journal article·2013-07

Some trends in the development of wear-resistant functional coatings

I. A. Podchernyaeva, D. V. Yurechko, V. M. Panashenko

Powder Metallurgy and Metal Ceramics· Volume 52· Issue 3-4
Publisher page

Abstract

Based on analysis of literature data on coatings playing a role of solid lubricants, prospective research areas have been identified. Two categories of coating materials are considered: with hardness lower than 10 GPa (polymers, soft metals, halides, dichalcogenides of transition metals, sulphates of alkaline earth metals, graphite) and with hardness higher than 10 GPa (oxides, carbides, nitrides, borides of transition metals, carbon-based composites). Methods of their deposition and surface structuring are discussed as well. The greatest effect is observed when coatings are deposited using combined techniques involving surface structuring. The development of new nanostructured high-temperature composite coatings that can adapt to extreme performance conditions is regarded as the most promising area of research for the next decade.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. C. Donnet and A. Erdemir, “Historical developments and new trends in tribological and solid lubricant coatings,” Surf. Coat. Technol., 180–181, 76–84 (2004).10.1016/j.surfcoat.2003.10.022 ↗
2. A. U. Stel’makh, “Experimental study of compression–vacuum friction mechanism,” Trenie Smaz. Mash. Mekhaniz., No. 5, 34–48 (2011).
3. A. A. Voevodin and J. S. Zabinski, “Nanocomposite and nanostructured tribological materials for space applications,” Compos. Sci. Technol., 65, 741–748 (2005).
4. A. Erdemir, “Solid lubricants and self-lubricating films,” in: B. Bhushan (ed.), Modern Tribology Handbook, CRC Press, New York (2001), pp. 787–825.
5. D. Jianxing, W. Ze, L. Yunsong, et al., “Performance of carbide tools with textured rake-face filled with solid lubricants in dry cutting processes,” J. Refract. Met. Hard Mater., 30, No. 1, 164–172 (2012).10.1016/j.ijrmhm.2011.08.002 ↗
6. I. L. Singer and H. M. Pollock (eds.), Fundamentals of Friction: Macroscopic and Microscopic Processes, Kluwer Academic, Dordrecht (1992), p. 237.10.1007/978-94-011-2811-7_13 ↗
7. J. M. Martin, C. Donnet, T. Le Mogne, and T. Epicier, “Superlubricity of molybdenum disulfide,” Phys. Rev., B48, No. 14, 10583–10586 (1993).10.1103/PhysRevB.48.10583 ↗
8. S. Gupta and M. W. Barsoum, “On the tribology of the MAX phases and their composites during dry sliding: a review,” Wear, 271, Issue 9–10, 1878–1894 (2011).10.1016/j.wear.2011.01.043 ↗
9. W. E. Jamison, “Plastics and plastic matrix materials,” in: E. R. Booser (ed.), Handbook of Lubrication and Tribology, CRC Press, Boca Raton (1994), p. 121.
10. T. A. Blanchet and F. E. Kennedy, “Sliding wear mechanism of polytetrafluoroethylene (PTFE) and PTFE composites,” Wear, 153, Issue 1, 229–243 (1992).10.1016/0043-1648(92)90271-9 ↗
11. P. J. John and J. S. Zabinski, “Sulfate based coatings for use as high temperature lubricants,” Tribol. Lett., 7, 31–37 (1999).10.1023/A:1019140530037 ↗
12. G. I. Kostyuk, Nanostructures and Nanocoatings: Prospects and Reality [in Russian], Khark. Aviat. Inst., Kharkov (2009), p. 106.
13. O. Knotek, M. Atzor, and H. G. Prengel, “On reactively sputtered Ti–Al–V carbonitrides,” Surf. Coat. Technol., 36, 265–273 (1988).10.1016/0257-8972(88)90156-9 ↗
14. V. M. Beresnev, M. Yu. Kopeikina, and S. A. Klimenko, “Multicomponent and multilayer vacuum-arc coatings for cutting tools,” Vopr. At. Nauk. Tekh. Ser. 17. Vak., Chist. Mater. Sverkhprovodn., No. 1, 152–158 (2008).
