Crystallographic Features of Nanosized Titanium Carbide Produced from Titanium and Carbon in a Planetary-Ball Mill
Source abstract
Abstract
Structural changes that occur in titanium during grinding of a powder mixture of titanium and carbon in an AIR-015M planetary-ball mill are studied. Grinding of the powder mixture results in the formation of titanium carbide single crystals with particles 7–50 nm in size over the entire reaction zone. At the initial stage of grinding, texturing of titanium occurs and the titanium lattice cell increases in volume, thus inducing internal stresses. Based on these data, it is suggested that the introduction of carbon into the strained titanium particles leads to stacking faults in the titanium hcp lattice, acting as nuclei of fcc titanium carbide in the titanium sites fragmented. Single-crystal TiC 10–20 nm nanoparticles are formed in these sites. The length of titanium–carbon contacts naturally increases with grinding time, giving rise to more nuclei of the new fcc phase. This promotes a mechanically induced self-propagating reaction. The heat generated in the reaction contributes to the sintering of titanium carbide nanoparticles. This results in the formation of particle aggregates 0.1–0.5 μm in size.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. K. B. Shelimov and P. Yu. Butyagin, “On explosive mechanochemical synthesis of refractory compounds,” Dokl. Akad. Nauk SSSR, 316, No. 6, 1439–1443 (1991).
2. M. Savyak, I. Uvarova, I. Timofeeva, et al., “Mechanochemical synthesis of nanophased refractory carbides,” in: Proc. Int. Symp. Metastable Mechanically Alloyed and Nanocrystalline Materials ISMANAM-99, Dresden, Germany (1999), pp. 256–263.
3. B. Ghosha and S. K. Pradhan, “Microstructure characterization of nanocrystalline TiC synthesized by mechanical alloying,” Mater. Chem. Phys., 120, 537–545 (2010).10.1016/j.matchemphys.2009.11.048 ↗
4. Q. Yuan, Y. Zheng, and H. Yu, “Mechanism of synthesizing nanocrystalline TiC in different milling atmospheres,” J. Refract. Met. Hard Mater., 27, 696–700 (2009).10.1016/j.ijrmhm.2008.11.003 ↗
5. N. J. Calos, J. S. Forrester, and G. B. Schaffer, “The mechanisms of combustion and continuous reactions during mechanical alloying,” J. Solid State Chem., 158, 268–278 (2001).10.1006/jssc.2001.9107 ↗
6. A. Teresiak, N. Mattern, H. Kubsch, and B. F. Kieback, “Structure and stability of nanocrystalline TiC powders obtained by reactive high energy milling,” Nanostruct. Mater., 4, No. 7, 775–786 (1994).10.1016/0965-9773(94)90083-3 ↗
7. L. L. Ye and M. X. Quan, “Synthesis of nanocrystalline TiC powders by mechanical alloying,” Nanostruct. Mater., 5, No. 1, 25–31 (1995).10.1016/0965-9773(95)00012-4 ↗
8. M. P. Saviak, A. B. Mel’nik, Yu. M. Solonin, et al., “Mechanosynthesis of nanosized titanium diboride,” Powder Metall. Met. Ceram., 53, Nos. 9–10, 497–504 (2015).10.1007/s11106-015-9643-5 ↗
9. R. A. Young, The Rietveld Method, Oxford University Press (1993).10.1093/oso/9780198555773.001.0001 ↗
10. G. K. Williamson and W. H. Hall, “X-ray line broadening from filed aluminum and wolfram,” Acta Metall., 1, No. 1, 22−31 (1953).10.1016/0001-6160(53)90006-6 ↗