Abstract

A comparative microstructural analysis of the scale formed on the NiAl–Re detonation coating shows that the mechanism of its high-temperature oxidation can be changed with preliminary magnetic abrasive treatment (MAT). The scale formed over the NiAl–Re coating in ordinary conditions includes several layers (NiO–NiAl2O4–Al2O3), while the scale formed on the MAT coating consists of an Al2O3 monolayer with spinel inclusions. The differences in the oxidation of the NiAl and NiAl–Re coatings after MAT are attributed to changes in their dislocation structure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. R. Darolia, D. F. Lahrman, and R. D. Field, “Overview of NiAl for high temperature structural application,” in: Ordered Intermetallics: Physical Metallurgy and Mechanical Behavior, NATO Science Series E, Kluwer Academic Publishers, Dordrecht (1992), Vol. 3, pp. 679– 698.10.1007/978-94-011-2534-5_43 ↗
2. W. Smarsly and L. Singheiser, “Potential of intermetallics to replace superalloys for advanced operation conditions in gas turbines,” J. Mat. Adv. Powder Eng., 2, 1731–1756 (1994).
3. M. B. Henderson, J. Hannis, and G. McColvin (eds.), “Materials issues for the industrial gas turbines,” in: Advanced Materials and Processes for Gas Turbines, The Minerals, Metals & Materials Society, Warrendale (2003), pp. 3–13.
4. Blanch Resistant and Thermal Barrier NiAl Coatings Systems for Advanced Copper Alloys, US Patent 6838191, Published 2005.
5. J. Angenete, K. Stiller, and V. Langer, “Oxidation of simple and Pt modified aluminide diffusion coatings on based superalloys. I. Oxide scale microstructure,” Oxid. Met., 60, No. 1–2, 47–82 (2004).
6. J. Doychak, J. L. Smialek, and T. E. Mitchell, “Transient oxidation of single-crystal beta-NiAl,” Met. Trans., 20A, 499–518 (1989).10.1007/BF02653930 ↗
7. H. Svenson, J. Angenete, K. Stiller, and V. Langer, “Microstructural studies of NiAl-based model alloys and commercial coatings after isothermal oxidation,” Mat. High Temp., 20, No. 3, 421–427 (2003).10.1179/mht.2003.049 ↗
8. A. Y. Lozovoy, A. Alavi, and M. W. Finnis, “Surface stoichiometry and initial oxidation of NiAl (110),” Phys. Rev. Let., 85, No. 3, 610–613 (2000).10.1103/PhysRevLett.85.610 ↗
9. Yu. A. Tamarin, Heat-Resistant Diffusion Coatings on Blades of Gas-Turbine Engines [in Russian], Mashinostroenie, Moscow (1978), p. 136.
10. M. Reid, M. J. Pomeroy, and J. S. Robinson, “Microstructural stability of a Ni–Pt–Al coating on CMSX-10 alloy at 950 and 1100°C,” Mat. High Temp., 20, No. 4, 467 (2003).10.1179/mht.2003.054 ↗
11. R. D. Noebe, R. R. Bowman, and M. V. Nathal, “Physical and mechanical properties of the B2 compound NiAl,” Int. Mat. Rev., 38, 193–232 (1993).10.1179/imr.1993.38.4.193 ↗
12. J. G. Webber and D. C. Van Aken, “Studies of a quasi-binary β-NiAl and α-Re eutectic,” Scr. Mat., 21, 193–196 (1989).10.1016/0036-9748(89)90409-2 ↗
13. R. Rablbauer, G. Frommeyer, and F. Stein, “Determination of the quasi-binary eutectic NiAl–Re system by DTA and microstructural investigations,” Mat. Sci. Eng., A343, 301–307 (2003).10.1016/S0921-5093(02)00388-X ↗
14. O. M. Barabash, M. Yu. Barabash, and V. E. Oliker, “Effect of rhenium on formation of the structure of eutectic alloys based on β-NiAl + γ-Re,” Powder Metall. Met. Ceram., 42, No. 3–4, 180–183 (2003).
15. V. E. Oliker, M. Yu. Barabash, E. F. Grechishkin, et al., “Mechanical properties of eutectic alloys β-NiAl + γ-Re and spray coatings,” Powder Metall. Met. Ceram., 45, No. 3–4, 173–180 (2006).10.1007/s11106-006-0060-7 ↗
16. V. Yu. Oliker, M. Yu. Barabash, T. Ya. Gridasova, et al., “Behavior of detonation coatings based on NiAl intermetallide in thermocyclic oxidation,” Nauk. Visti NTUU KPI, No. 6, 56–63 (2005).
17. H. Hindam and W. W. Smeltzen, J. Electrochem. Soc., 127, 1622–1630 (1980).10.1149/1.2129964 ↗
18. P. Saltykov, O. Fabrichnaya, J. Golczewski, and F. Aldinger, “Thermodynamic modeling oxidation of Al–Cr–Ni alloys,” J. All. Comp., 381, No. 1–2, 99–113 (2004).10.1016/j.jallcom.2004.02.053 ↗
19. B. A. Pint, J. A. Haynes, K. L. More, et al., “Composition effects on aluminide oxidation performance: objectives for improved bond coats,” in: Proc. ASM-TMS Superalloys 2000, Seven Springs, Pennsylvania (2000).
20. F. Dettenvanger, E. Schumann, M. Ruhle, et al., “Microstructural study of oxidized-TiAl,” Oxid. Met., 50, No. 3–4, 269–274 (1998).10.1023/A:1018892422121 ↗
21. V. E. Oliker, Powders for Magnetic Abrasive Treatment and Wear-Resistant Coatings [in Russian], Metallurgiya, Moscow (1990), p. 176.
22. S. T. Kishkin and A. A. Klypin, “Electric and magnetic effects on the creep of metals and alloys,” Dokl. AN SSSR, 211, No. 2, 325–327 (1973).
23. Yu. I. Golovin, “Magnetic plasticity of solids,” Fiz. Tverd. Tela, 46, No. 5, 769–803 (2004).
24. O. V. Brodovoi, Magnetic Properties of Structurally Disordered Weak-Magnetic Solids [in Russian], Authors’ Abstract of ScD Thesis, Kiev (2007).
25. V. M. Mironov, Self- and Heterodiffusion in Metals under Magnetic Fields and Pulse Strains [in Russian], Author’s Abstract of ScD Thesis, Moscow (2005).
26. V. E. Oliker, Application, Classification, and Development Trends of Abrasive Treatment with Ferromagnetic Powders [in Russian], Preprint, Inst. Probl. Materialoved. AN USSR, Kiev (1984), p. 66.
27. V. E. Oliker, M. Yu. Barabash, E. F. Grechishnik, etc., “High-temperature air oxidation of coatings based on eutectic (β-NiAl + γ-Re) alloys and NiAl intermetallide,” Powder Metall. Met. Ceram., 46, No. 3–4, 175–181 (2007).10.1007/s11106-007-0028-2 ↗
28. P. T. Koldomytsev, Heat-Resistant Diffusion Coatings [in Russian], Metallurgiya, Moscow (1979), p. 271.
29. J. Bénard (ed.), Oxidation of Metals [in French], Vol. 1, Gauthier-Villars, Paris (1962).
30. O. Kubaschewski and B. E. Hopkins, Oxidation and Metals and Alloys, Butterworth, London (1962).
31. C. L. Fu, M. H. Yoo, and K. M. Ho, “Equilibrium point defects in intermetallics with the B2 structures NiAl and FeAl,” Phys. Rev., 48, 6712–6715 (1993).10.1103/PhysRevB.48.6712 ↗