Photoluminescence, phosphorescence, the relative quantum efficiency, and the buildup of the luminescence are studied in zinc orthosilicate doped with different Mn and Ga concentrations. Peak emissions are found at 405 and 525 nm. For excitation in the absorption bands due to the Gadoping (γex < 270 nm) the Zn2SiO4: Mn: Ga shows a fatiguing with prolonged excitation and a long persistent decay of the green luminescence. The fatiguing can be reversed by keeping the sample in dark at a given temperature for a time td, or by irradiation with wavelengths 270 nm < γ < < 460 nm. The fatiguing is ascribed to trapping of holes from excited donar-centers by Mn-centers. Die Photolumineszenz, die Phosphoreszenz, die relative Quantenausbeute und das Anklingen der Lumineszenz werden bei Zinkorthosilikat bei verschiedenen Mn- und Ga-Dotierungskonzentrationen untersucht. Die Emissionsmaxima liegen bei 405 und 525 nm. Bei Anregung in die Absorptionsbande infolge Ga-Dotierung (γex < 270 nm) zeigt Zn2SiO4:Mn:Ga eine Abnahme der Quantenausbeute, mit zunehmcnder Anregungsdauer und ein langanhaltendes Abklingen der grünen Lumineszenz. Dieser Ermüdungseffekt kann rückgängig gemacht werden, wenn die Probe eine der jeweiligen Temperatur entsprechende Zeit im Dunkeln gehalten oder mit Wellenlängen 270 nm < γ < < 460 nm bestrahlt wird. Der Ermüdungseffekt wird dem Einfang von Löehern von angeregten Donatoren durch die Mn-Zentren zugeschrieben.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Glass properties and applications · Luminescence Properties of Advanced Materials · Photonic Crystals and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.