15. E. N. Reshetnyak and V. E. Strel’nitskii, “Synthesis of hardening nanostructured coatings,” Vopr. At. Nauk. Tekh. Ser. 92. Fiz. Radiats. Povrezhd. Radiats. Materialoved., No. 2, 119–130 (2008).
16. S. N. Grigor’ev, “Methods for deposition of wear-resistant nanocoatings in tool making,” Metall. Mashinostr., No. 1, 37–43 (2011).
17. H. Kato and K. Komai, “Tribofilm formation and mild wear by tribosintering of nanometer-sized oxide particles on rubbing steel surfaces,” Wear, 262, Issue 1–2, 36–41 (2007).10.1016/j.wear.2006.03.046 ↗
18. A. Matthews, “Developments in PVD-tribological coatings (IUVSTA highlights seminar-vacuum metallurgy division),” Vacuum, 65, No. 2, 237–238 (2002).10.1016/S0042-207X(01)00396-7 ↗
19. Y. Pauleau and P. B. Berna (eds.), Protective Coatings and Thin Films, Kluwer Academic, Dordrecht (1997), pp. 1–12.10.1007/978-94-011-5644-8 ↗
20. I. M. Hutching (ed.), New Directions in Tribology, Mechanical Engineering Publications, London (1997), pp. 121–133.
21. Yu. S. Borisov, A. L. Borisova, A. Yu. Tunik, et al., “Effect of microplasma spraying parameters on the structure, phase composition, and texture of hydroxyapatite coatings,” Avtomat. Svarka, No. 4, 15–20 (2008).
22. I. A. Podchernyaeva, A. D. Panasyuk, V. V. Shchepetov, et al., “Tribological properties of detonationsprayed SiC–Al2O3–ZrO2 coatings,” Probl. Tribol., No. 1, 81–86 (2003).
23. J. M. Guilemany, N. Llorga-Isern, M. D. Nunez, et al., “Study of interface interactions for metal–metal and metal–ceramic coating obtained by plasma and HVOF spraying,” Sci. Met. Mater., 31, No. 8, 1121–1126 (1994).10.1016/0956-716X(94)90537-1 ↗
24. V. I. Kalita, D. I. Komlev, V. B. Yashin, et al., “Cermet plasma coatings based on nanosized tungsten carbide,” Fiz. Khim. Obrab. Mater., No. 5, 32–43 (2011).
25. H. W. Liu, X. J. Xu, M. H. Zxu, et al., “High temperature fretting wear behavior of WC–25Co coatings prepared by D-gun spraying on Ti–Al–Zr titanium alloy,” Tribol. Int., 44, No. 11, 1461–1470 (2011).10.1016/j.triboint.2011.01.002 ↗
26. Y. S. Borisov, A. L. Borisova, and E. Dyad’ko, “Composite Ti–Si–C system coatings,” Mater. Manuf. Processes, 10, No. 4, 831–835 (1995).10.1080/10426919508935070 ↗
27. Yu. S. Borisov, A. L. Borisova, and A. Yu. Tunik, “Thermal-spray coatings for high-temperature dry friction applications,” in: Proc. Int. Conf. Materials and Coatings in Extreme Conditions (Katsiveli, 2010), Kiev (2010), p. 253.
28. A. L. Borisova, A. Yu. Tunik, G. M. Grigorenko, et al., “Tribotechnical properties of thermal-spray coatings with solid lubricants at high temperatures,” Avtomat. Svarka, No. 11, 30–34 (2010).
29. A. L. Borisova, A. Yu. Tunik, L. I. Adeeva, and G. N. Gordan’, “Antifriction thermal-spray coatings of a mechanical mixture of cast iron and calcium fluoride powders,” Avtomat. Svarka, No. 7, 24–29 (1999).
30. A. L. Borisova, L. I. Adeeva, and A. Yu. Tunik, “Structure and properties of thermal-spray coatings based on titanium carbide, titanium oxide, and chromium oxide containing solid lubricants,” Avtomat. Svarka, No. 1, 20–28 (1996).
31. N. L. Golego, A. L. Borisova, A. L. Gaidarenko, et al., “Tribotechnical properties of plasma oxide coatings. І. Wear resistance of oxide coatings under friction–sliding,” Trenie Iznos, 11, No. 6, 1009–1013 (1990).
