Interaction between Hydrogen and Ground SmCo5 Alloy
Source abstract
Abstract
The paper determines the phase composition of the ground KS37 alloy after conventional and solid hydrogenation and disproportionation (SmCo5 being the main phase and Sm2Co7 the impurity phase) at a hydrogen pressure of 0.1–0.4 MPa and at temperatures up to 950°C for 5 h. It is established that products resulting from grinding of the Sm2Co7 phase interact with hydrogen to 560°C to form Sm5Co19 and unidentified phases. The SmCo5 phase disproportionates in the temperature range 560–650°C and pressure range 0.1–0.4 MPa for 2 h. Recombination at 650–950°C leads to the SmCo5, Sm2Co7, and Sm2Co17 phases. The SmCo5 content of the recombined alloy is the highest at 950°C. It is shown that grinding in hydrogen prior to hydrogenation, disproportionation, desorption, and recombination accelerates the disproportionation reaction owing to the formation of defects during grinding. The high-temperature recombination of the SmCo5 phase in hydrogen is confirmed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Rare-earth and actinide compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. D. Goll and H. Kronmuller, “High-performance permanent magnets, “Naturwissenschaften, 87, 423–438 (2000).10.1007/s001140050755 ↗
2. E. F. Kneller and R. Hawig, “The exchange-spring magnet: a new material principle for permanent magnets,” IEEE Trans. Magn., 27, 3588–3600 (1991).10.1109/20.102931 ↗
3. J. Ding, P. G. McCormick, and R. Street, “Remanence enhancement in mechanically alloyed isotropic Sm7Fe93-nitride,” J. Magn. Magn. Mater., 124, 1–4 (1993).10.1016/0304-8853(93)90060-F ↗
4. O. Donnell, C. Kuhrt, and J. M. D. Coey, “Influence of nitrogen content on coercivity in remanenceenhanced mechanically alloyed Sm–Fe–N,” J. Appl. Phys., 76, 7068–7070 (1994).10.1063/1.358029 ↗
5. M. Kubis, A. Handstein, B. Gebel, et al., “Highly coercive SmCo5 magnets prepared by a modified hydrogenation–disproportionation–desorption–recombination process,” J. Appl. Phys., 85, 5666–5668 (1999).10.1063/1.369834 ↗
6. O. Gutfleisch, M. Kubis, A. Handstein, et al., “Hydrogenation disproportionation desorption recombination in Sm–Co alloys by means of reactive milling,” Appl. Phys. Lett., 73, 3001–3003 (1998).10.1063/1.122657 ↗
7. Handstein, M. Kubis, O. Gutfleisch, et al., “HDDR of Sm–Co alloys using high hydrogen pressures,” J. Magn. Magn. Mater., 192, 73–76 (1999).10.1016/S0304-8853(98)00379-5 ↗
8. N. Cannesan and I. R. Harris, “Aspects of NdFeB HDDR powders: fundamentals and processing,” in: G. C. Hadjipanayis (ed.), Bonded Magnets. NATO Science Series. II. Mathematics, Physics and Chemistry, Vol. 118, 13–36 (2002).
9. I. Bulik, Yu. B. Basaraba, A. M. Trostyanchin, and V. M. Davidov, “Disproportionation in hydrogen and recombination of the Laves phases of zirconium with chromium,” Fiz. Khim. Mekh. Mater., No. 3, 101–108 (2005).
10. Electronic Resource. Access Page: http://www.ccp14.ac.uk/tutorial/powdcell .
11. Electronic Resource. Access Page: www.ill.eu/sites/fullprof .
12. Electronic Resource. Access Page: www.sigmaaldrich.com .
13. I. Bulik, A. M. Trostyanchin, and V. I. Markovich, “Phase transformations in the SmCo5 alloy initiated by hydrogen under pressure to 650 kPa,” Fiz. Khim. Mekh. Mater., No. 1, 94–98 (2007).
14. I. Bulik, A. M. Trostyanchin, and P. Ya. Lyutyi, “Effect of the duration of interaction between the SmCo5 alloy and hydrogen at low pressure on the phase composition,” Fiz. Khim. Mekh. Mater., No. 3, 53–58 (2012).
15. O. Gutfleisch, M. Matzinger, J. Fidler, and I. R. Harris, “Characterization of solid-HDDR processed Nd16Fe76B8 alloys by means of electron microscopy,” J. Magn. Magn. Mater., 147, 320–330 (1995).10.1016/0304-8853(95)00026-7 ↗