Interaction and Phase Formation in the WC–Fe2O3–NiO–C System Heated in Vacuum and Argon
Source abstract
Abstract
The interaction and phase formation in the WC–33 wt.% (80% Fe2O3 + 20% NiO) system with and without free carbon when heated in vacuum and in an argon atmosphere have been studied. Superfine soot and sucrose were used as free carbon. The powders pressed as pellets were heated by incremental temperature rise. In the absence of free carbon, the carbon contained in tungsten carbide and the oxygen contained in iron and nickel oxides actively interact in the carbide–oxide system, leading to weight loss of the samples. The intermetallic (Fe, Ni)7W6 phase, (Fe, Ni)WO4 oxide, and tungsten form as a result. The addition of free carbon allows tungsten carbide to be retained partially or completely and iron and nickel to be reduced from oxides. If there is a lack of free carbon, some part of the carbon contained in tungsten carbide begins to interact with oxygen to form complex Me6C carbide in the system, the metal phase having fcc and bcc lattices. When heating proceeds in vacuum, more carbon is spent to remove the same amount of oxygen than in heating in an argon atmosphere, but temperature of active interaction between carbon and oxygen decreases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. I. N. Chaporova, V. I. Kudryavtseva, and A. V. Varaksina, “Study of the structure and properties of WC–Fe–Ni alloys,” in: Solid Alloys (Collected Papers) [in Russian], VNIITS (1973), Issue 12, pp. 84–91.
2. Michael Humenik, Allen Dark, and David Moskowitz, Iron Bonded Tungsten Carbide, US Patent No. 3384465, Ford Motor Company, NCI 29-182-8, appl. June 22, 1967; May 21 (1968).
3. B. Wittmann, W. D. Schubert, and B. Lux, “WC grain growth and grain growth inhibition in nickel and iron binder hardmetals,” Int. J. Refract. Met. Hard Mater., 20, No. 1, 51–60 (2002).10.1016/S0263-4368(01)00070-1 ↗
4. A. I. Tolochin, A. V. Laptev, M. E. Golovkova, et al., “Ultrafine high-cobalt VK40 hard alloy. I. Structure and properties,” Powder Metall. Met. Ceram., 47, No. 3–4, 176–182 (2008).10.1007/s11106-008-9002-x ↗
5. A. I. Tolochin, A. V. Laptev, I. Yu. Okun, et al., “Composite WC–35% Ni produced from ultrafine WC + NiO powders. II. Mechanical properties,” Powder Metall. Met. Ceram., 50, No. 9–10, 625–631 (2012).10.1007/s11106-012-9368-7 ↗
6. A. Laptiev, Z. Pakiela, O. Tolochyn, et al., “Microstructure and mechanical properties of WC–40Co composite obtained by impact sintering in solid state,” J. Alloys Compd., 687, 135–142 (2016).10.1016/j.jallcom.2016.05.343 ↗
7. G. Nolze, “PowderCell: A mixture between crystal structure visualizer, simulation and refinement tool,” in: Proc. 2nd Int. School on Powder Diffraction (January 20–23, 2002, IACS, Kolkata, India), Kolkata (2002), pp. 146–155.
8. O. A. Esin and P. V. Geld, Physical Chemistry of Igneous Metallurgy Process [in Russian], Metallurgizdat, Sverdlovsk (1962), Part 1, p. 672.