journal article·2009-07

Effect of deposition temperature on the microstructure and dielectric properties of Ba0.6Sr0.4TiO3 thin film deposited by radio‐frequency magnetron sputtering

Zuyong Feng, Wei Chen, Ooi Kiang Tan

physica status solidi (a)· Volume 206· Issue 7
Publisher page

Abstract

Abstract Ba0.6Sr0.4TiO3 (BST) thin films with the thickness of 300 nm were deposited on Pt/SiO2/Si substrates at various deposition temperatures by RF magnetron sputtering technique, and their electric properties were investigated. Due to the high temperature annealing process at substrate temperature of 600 °C, well‐crystallized BST film was deposited. The dielectric constant and dielectric loss of the film deposited at 600 °C are 300 and 0.033 at 100 kHz, respectively. Due to the good crystallinity of the BST films deposited by RF magnetron sputtering, high dielectric tunability up to 39.2% is achieved at a low applied voltage of 5 V. (© 2009 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. 10.1088/0022-3727/41/6/06300110.1088/0022-3727/41/6/063001 ↗
2. 10.1063/1.237257510.1063/1.2372575 ↗
3. 10.1063/1.12621210.1063/1.126212 ↗
4. P.Scheele S.Muller C.Weil andR.Jakoby Proceedings of the 34th European Microwave Conference (Amsterdam Holland 2004) p. 1501.
5. 10.1088/0964-1726/8/2/00910.1088/0964-1726/8/2/009 ↗
6. 10.1063/1.156939210.1063/1.1569392 ↗
7. 10.1063/1.139472310.1063/1.1394723 ↗
8. 10.1063/1.134086310.1063/1.1340863 ↗
9. 10.1063/1.12527210.1063/1.125272 ↗
10. 10.1063/1.135914110.1063/1.1359141 ↗
11. 10.1088/0022-3727/37/16/00610.1088/0022-3727/37/16/006 ↗
12. 10.1063/1.131823310.1063/1.1318233 ↗
13. 10.1063/1.149483710.1063/1.1494837 ↗
14. 10.1143/JJAP.32.412610.1143/JJAP.32.4126 ↗
15. 10.1063/1.36358310.1063/1.363583 ↗
16. 10.1063/1.36687210.1063/1.366872 ↗
17. 10.1063/1.215955710.1063/1.2159557 ↗
18. 10.1063/1.275435810.1063/1.2754358 ↗
19. 10.1063/1.302671910.1063/1.3026719 ↗
20. 10.1143/JJAP.36.694610.1143/JJAP.36.6946 ↗
21. 10.1109/58.85206710.1109/58.852067 ↗
22. 10.1063/1.222053010.1063/1.2220530 ↗
23. 10.1088/0022-3727/39/11/02410.1088/0022-3727/39/11/024 ↗
24. 10.1016/S0254-0584(01)00566-110.1016/S0254-0584(01)00566-1 ↗
25. 10.1063/1.36566510.1063/1.365665 ↗
26. Varadan V. K. · Microw. J. · 1992 · 35 · 116
27. 10.1088/0953-8984/16/41/L0410.1088/0953-8984/16/41/L04 ↗
28. 10.1063/1.299076010.1063/1.2990760 ↗