journal article·2004-01

Hard Alloy WC–24% Ni Obtained in the Solid Phase from Ultrafine WC, NiO, and C Powders. Part 2. Mechanical Properties

Laptev, Alexander I. Tolochin, Larisa F. Ochkas

Powder Metallurgy and Metal Ceramics· Volume 43· Issue 1-2
Publisher page

Abstract

Mechanical properties of WC–24 mass% Ni alloy prepared by a combination in single stage of metal phase synthesis and compaction of an ultrafine mixture of WC–Ni powders by high-energy compaction and sintering are studied. Tungsten carbide, nickel oxide, and carbon are selected as the starting powders. After milling the initial powders the average particle size is 200-300 nm. Previously compacted briquettes of WC + NiO + C are heated, sintered, and pressed in the range 950-1300°C at vacuum of 0.133 Pa. Briquettes are also sintered in the liquid phase at 1350°C for comparison. Ultimate strength in bending, fracture toughness, ultimate strength in compression, and Vickers hardness are determined for specimens prepared at different temperatures. The dependence of mechanical properties on specimen consolidation temperature is studied. It is shown that these dependences for pressed specimens have a maximum at 1200-1250°C. The high level of properties (ultimate strength in bending 2500 MPa, ultimate strength in compression 3100 MPa, fracture toughness 19 MPa·m1/2, and hardness 10.0 GPa) are achieved for a WC + Ni + C powder mixture to which carbon is added in the form of a liquid carbon-containing compound. Introduction into the mixture of commercial carbon grade P803 leads to low specimen mechanical properties. The effect on mechanical properties of porosity and pore size, and also grain boundary quality between particles is studied.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Orthopaedic implants and arthroplasty · Tunneling and Rock Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. A. V. Laptev, A. I. Tolochin, and L. F. Ochkas, “Hard alloy WC — 24% Ni prepared in the solid phase from ultrafine WC, NiO, and C powders. I. Specimen density and structure,” Poroshk. Metall., Nos. 11–12, 84–85 (2003).
2. S. Ekemar, L. Lindholm, and T. Hartzell, “Nickel as a binder in WC-based cemented carbide,” Int. J. Refract. Hard Metals., 1,No. 1, 37–40 (1982).
3. A. V. Laptev, S. S. Ponamarev, and L. F. Ochkas, “Study of the possibility of solid phase production of poreless WC — 26% Co hard metal with high-energy pressing,” Proc. EURO PM'99 Conf. on Advances in Hard Materials Production (8–10 November 1999, Turin, Italy), Turin (1999).
4. A. V. Laptev and L. F. Ochkas, “Study of solid-phase consolidation of ultrafine grained WC — 26% Ni hard metal during high-energy hot pressing,” Proc. Europ. Cong PM2001 (21–23 october 2001, Nice, France), Vol. 1, Nice (2001).
5. G. S. Upadhyaya and D. Banerjee, “Role of Cr3C2 on tungsten carbide based composites,” Proc. 14th Int. Plansee Seminar '97 (12–16 May 1997, Reutte, Tirol, Austria), Vol. 2, Reutte, Tyrol (1997).
6. V. V. Sverdel, A. V. Shatov, N. A. Yurchuk, and O. V. Bakun, “Finely dispersed WC — Ni hard alloys. I. Mechanical properties,” Poroshk. Metall., Nos. 1–2, 73–76 (1994).
7. A. F. Lisovskii, “Properties of sintered WC — Ni hard alloys with a nonuniform structure,” Poroshk. Metall., No. 11, 28–33 (1988).
8. H. E. Exner, “Understanding the toughness and the strength of WC — Co hard metals,” Proc. 1996 Conf. Eur. Conf. on Advances in Hard Materials Production (27–29 May 1996, Stockholm, Sweden), Stockholm (1996).
9. B. Roebuck, “Effect of testpiece geometry on the flexural strength of representative hard metals and cermets,” Proc. 14th Int. Plansee Seminar '97 (12–16 May 1997, Reutte, Tirol, Austria), Vol. 2, Reutte, Tyrol (1997).
10. A. V. Shatov, S. A. Firstov, V. V. Sverdel, and N. A. Yurchuk, “Finely dispersed WC — Ni hard alloys. III. Structure,” Poroshk. Metall., Nos. 11–12, 51–54 (1995).
11. J. L. Chermant and F. Osterstock, “Fracture toughness and fracture of WC — Co composites,” J. Mat. Sci., 11,No. 2, 1939–1951 (1976).10.1007/BF00708272 ↗
12. R. Warren and B. Johanneson, “The fracture toughness of hardness,” Int. J. Refract. Hard Metals, 2,No. 4, 187–191 (1984).
13. W. D. Schubert, H. Neumeister, G. Klinger, and B. Lux, “Hardness to toughness relationship for fine-grained WC — Co hard metals,” Proc. 14th Int. Plansee Seminar '97 (12–16 May 1997, Reutte, Tirol, Austria), Vol. 2, Reutte, Tyrol (1997).10.1016/S0263-4368(98)00028-6 ↗
14. K. Jia, T. Fischer, and B. Gallois, “The microstructure, hardness and toughness of nanostructured and conventional WC — Co composites,” Nanostructured Mat., 10,No. 5, 875 (1998).10.1016/S0965-9773(98)00123-8 ↗
15. G. Gille, B. Szesny, K. Dreyer, H. Van Den Berg, et al., “Submicron and ultrafine grained hard metal for microdrills and metal cutting inserts,” Proc. 15th Int. Plansee Seminar'97 (27 May–1 June 2001, Reutte, Tirol, Austria), Vol. 2, Reutte, Tyrol (2001).
16. A. V. Laptev, S. S. Ponomarev, and L. F. Ochkas, “Solid phase consolidation fine grained WC — 16 mass% Co hard metals,” J. Advanced Mat., 33,No. 3, 42–51 (2001).