32. M. M. Gasik, K. R. Lilius, and P. N. Ostrik, “Modeling the properties of functional gradient materials,” Probl. Spets. Élektrometall., No. 4, 43–47 (1997).
33. I. A. Podchernyaeva, D. V. Yurechko, A. D. Panasyuk, and M. A. Teplenko, “Mass transfer and adhesion in electrospark alloying of AL9 alloy with AlN–Ti(Zr)B2–Ti(Zr)Si2 ceramic electrodes,” Powder Metall. Met. Ceram., 43, No. 9–10, 473–479 (2004).10.1007/s11106-004-0007-9 ↗
34. E. Sheinman, “Superhard nanocomposite coatings: review of foreign publications,” Metalloved. Term. Obrab. Met., No. 12, 41–47 (2008).
35. A. Savan, E. Pfluger, R. Goller, and W. Gissler, “Use of nanoscaled multilayer and compound films to realize a soft lubrication phase within a hard, wear-resistant matrix,” Surf. Coat. Technol., 126, 159–165 (1999).10.1016/S0257-8972(00)00542-9 ↗
36. A. Leyland and A. Matthews, “On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimized tribological behavior,” Wear, 246, Issue 1–2, 1–11 (2000).10.1016/S0043-1648(00)00488-9 ↗
37. A. V. Ragulya and V. V. Skorokhod, Consolidated Nanostructured Materials [in Russian], Naukova Dumka, Kiev (2007), p. 374.
38. S. A. Barnett, A. Madan, I. Kim, and K. Martin, “Stability of nanometer-thick layers in hard coatings,” MRS Bull., 28, No. 3, 169–172 (2003).10.1557/mrs2003.57 ↗
39. R. Le Harzic, N. Huot, E. Audouard, et al., “Comparison of heat-affected zones due to nanosecond and femtosecond laser pulses using transmission electronic microscopy,” Appl. Phys. Lett., 80, No. 21, 3886–3888 (2002).10.1063/1.1481195 ↗
40. T. M. Kononenko, S. V. Garnov, S. M. Pimenov, et al., “Laser ablation and micropatterning of thin TiN coatings,” Appl. Phys., A71, 627–631 (2000).10.1007/s003390000572 ↗
41. A. A. Voevodin, J. Bultman, and J. S. Zabinski, “Investigation into three-dimensional laser processing of tribological coatings,” Surf. Coat. Technol., 107, 12–19 (1998).10.1016/S0257-8972(98)00543-X ↗
42. B. A. Lyashenko, E. K. Solovykh, V. I. Mirnenko, et al., Optimization of Coating Processes by Strength and Wear Resistance Criteria [in Russian], Inst. Probl. Prochn. NAN Ukrainy, Kiev (2010), p. 193.
43. B. A. Lyashenko, “On criteria of adhesive–cohesive uniform strength and heat resistance of protective coatings,” Probl. Prochn., No. 10, 114–126 (1980).
44. I. A. Podchernyaeva, A. D. Panasyuk, V. M. Panashenko, et al., “Electroerosion resistance and structural phase transformations in electrospark and laser deposition of titanium alloys using composite ceramics based on ZrB2-ZrSi2 and TiN-Cr3C2 systems,” Powder Metall. Met. Ceram., 47, No. 1–2, 116–123 (2008).10.1007/s11106-008-0016-1 ↗
45. O. B. Soroka, M. Yu. Kopeikina, V. S. Antonyuk, and S. A. Klimenko, “Evaluation of residual stresses in plasma vacuum coatings,” Visn. Zhitom. Derzh. Tekh. Univ. Tekh. Nauki, Issue 42, No. 3, 41–45 (2007).
46. E. B. Soroka, S. A. Klimenko, and M. Yu. Kopeikina, “Adhesive and cohesive strength of vacuum plasma (TiAl)N and TiN coatings,” Deform. Razrush. Mater., No. 5, 26–31 (2010).
