Synthesis and characterization of porous Fe–25 wt.% Al alloy with controllable pore structure
Source abstract
Abstract
Porous Fe-25 wt.% Al alloy is synthesized by reactive synthesis with Fe and Al powders as the raw materials. Various processing parameters such as the final sintering temperature, pressure during cold pressing, and powder size are investigated to control the pore structure of the alloy. It has been shown that the optimal final sintering temperature is around 950-1050 degrees C. When the pressure is higher than 110 MPa, the variation of the pore structure is mainly caused by the change of the pore nature in the as-pressed compact. In addition, the pore structure of porous Fe-25 wt.% Al alloys depends on the size of the raw powders and the weight fraction of different-sized raw powders. ©2010 Springer Science+Business Media, Inc.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Cellular and Composite Structures · Aluminum Alloys Composites Properties · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. S. C. Deevi, V. K. Sikka, and C. T. Liu, “Processing, properties, and applications of nickel and iron aluminides,” Prog. Mater. Sci., 42, 177–192 (1997).10.1016/S0079-6425(97)00014-5 ↗
2. A. Paul, M. J. H. Dal, A. A. Kodentsov, et al., “The Kirkendall effect in multiphase diffusion,” Acta Mater., 52, 623–630 (2004).10.1016/j.actamat.2003.10.007 ↗
3. A. Bouayad, C. Gerometta, A. Belkebir, et al., “Kinetic interactions between solid iron and molten aluminum,” Mater. Sci. Eng. A, 363, 53–61 (2003).10.1016/S0921-5093(03)00469-6 ↗
4. R. Nakamura, K. Takasawa, Y. Yamazaki, et al., “Single-phase interdiffusion in the B2 type intermetallic compounds NiAl, CoAl and FeAl,” Intermetallics, 10, 195–204 (2002).10.1016/S0966-9795(01)00125-X ↗
5. C. T. Liu, E. P. George, P. J. Mazias, et al., “Recent advances in B2 iron aluminide alloys: deformation, fracture and alloy design,” Mater. Sci. Eng. A, 258, 84–98 (1998).10.1016/S0921-5093(98)00921-6 ↗
6. T. Grosdidiier, E. Suzon, and F. Wagner, “Primary recrystallization in an ODS FeAl alloy: an effective way to modify texture and microstructure,” Intermetallics, 12, 645–654 (2004).10.1016/j.intermet.2004.03.014 ↗
7. N. Masahashi, K. Komatsu, S. Watanabe, et al., “Microstructure and properties of iron aluminum alloy/CrMo steel composite prepared by clad rolling,” J. Alloy Compd., 379, 272–279 (2004).10.1016/j.jallcom.2004.02.043 ↗
8. M. A. Munoz-Morris, O. C. Garcia, and D. G. Morris, “Microstructure and room temperature strength of Fe-40Al containing nanocrystalline oxide particle,” Acta Mater., 51, 5187–5197 (2003).10.1016/S1359-6454(03)00382-3 ↗
9. M. Krasnowski and T. Kulik, “Nanocrystalline FeAl intermetallic produced by mechanical alloying followed by hot-pressed consolidation,” Intermetallics, 15, 201–205 (2007).10.1016/j.intermet.2006.05.008 ↗
10. H. Skoglund, M. Knutson, and B. Karisson, “Processing of fine-grained mechanically alloyed FeAl. Intermetallics,” Intermetallics, 12, 977–983 (2004).10.1016/j.intermet.2004.03.004 ↗
11. J. Banhart, “Manufacture, characterization and application of cellular metals and metal foams,” Prog. Mater. Sci., 46, 559–632 (2001).10.1016/S0079-6425(00)00002-5 ↗
12. J. She and T. Ohji, “Thermal Shock Behavior of Porous Silicon Carbide Ceramics,” J. Am. Soc., 85, 2125–2127 (2002).
13. P. S. Liu, Introduction to Cellular Materials, Tsinghua University Press, Beijing (2004), p.98.
14. Y .H. He, Y. Jiang, N. P. Xu, et al., “Fabrication of Ti–Al Micro/Nanometer-Sized Porous Alloys through the Kirkendall Effect,” Adv. Mater., 19, 2102–2106 (2007).10.1002/adma.200602398 ↗
15. Y. Jiang, Y. H. He, N. P. Xu, et al., “Effects of the Al content on pore structures of porous Ti-Al alloys,” Intermetallics, 16, 327–332 (2008).10.1016/j.intermet.2007.11.002 ↗
16. H. Y. Gao, Y. H. He, P. Z. Shen, et al., “Effect of heating rate on pore structure of porous FeAl material,” Powder Metall., 51, 171–175 (2008).10.1179/174329008X271673 ↗
17. R. M. German, Powder Metallurgy Science, Metal Powder Industries Federation, Princeton (1994), pp. 207–370.
18. B. J. Wang and H. S. Gao, Analytical Chemistry, Higher Education Press, Beijing (1995), p.18.
19. S. Ranganath, T. L. Prakash, and J. Subrahmanyam, “Synthesis of iron aluminide under thermal explosion conditions,” Mater. Lett., 10, 215–217 (1990).10.1016/0167-577X(90)90091-Y ↗
20. S. Gedevanishvili and S. C. Deevi, “Processing of iron aluminides by pressureless sintering through Fe+Al elemental route,” Mater. Sci. Eng. A, 325, 163–176 (2002).10.1016/S0921-5093(01)01442-3 ↗
21. K. Morsi, T. Fujii1, H. McShane, et al., “Control of heat generation during reaction synthesis,” Scripta Mater., 40, 359–364 (1999).10.1016/S1359-6462(98)00439-4 ↗
22. ASM, ASM Handbook, Vol. 2 [in Chinese], Mechanical Industry Press, Beijing (1975), p. 906.
23. P. Y. Huang, Principles of Powder Metallurgy, Metallurgical Industry Press, Beijing (1997), p. 174.