Reversible Hydriding of LaNi5 − xAlx ― Pd Composites in the Presence of Carbon Monoxide
Source abstract
Abstract
Carbon monoxide is one of the most dangerous impurities in gas mixtures involved in the hydriding of intermetallic compounds, and up to the present time the concentration limit 0.03 vol.% CO has not been surmounted. The objective of the present work was to investigate the possibility of reversibly hydriding LaNi5 − xAlx ― Pd composites in gas mixtures containing up to 5 vol.% CO. The experimental specimens were mixtures of palladium black and LaNi5, LaNi4.7Al0.3, LaNi4.5Al0.5, LaNi4.2Al0.8, and LaNi4Al powders cold pressed at 300 MPa. The intermetallics were preliminarily dispersed by hydriding and mechanical grinding. The concentration of palladium black in the powder mixtures was varied from 0 to 1.5 mass%. It was shown that it is possible to reversibly hydride LaNi5 − xAlx ― Pd composites in mixtures of hydrogen and carbon monoxide containing up to 5 vol.% CO at the temperatures 423 and 473 K. It was established that alloying LaNi5 with aluminum in amounts which raised the stoichiometric concentration above 0.5 stabilized the absorption properties of LaNi5 − xAlx ― Pd in the presence of CO. The composition LaNi4Al was optimal. Palladium additions to LaNi5 − xAlx ― Pd composites also increased the stability of hydrogen absorption by the intermetallic. It is noted that the effect of palladium was more positive than that of aluminum.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Catalysis and Hydrodesulfurization Studies · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. B. P. Tarasov and S. P. Shilkin, “Possibility of separating and storing very pure hydrogen with the aid of intermetallic compounds,” Zh. Prikl. Khim., 68, No. 1, 21-26 (1995).
2. G. D. Sandrock and P. D. Goodell, “Surface poisoning of LaNi5, FeTi, and (Fe, Mn)Ti by O2, Co, and H2O,” J. Less-Common Met., 73, 161-168 (1980).10.1016/0022-5088(80)90355-0 ↗
3. F. G. Eisenberg and P. D. Goodell, “Cyclic response of reversible hydriding alloys in hydrogen containing carbon monoxide,” J. Less-Common Met., 89, No. 1, 55-62 (1983).10.1016/0022-5088(83)90248-5 ↗
4. D. G. Ivey and D. O. Nortwood, “Storing energy in metal hydrides: a review of the physical metallurgy,” J. Mater. Sci., 18, No. 2, 321-347 (1983).10.1007/BF00560621 ↗
5. F. R. Block and H. J. Bahs, “Investigation of selective absorption of hydrogen by LaNi5 and FeTi,” J. Less-Common Met., No. 1, 77-84 (1983).10.1016/0022-5088(83)90251-5 ↗
6. H. Uchida, “Surface processes of hydrogen on rare earth based hydrogen storage alloys with various surfaces modifications,” Int. J. Hydrogen Energy, 24, No. 9, 861-869 (1999).10.1016/S0360-3199(98)00160-8 ↗
7. B. P. Nikol'skoi (ed.), Handbook of Chemistry, Vol. 1 [in Russian], Gos. N.-T. Izd. Khim. Lit., Moscow-Leningrad (1962).
8. M. Kh. Karapet'yants and M. L. Karapet'yants, Tables of Some Thermodynamic Properties of Various Substances, Vol. XXXIV [in Russian], Tr. Khim. Tekh. Inst., Moscow (1961).
9. B. A. Kolachev, R. E. Shalin, and A. A. Il'in, Alloys ??Hydrogen Accumulators: Handbook [in Russian], Metallurgiya, Moscow (1995).