simulating sea water, using anodic polarization curves, is studied. It is demonstrated that the introduction of more corrosionresistant components (chromium diboride) into the NiAl intermetallic alloy has no significant effect on the durability of such composites in sea water. The basic mechanisms of corrosion in the developed composite materials in corrosive aqueous medium are established.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. A. A. Shokati, N. Parvin, and M. Shokati, “Combustion synthesis of NiAl matrix composite powder reinforced by TiB2 and TiN particulates from Ni–Al–Ti–BN reaction system,” J. All. Compd., 585, 637–643 (2014).10.1016/j.jallcom.2013.09.020 ↗
2. K. G. Kumar and T. J. Sahaya Anand, “A novel intermetallic nickel aluminide (Ni3Al) as alternative automotive body material,” Int. J. Engin. Technol., 11, No. 1, 274–283 (2011).10.7763/IJET.2011.V3.237 ↗
3. A. P. Umanskii, E. N. Polyarus, M. S. Ukrainets, et al., “Study on the structure and properties of the NiAl–TiB2 composite materials and the coatings based on them,” Aviats. Kosm. Tekh. Tekhnol., 107, No. 10, 20–24 (2013).
4. A. P. Umanskii, E. N. Polyarus, M. S. Ukrainets, et al., “Study on the structure, physical and chemical properties, and tribotechnical characteristics of NiAl–ZrB2 composites,” Sverkhtverd. Mater., No. 4, 53–62 (2015).
5. R. Darolia, D. F. Lahrman, and R. D. Field, “Ordered intermetallics,” Phys. Metal. Mechan. Behavior, 3, 679–698 (1992).
6. M. B. Henderson, J. Hannis, G. McColvin, et al., “Materials issues for the design of industrial gas turbines,” Minerals, Metals Mat. Soc., 3–13 (2002)
7. B. Movahedi, “Fracture toughness and wear behavior of NiAl-based nanocomposite HVOF coatings,” Surf. Coat. Technol., 235, 212–219 (2013).10.1016/j.surfcoat.2013.07.035 ↗
8. Y. Wang and W. Chen, “Microstructures, properties and high-temperature carburization resistances of HVOF thermal sprayed NiAl intermetallic-based alloy coatings,” Surf. Coat. Technol., 183, No. 1, 18–28 (2004).10.1016/j.surfcoat.2003.08.080 ↗
9. Klöwer, U. Brill, and U. Heubner, “High temperature corrosion behavior of nickel aluminides: effects of chromium and zirconium,” Intermetallics. 7, No. 10, 1189–1194 (1999).10.1016/S0966-9795(99)00042-4 ↗
10. M. Antonov, M. Stack, and I. Hussainova, “Erosion-corrosion of Cr3C2–Ni cermets in salt water,” Proc. Estonian Academy Sci. Engin., 12, 176–187 (2006).10.3176/eng.2006.3.02 ↗
11. O. Polyarus, V. Talash, O. Umanskii, et al., “The structure and anodic resistance of the NiAl–CrB2 composite material in 3% NaCl solution,” Fiz. Khim. Mekh. Mater., No. 10, 293–296 (2014).
12. R. S. Lillard and J. R. Scullu, “Electrochemical passivation of ordered NiAl,” J. Electrochem. Soc., 145, No. 6, 2024–2032 (1998).10.1149/1.1838593 ↗
13. S. Transatti and J. Ippolito, “Electrochemical behavior of nickel-aluminum alloys in sodium chloride solutions,” Adv. Mat. Res., 138, 7–20 (2010).10.4028/www.scientific.net/AMR.138.7 ↗
14. R. Tiwari, S. Sampath, H. Herman, and Y. Anekawa, Cavitation-Erosion of Plasma Sprayed Nickel Aluminides, in: Proc. National Thermal Spray Conf. (7–11 June 1993, Anaheim), Anaheim (1993), 423–428.
15. V. A. Lavrenko and V. N. Talash, Electrochemical Corrosion of Non-Metallic Materials [in Russian], G. G. Gnesin and V. V. Skorokhod (eds.), Neorgan. Materialloved., Vol. 1, Nauk. Dumka, Kiev (2008), pp. 663–675.
16. V. A. Shvets, V. A. Lavrenko, V. N. Talash, and O. A. Frernkel’, “Corrosion properties of the new TiB2–TiN and TiB2–AlN composite ceramic materials in 3 % NaCl solution,” Fiz. Khim. Mekh. Mater., 1, No. 1, 411–416 (2000).
17. A. D. Chirkin, V. A. Lavrenko, V. N. Talash, and A. D. Panasyuk, “Formation of oxide nanofilms on the surface of titanium, molybdenum, and tungsten disilicides during anodic polarization,” Dop. NAS of Ukraine, No. 12, 96–101 (2006).
18. C. Monticelli, F. Zucchi, A. Pagnoni, and M. Dal Colle, “Corrosion of a zirconium diboride/silicon carbide composite in aqueous solutions,” Electrochim. Acta, 50, 3461–3469 (2005).10.1016/j.electacta.2004.12.023 ↗
19. C. Monticelli, A. Balbo, and F. Zucchi, “Corrosion and tribocorrosion behaviour of cermet and cermet/nanoscale multilayer CrN/NbN coatings,” Surf. Coat. Technol., 204, 1452–1460 (2010).10.1016/j.surfcoat.2009.09.046 ↗