journal article·2010-12

Destructive hydrogenation and recombination of α2-Ti3Al alloy: production of solid nanocomposites and coatings with improved properties. I. Mechanism of destructive hydrogenation of Ti3Al

T. I. Bratanich, V. V. Skorokhod, L. I. Kopylova, A. V. Kotko, M. O. Krapivka

Powder Metallurgy and Metal Ceramics· Volume 49· Issue 7-8
Publisher page

Abstract

It is shown that α2-Ti3Al alloy and hydrogen interact at 298–1533 K in accordance with the destructive hydrogenation reaction whose products are titanium hydride and intermetallic compounds rich in aluminum. The structural mechanism of α2-Ti3Al destructive hydrogenation is as follows. Hydrogen dissolves in Ti3Al, thus leading to disordering of its crystalline structure. Then hydrogen interacts with titanium, but not with the disordered alloy, according to the following scheme: α-Ti (hcp) → α-TiHx (hcp) → β-TiHy (bcc) → TiH1.9 (fcc) → TiH2 (bct). Intermetallic compounds rich in aluminum show up when new stoichiometric concentrations of titanium and aluminum form in accordance with the Ti–Al phase diagram. Solid composites with nanosized components result from the destructive hydrogenation of Ti3A at 973 K for 1 and 4 h. Their phase compositions are Ti3Al–(α-TiH–Ti3–xAl) and ((α-Ti–Hx)–(β-Ti-Hy)–TiH1.9 (fcc)–TiH2 (bct))–(Ti3Al–TiAl–TiAl2), respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Applications · Environmental Policies and Emissions · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. P. S. Rudman, J. J. Reilly, and R. H. Wiswall, “The formation of metastable hydrides Ti0.75Al0.25H x with x < 1.5,” J. Less-Common Met., 58, 231–240 (1978).10.1016/0022-5088(78)90204-7 ↗
2. Akito Takasaki, Yoshio Furuya, and Youji Taneda, “Hydrogen uptake in titanium aluminides in high pressure hydrogen,” Mater. Sci. Eng., 239–240, 265–270 (1997).10.1016/S0921-5093(97)00591-1 ↗
3. D. Sornadurai, B. K. Panigrahi, K. Shashikala, et al., “X-ray diffraction and differential scanning calorimetry investigations on high-pressure hydrogen gas charged Ti3Al,” J. All. Comp., 312, No. 1–2, 251–256 (2000).10.1016/S0925-8388(00)01029-X ↗
4. K. Hashi, K. Ishikawa, K. Suzuki, and K. Aoki, “Hydrogen-induced amorphization in off-stoichiometric Ti3Al,” Scr. Mat., 44, 2591–2595 (2001).10.1016/S1359-6462(01)00922-8 ↗
5. K. Ishikawa, K. Hashi, K. Suzuki, and K. Aoki, “Effect of substitutional elements on the hydrogen absorption-desorption properties of Ti3Al,” J. All. Comp., 314, No. 1–2, 257–261 (2001).10.1016/S0925-8388(00)01231-7 ↗
6. Kazuhiro Ito, Yoshiharu Okabe, T. Lanting, “Reversible hydrogen absorption/desorption and related phase transformations in a Ti3Al alloy with the stoichiometry composition,” Acta Mat., 50, No. 19, 4901–4912 (2002).10.1016/S1359-6454(02)00360-9 ↗
7. K. Hashi, K. Ishikawa, K. Suzuki, and K. Aoki, “Hydrogen absorption and desorption in the binary Ti–Al system,” J. All. Comp., 330–332, 547–550 (2002).10.1016/S0925-8388(01)01660-7 ↗
8. K. Ishikawa, K. Hashi, K. Suzuki, and K. Aoki, “Hydrogen absorption properties of Ti3Al-based ternary alloys,” J. All. Comp., 330–332, 543–546 (2002).10.1016/S0925-8388(01)01655-3 ↗
9. Y. Kojima, M. Watanabe, M. Yamada, and K. Tanaka, “Phase stability and thermal desorption properties of Ti3Al hydrides,” J. All. Comp., 359, No. 1–2, 272–277 (2003).10.1016/S0925-8388(03)00202-0 ↗
10. M. Kh. Karapetyants and M. L. Karapetyants, Basic Thermodynamic Constants of Inorganic and Organic Substances [in Russian], Khimiya, Moscow (1968), p. 546.
11. M. Kh. Karapetyants and M. L. Karapetyants, Tables of Some Thermodynamic Properties of Different Substances (Collected Papers) [in Russian], Issue 34, Khim. Tekhnol. Inst., Moscow (1961), p. 166.
12. V. P. Glushko (ed.), Thermal Constants of Substances [in Russian], Issue 7, Part 1, VINITI, Moscow (1972), p. 370.
13. V. P. Glushko (ed.), Thermal Constants of Substances [in Russian], Issue 6, Part 1, VINITI, Moscow (1974), p. 344.
14. T. I. Bratanich, T. V. Permyakova, and V. V. Skorokhod, “Study of the process of destructive hydrogenation of powder intermetallic systems. I. Thermodynamic analysis of the processes of direct and destructive hydrogenation of intermetallics,” Powder Metall. Met. Ceram., 43, No. 11–12, 623–629 (2004).10.1007/s11106-005-0031-4 ↗
15. V. A. Livanov, A. A. Bukhanova, and B. A. Kolachev, Hydrogen in Titanium [in Russian], GNTILChTsM, Moscow (1962), p. 246.