47. E. B. Soroka, S. A. Klimenko, and M. Yu. Kopeikina, “Evaluation of residual stresses in PVD-coatings. Part 2,” Strength Mater., 42, Issue 4, 450–458 (2010).10.1007/s11223-010-9236-y ↗
48. O. B. Soroka, S. A. Klymenko, and M. Y. Kopeikina, “Ensuring of the adhesion and cohesion strength of PVD (TiAl)N and TiN coatings,” Russ. Metall., 2011, No. 4, 350–355 (2011).10.1134/S0036029511040203 ↗
49. A. Blomberg, S. Hogmark, and J. Lu, “An electron microscopy study of worn ceramic surfaces,” Tribol. Int., 26, 369–381 (1993).10.1016/0301-679X(93)90075-C ↗
50. I. A. Podchernyaeva, A. D. Panasyuk, V. M. Panashenko, and O. N. Grigor’ev, “Abrasive wear of ZrB2-containing spark-deposited and combined coatings on titanium alloy. I. microstructure and composition of ZrB2-containing coatings,” Powder Metall. Met. Ceram., 48, No. 5–6, 316–325 (2009).10.1007/s11106-009-9126-7 ↗
51. I. A. Podchernyaeva, A. D. Panasyuk, V. M. Panashenko, et al., “Abrasive wear of ZrB2-containing sparkdeposited and combined coatings on titanium alloy. II. Nonfixed-abrasive wear of ZrB2-containing coatings,” Powder Metall. Met. Ceram., 48, No. 7–8, 435–440 (2009).10.1007/s11106-009-9148-1 ↗
52. I. A. Podchernyaeva, A. I. Dukhota, V. M. Panashenko, et al., “Kinetics and mechanisms of fretting corrosion of spark- and laser-deposited ZrB2-containing coatings on VT3-1 alloy,” Probl. Tribol., No. 1, 62–72 (2012).
53. H. W. Strauss, R. R. Chromik, S. Hassani, and J. E. Klemberg-Sapieha, “In situ tribology of nanocomposite Ti–Si–C–H coatings prepared by PE-CVD,” Wear, 272, Issue 1, 133–148 (2011).10.1016/j.wear.2011.08.001 ↗
54. M. Aristizabal, L. C. Ardila, F. Veiga, et al., “Comparison of the friction and wear behavior of WC–Ni–Co–Cr and WC–Co hardmetals in contact with steel at high temperatures,” Wear, 280–281, Issue 1–2, 15–21 (2012).10.1016/j.wear.2012.01.015 ↗
55. Ya-e Qi, Yong-Sheng Zhang, and Li-Tian Hu, “High-temperature self-lubricated properties of Al2O3–Mo laminated composites,” Wear, 280–281, Issue 1–2, 1–4 (2012).10.1016/j.wear.2012.01.010 ↗
56. S. Carvalho, E. Ribeiro, L. Rebouta, et al., “Effect of morphology and structure on the elastic behavior of (Ti, Si, Al)N nanocomposites,” Surf. Coat. Technol., 174–175, 984–991 (2003).10.1016/S0257-8972(03)00386-4 ↗
57. E. Ribeiro, A. Malezyk, S. Carvalho, et al., “Effect of ion bombardment on properties of d. c. sputtered superhard (Ti, Si, Al)N nanocomposite coatings,” Surf. Coat. Technol., 151–152, 515–520 (2002).10.1016/S0257-8972(01)01578-X ↗
58. S. K. Kim, P. V. Vinh, J. H. Kim, and T. Ngoc, “Deposition of superhard Ti–Al–Si–N thin films by cathodic arc plasma deposition,” Surf. Coat. Technol., 200, 1391–1394 (2005).10.1016/j.surfcoat.2005.08.109 ↗
59. S. Mukherjce, F. Prokert, E. Richter, and W. Moller, “Comparison of TiN and Ti–Al–N coatings deposited on Al using plasma immersion ion implantation assisted deposition,” Surf. Coat. Technol., 200, 2459–2464 (2005).10.1016/j.surfcoat.2004.11.028 ↗
60. M. Balzer, H. Kappl, H. A. Jehn, and V. Güther, “Cathodic-arc deposition with boron-alloyed titanium cathodes,” Surf. Coat. Technol., 119, 766–771 (1999).10.1016/S0257-8972(99)00275-3 ↗
61. S. Paldey and S. C. Deevi, “Single layer and multilayer wear resistant coatings of (Ti, Al)N: a review,” Mater. Sci. Eng., A342, 58–79 (2003).10.1016/S0921-5093(02)00259-9 ↗
62. T. J. Robertson, “Diamond-like amorphous carbon,” Mater. Sci. Eng., R37, 129–281 (2002).10.1016/S0927-796X(02)00005-0 ↗
63. S. A. Klimenko, V. M. Beresnev, M. Yu. Kopeikina, and V. I. Gritsenko, “Layer vacuum-arc Ti–NbN–Al2O3 and Nb–NbN–Al2O3 coatings on tools with polycrystalline superhard materials based on cubic boron nitride,” Fiz. Inzhin. Poverkhn., 5, No. 1–2, 87–97 (2007).
