Abstract

Blends of poly(methyl methacrylate) (PMMA) with ethylene - methyl acrylate (EMA) copolymers of different compositions, viz. 95/05, 90/10, 85/15 and 80/20 wt.% were prepared by a melt mixing technique using a twin-screw extruder. The blends were characterized by thermo-analytical methods, viz. differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) and dynamic mechanical analysis (DMA). The TGA of PMMA/EMA blends show that thermal degradation takes place in two steps and the temperature of the decomposition rate maximum is proportional to the compositions of the blends. The DSC studies reveal two glass-transition temperatures (T g ) for all the blends corresponding to their individual components which indicates that the blends are incompatible. The DMA thermograms exhibit two steps in the dynamic modulus-temperature curves for higher EMA content, which is characteristic of immiscible polymers in a two phase system.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Polymer crystallization and properties · Polymer Nanocomposites and Properties · biodegradable polymer synthesis and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Central Institute of Plastics Engineering and Technology, City Centre, Debhog, Purba, Medinipur, Haldia-721657, India

Central Institute of Plastics Engineering and Technology, IDA, Phase-II, Cherlapally, Hyderabad-500051, India

Department of Polymer Science & Technology, Sri Jayachamarajendra College of Engineering, Mysore-570006, India

References (27)

Show source-provided references
1. Sperling L.H. · 1997
2. 10.1016/B978-0-12-546802-2.50012-910.1016/B978-0-12-546802-2.50012-9 ↗
3. 10.1007/978-1-4615-5789-010.1007/978-1-4615-5789-0 ↗
4. Utracki L.A. · 2002 · 1
5. 10.1080/1060132050020576410.1080/10601320500205764 ↗
6. 10.1016/j.polymertesting.2006.08.00910.1016/j.polymertesting.2006.08.009 ↗
7. 10.1016/0014-3057(70)90017-010.1016/0014-3057(70)90017-0 ↗
8. 10.1002/pol.1976.17014020810.1002/pol.1976.170140208 ↗
9. 10.1080/0022233780806316110.1080/00222337808063161 ↗
10. 10.1007/BF0218885410.1007/BF02188854 ↗
11. 10.1016/j.polymdegradstab.2005.07.00310.1016/j.polymdegradstab.2005.07.003 ↗
12. 10.1002/app.2669610.1002/app.26696 ↗
13. 10.1007/BF0055027410.1007/BF00550274 ↗
14. 10.1021/ma991453v10.1021/ma991453v ↗
15. KotamaK., Jpn. Pat. 009, 740, 1972, Mitsubishi Rayon Company Limited.
16. KishikawaH., YasunoK., and KitamuraS. Ger. Offen. 2,119,376, (1971), Sumitomo Chemical Company Limited.
17. 10.1016/0032-3950(90)90071-D10.1016/0032-3950(90)90071-D ↗
18. 10.1016/j.polymer.2006.03.10810.1016/j.polymer.2006.03.108 ↗
19. 10.1002/app.2848610.1002/app.28486 ↗
20. Kalkar R.A. · Polymer Science Contemporary Themes II · 1991 · 894
21. 10.1007/BF0110681110.1007/BF01106811 ↗
22. Ward I.M. · 1971
23. 10.1002/pol.1954.12013720510.1002/pol.1954.120137205 ↗
24. 10.1016/0032-3861(64)90199-510.1016/0032-3861(64)90199-5 ↗
25. 10.1002/pol.1960.120421390210.1002/pol.1960.1204213902 ↗
26. Heijboer J. · 1965
27. 10.1002/pol.1970.16008120610.1002/pol.1970.160081206 ↗