journal article·2013-01

Microstructure, Growth Kinetics, and Abrasive Wear Resistance of Boride Layers on Fe–30% Cr Alloy

V. I. Dybkov, V. R. Sidorko, L. V. Goncharuk, V. G. Khoruzha, A. V. Samelyuk

Powder Metallurgy and Metal Ceramics· Volume 51· Issue 9-10
Publisher page

Abstract

Two boride layers are found to form at the interface between reacting phases in the course of boriding a Fe–30% Cr alloy in boron powder with KBF4 (activator) in the temperature range of 850–950°C and reaction times 3600–43200 sec (1–12 h). Each of these layers is single-phase structurally (crystallographically) and two-phase compositionally (chemically). The outer boride layer bordering boron consists of the crystals of the (Fe, Cr)B and (Cr, Fe)B compounds, while the inner layer adjacent to the alloy base comprises the crystals of the (Fe, Cr)2B and (Cr, Fe)2B compounds. The characteristic feature of both layers is a profound texture. Diffusional layer-growth kinetics are close to parabolic and can alternatively be described by a system of two non-linear differential equations dx/dt = (kB/x) – (rgkFe/py), dy/dt = (kFe/y) – (qkB/sgx), where x is the outer FeB layer thickness (m), y is the inner Fe2B layer thickness (m), kB is the FeB layer growth-rate constant (m2⋅sec–1), kFe is the Fe2B layer growth-rate constant (m2⋅sec–1), g is the ratio of the FeB and Fe2B molar volumes, p = q = r = 1, and s = 2 (factors from the chemical formulae of FeB and Fe2B). The temperature dependence of the layer growth-rate constants obeys a relation of the Arrhenius type K = Aexp (–E/RT), where K stands for any constant, A is the frequency factor, E is the activation energy, R is the gas constant, and T is the absolute temperature. Application of the least-squares fit method yielded the following equations: kB = 3.42⋅10–8⋅exp(–175.4 kJ × × mol–1/RT) m+⋅sec–1, kFe = 7.45⋅10–9 exp(–144.6 kJ⋅mol–1/RT) m2⋅sec–1. Microhardness values are 18.1 GPa for the outer boride layer, 15.2 GPa for the inner layer, and 1.75 GPa for the alloy base. The dry abrasive wear resistance of the outer boride layer, found from mass loss measurements, is more than 300 times greater than that of the Fe–30% Cr alloy base. Such a huge increase in wear resistance is due to the microstructure of boride layers having a peculiar regular arrangement of enhanced rigidity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. L. G. Voroshnin and L. S. Lyakhovich, Borided Steels [in Russian], Metallurgiya, Moscow (1978), p. 240.
2. L. G. Voroshnin, Boriding of Industrial Steels and Cast Iron [in Russian], Minsk, Belarus (1981), p. 208.
3. M. Hansen, Constitution of Binary Alloys, 2nd ed., McGraw-Hill, New-York (1958), p. 249.
4. H. Okamoto, “B-Fe (boron–iron),” J. Phase Equilib. Diffusion, 25, 297–298 (2004).10.1007/s11669-004-0128-3 ↗
5. P. Goeuriot, R. Fillit, F. Thevenot, et al., “The influence of alloying element additions on the boriding of steels,” Mater. Sci. Eng., 55, No. 1, 9–19 (1982).10.1016/0025-5416(82)90078-7 ↗
6. G. Palombarini, M. Carbucicchio, and L. Cento, “Electron probe microanalysis of nickel and chromium in Fe–Cr–Ni and Fe–C–Cr alloys borided at 850°C,” J. Mater. Sci., 19, No. 11, 3732–3738 (1984).10.1007/BF02396946 ↗
7. K. Genel, I. Ozbek, and C. Bindal, “Kinetics of boriding of AISI W1 steel,” Mater. Sci. Eng. A, 347, No. 1–2, 311–314 (2003).10.1016/S0921-5093(02)00607-X ↗
8. M. Kulka and P. Pertek, “Microstructure and properties of borided 41Cr4 steel after laser surface modification with remelting,” Appl. Surf. Sci., 214, 278–288 (2003).10.1016/S0169-4332(03)00500-2 ↗
9. E. Galvanetto, F. Borgioli, T. Bacci, and G. Pradelli, “Wear behavior of iron boride coatings produced by VPS technique on carbon steels,” Wear, 260, No. 7–8, 825–831 (2006).10.1016/j.wear.2005.04.005 ↗
