The Ti–Al–Si–B–N films are deposited by dc magnetron sputtering of a composite Ti–Al–Si–B–N target in argon plasma. The structure and phase composition of the films were studied by X-ray diffraction. The chemical bonds in films were examined by X-ray photoelectron spectroscopy. The influence of vacuum annealing on film structure, hardness, and mechanical properties was analyzed. The films deposited at temperatures in the range 200–500°C and bias voltages of 0…–250 exhibited amorphous structure, which was preserved during annealing up to 800°C. At higher annealing temperatures, nanocrystalline phases started to form in the films. Annealing also resulted in increase of hardness and improvement of mechanical characteristics of the films.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. S. Veprek, “Recent attempts to design new super- and ultrahard solids lead to nanosized and nanostructured materials and coatings,” J. Nanosci. Nanotechnol., 11, 14–35 (2011).10.1166/jnn.2011.3815 ↗
2. Fei Cai, Shihong Zhang, Jinlong Li, et al., “Effect of nitrogen partial pressure on Al–Ti–N films deposited by arc ion plating,” Appl. Surf. Sci., 258, 1819–1825 (2011).10.1016/j.apsusc.2011.10.053 ↗
3. C. W. Zou, J. Zhang, W. Xie, et al., “Structure and mechanical properties of Ti–Al–N coatings deposited by combined cathodic arc middle frequency magnetron sputtering,” J. Alloys Compd., 509, 1989–1993 (2011).10.1016/j.jallcom.2010.10.110 ↗
4. S. M. Aouadi, F. Namavar, T. Z. Gorishnyy, and S. L. Rhode, “Characterization of TiBN films grown by ion beam assisted deposition,” Surf. Coat. Technol., 160, 145–151 (2002).10.1016/S0257-8972(02)00330-4 ↗
5. C. López-Cartes, D. Martínez-Martínez, J. C. Sánchez-López, et al., “Characterization of nanostructured Ti–B–(N) coatings produced by direct current magnetron sputtering,” Thin Solid Films, 515, 3590–3596 (2007).10.1016/j.tsf.2006.11.013 ↗
6. S. Carvalho, L. Rebouta, E. Ribeiro, et al., “Structural evolution of Ti–Al–Si–N nanocomposite coatings,” Vacuum, 83, 1206–1212 (2009).10.1016/j.vacuum.2009.03.009 ↗
7. P. J. Martin, A. Bendavid, J. M. Cairney, and M. Hoffman, “Nanocomposite Ti–Si–N, Zr–Si–N, Ti–Al–Si–N, Ti–Al–V–Si–N thin film coatings deposited by vacuum arc deposition,” Surf. Coat. Technol., 200, 2228–2235 (2005).10.1016/j.surfcoat.2004.06.012 ↗
8. Y. Tanaka, N. Ichimiya, Y. Onoshi, and Y. Yamada, “Structure and properties of Al–Ti–Si–N coatings prepared by the cathodic arc ion plating method for high speed cutting applications,” Surf. Coat. Technol., 146–147, 215–221 (2001).10.1016/S0257-8972(01)01391-3 ↗
9. Chi-Lung Chang, Jyh-Wei Lee, and Ming-Don Tseng, “Microstructure, corrosion, and tribological behaviors of TiAlSiN coatings deposited by cathodic arc plasma deposition,” Thin Solid Films, 517, 5231–5236 (2009).10.1016/j.tsf.2009.03.082 ↗
10. C. Rebholz, M. A. Monclus, M. A. Baker, et al., “Hard and superhard TiAlBN coatings deposited by twin electro-beam evaporation,” Surf. Coat. Technol., 201, 6078–6083 (2007).10.1016/j.surfcoat.2006.08.121 ↗
11. I. Zukerman, A. Raveh, Y. Shneor, et al., “Internal stress in TiAlBN at high temperatures,” Surf. Coat. Technol., 201, 6161–6166 (2007).10.1016/j.surfcoat.2006.08.136 ↗
12. C. Rebholz, A. Leyland, and A. Matthews, “Deposition and characterization of TiAlBN coatings produced by direct electron-beam evaporation of Ti and Ti–Al–B–N material from a twin crucible source,” Thin Solid Films, 343–344, 242–245 (1999).10.1016/S0040-6090(98)01635-6 ↗
13. D. V. Shtansky, A. N. Sheveiko, M. I. Petrzhik, et al., “Hard tribological Ti–B–N, Ti–Cr–B–N, Ti–Si–B–N, and Ti–Al–Si–B–N coatings,” Surf. Coat. Technol., 200, 208–212 (2005).10.1016/j.surfcoat.2005.02.126 ↗
14. Ph. V. Kiryukhantsev-Korneev, D. V. Shtansky, M. I. Petrzhik, et al., “Thermal stability and oxidation resistance of Ti–B–N, Ti–Cr–B–N, Ti–Si–B–N and Ti–Al–Si–B–N films,” Surf. Coat. Technol., 201, 6143–6147 (2007).10.1016/j.surfcoat.2006.08.133 ↗
15. C. Paternoster, A. Fabrizi, R. Cecchini, et al., “Thermal evolution and mechanical properties of hard Ti–Cr–B–N and Ti–Al–Si–B–N coatings,” Surf. Coat. Technol., 203, 736–740 (2008).10.1016/j.surfcoat.2008.08.013 ↗
16. A. Mahmood, R. Machorro, S. Muhl, et al., “Optical and surface analysis of DC-reactive sputtered AlN films,” Diamond Relat. Mater., 12, 1315–1321 (2003).10.1016/S0925-9635(03)00076-1 ↗
17. E. Benko, T. L. Barr, S. Hardcastle, et al., “XPS study of the cBN–TiC system,” Ceram. Intern., 27, 637–641 (2001).10.1016/S0272-8842(01)00011-6 ↗
18. M. A. Baker, “Advanced characterization of nanocomposite coatings,” Surf. Coat. Technol., 201, 6105–6111 (2007).10.1016/j.surfcoat.2006.08.118 ↗
19. Yan Guo, Shengli Ma, and Kewei Xu, “Effects of carbon content and annealing temperature on the microstructure and hardness of super hard Ti–Si–C–N nanocomposite coatings prepared by pulsed d.c. PCVD,” Surf. Coat. Technol., 201, 5240–5243 (2007).10.1016/j.surfcoat.2006.07.122 ↗
20. S. Veprek and A. S. Argon, “Towards the understanding of mechanical properties of super- and ultrahard nanocomposites,” J. Vac. Sci. Technol., B20, 650–665 (2002).10.1116/1.1459722 ↗