64. M. Yu. Kopeikina, S. A. Klimenko, Yu. A. Mel’niichuk, and V. M. Beresnev, “Improvement of cutting tools with polycrystalline superhard materials based on cubic boron nitride by vacuum-arc coatings,” Sverkhtverd. Mater., No. 5, 87–97 (2008).
65. A. D. Panasyuk, I. A. Podchernyaeva, N. S. Boltovets, et al., “Structure and properties of thin ceramic coatings in the system AlN-TiCrB2,” Powder Metall. Met. Ceram., 45, No. 5–6, 244–250 (2006).10.1007/s11106-006-0071-4 ↗
66. J. H. Ouyang, Z. L. Yang, Z. G. Liu, and X. S. Liang, “Friction and wear properties of reactive hot-pressed TiB2–TiN composites in sliding against Al2O3 ball at elevated temperatures,” Wear, 271, Issue 9–10, 1966–1973 (2011).10.1016/j.wear.2010.11.057 ↗
67. A. A. Voevodin and J. S. Zabinski, “Supertough wear-resistant coatings with “chameleon” surface adaptation,” Thin Solid Films, 370, 223–231 (2000).10.1016/S0040-6090(00)00917-2 ↗
68. P. J. John, S. V. Prasad, A. A. Voevodin, and J. S. Zabinski, “Calcium sulfate as a high temperature solid lubricant,” Wear, 219, Issue 2, 155–161 (1998).10.1016/S0043-1648(98)00167-7 ↗
69. S. D. Walck, J. S. Zabinski, N. T. McDevitt, and J. E. Bultman, “Characterization of air-annealed, pulsed laser deposited ZnO–WS2 solid film lubricants by transmission electron microscopy,” Thin Solid Films, 305, 130–143 (1997).10.1016/S0040-6090(97)00129-6 ↗
70. A. Cavaleiro and C. Louro “Nanocrystalline structure and hardness of thin films,” Vacuum, 64, No. 3, 211–218 (2002).10.1016/S0042-207X(01)00337-2 ↗
71. J. S. Zabinski, J. H. Sanders, J. Nainaparampil, and S. V. Prasad, “Lubrication using a microstructurally engineered oxide: performance and mechanisms,” Tribol. Lett., 8, 103–116 (2000).10.1023/A:1019187202237 ↗
72. A. G. Kostornov, O. I. Fushchich, V. F. Gorban’, et al., “Dependence of antifriction properties of selflubricating copper-based composite on the elastoplastic characteristics of tribosynthesis region,” Powder Metall. Met. Ceram., 47, No. 11–12, 674–679 (2008).10.1007/s11106-009-9077-z ↗
73. A. G. Kostornov, O. I. Fushchich, T. M. Chevychelova, et al., “Structural and phase transformations in the tribosynthesis area of copper-based self-lubricating composite material,” Powder Metall. Met. Ceram., 48, No. 5–6, 358–364 (2009).10.1007/s11106-009-9123-x ↗
74. T. V. Mosina, A. D. Panasyuk, O. N. Grigor’ev, and A. I. Yuga, “Friction properties of composite materials of the system TiN–AlN. II. Effect of oxide films on friction and wear of a ceramic material—steel system,” Powder Metall. Met. Ceram., 39, No. 1–2, 105–108 (2000).10.1007/BF02677451 ↗