10. S. Taktak, “A study on the diffusion kinetics of borides on boronized Cr-based steels,” J. Mater. Sci., 41, No. 22, 7590–7596 (2006).10.1007/s10853-006-0847-4 ↗
11. I. Campos, R. Rosas, U. Figueroa, et al., “Fracture toughness evaluation using Palmqvist crack models on AISI 1045 borided steels,” Mater. Sci. Eng. A, 488, No. 1–2, 562–568 (2008).10.1016/j.msea.2007.11.082 ↗
12. X. Tian, Y. Lu, S. J. Sun, et al., “Effect of boronizing on mechanical properties, wear and corrosion of N80 steel,” Mater. Sci. Technol., 24, No. 3, 314–319(6) (2008).10.1179/174328408X278448 ↗
13. V. I. Dybkov, W. Lengauer, and K. Barmak, “Formation of boride layers at the Fe–10%Cr alloy–boron interface,” J. Alloys Compd., 398, 113–122 (2005).10.1016/j.jallcom.2005.02.033 ↗
14. V. I. Dybkov, V. R. Sidorko, V. G. Khoruzha, et al., “Interaction of 25% chromium steel with boron powder,” Powder Metall. Met. Ceram., 50, No. 7–8, 564–571 (2011).10.1007/s11106-011-9360-7 ↗
15. L. I. Mirkin, Handbook on X-Ray Diffraction Analysis of Polycrystals [in Russian], Fizmatgiz, Moscow (1961).
16. S. S. Gorelik, L. N. Rastorguev, and Yu. A. Skakov, X-Ray Analysis and Electron Optical Analysis: Applications [in Russian], Metallurgiya, Moscow (1970), p. 106.
17. V. A. Barinov, G. A. Dorofeev, L. V. Ovechkin, and E. P. Elsukov, “Structure and magnetic properties of the α-FeB phase obtained by mechanical working,” Phys. Status Solidi A, 123, 527–534 (1991).10.1002/pssa.2211230217 ↗
18. C. Gianoglio and C. Badini, “Distribution equilibria of iron and nickel in two phase fields of the Fe–Ni–B system,” J. Mater. Sci., 21, 4331–4334 (1986).10.1007/BF01106551 ↗
19. S. Okada, T. Atoda, and I. Higashi, “Structural investigation of Cr2B3, Cr3B4, and CrB by single-crystal diffractometry,” J. Solid State Chem., 68, 61–67 (1987).10.1016/0022-4596(87)90285-4 ↗
20. C. Gianoglio, G. Pradelli, and M. Vallino, “Solid state equilibria in the Cr–Fe–B system at the temperature of 1373 K,” Metall. Sci. Technol., 1, 51–57 (1983).
21. A. A. Bondar, “Boron–chromium–iron,” in: G. Effenberg and S. Ilyenko (eds.) Landolt-Börnstein, Vol. 11D1, Springer, Berlin–Heidelberg (2007), pp. 320–343.
22. C. Martini, G. Palombarini, and M. Carbucicchio, “Mechanism of thermochemical growth of iron borides on iron,” J. Mater. Sci., 39, No. 3, 933–937 (2004).10.1023/B:JMSC.0000012924.74578.87 ↗
23. J. Brandstötter and W. Lengauer, “Reaction diffusion in transition metal–boron systems,” J. Alloys Compd., 390–396, 390–396 (1997).10.1016/S0925-8388(97)00342-3 ↗
24. W. Seith, Diffusion in Metals [in German], Springer, Berlin (1955).10.1007/978-3-642-53297-9 ↗
25. K. Hauffe, Reactions in and on Solids [in German], Springer, Berlin (1955).
26. V. I. Dybkov, Reaction Diffusion and Solid State Chemical Kinetics, Trans Tech Publications, Zürich (2010), p. 334.
27. V. I. Dybkov, W. Lengauer, and P. Gas. “Formation of boride layers at the Fe–25% Cr alloy–boron interface,” J. Mater. Sci., 41, No. 15, 4948–4960 (2006).10.1007/s10853-006-0032-9 ↗
28. V. I. Dybkov, “Growth of boride layers on the 13% Cr steel surface in a mixture of amorphous boron and KBF4,” J. Mater. Sci., 42, No. 16, 6614–6627 (2007).10.1007/s10853-007-1512-2 ↗
29. V. I. Dybkov, “Diffusional growth kinetics of boride layers at the 13% Cr steel interface with amorphous boron,” Defect Diffusion Forum, 263, 183–188 (2007).10.4028/www.scientific.net/DDF.263.183 ↗
30. V. I. Dybkov, L. V. Goncharuk, V. G. Khoruzha, et al., “Diffusional growth kinetics of boride layers on iron–chromium alloys,” Solid State Phenom., 138, 181–187 (2008).10.4028/www.scientific.net/SSP.138.181 ↗
31. V. I. Dybkov, L. V. Goncharuk, V. G. Khoruzha, et al., “Growth kinetics and abrasive wear resistance of boride layers on Fe–15% Cr alloy,” Mater. Sci. Technol., 27, No. 10, 1502–1512 (2011).10.1179/026708310X12683157551577 ↗