Dielectric properties of TbAsO4 single crystals

Binod Kumar Choudhary, R. N. P. Choudhary, K. V. Rao

Publisher page

Abstract

The dielectric constant (K), loss (tan σ), and hence conductivity (σ) of TbAsO4 single crystals are measured in the frequency range 102 to 107 Hz and in the temperature region 30 to 350 °C. These measurements are also taken after the crystals are irradiated with γ-rays. K of TbAsO4 at 30 °C is found to decrease with frequency attaining a constant value beyond 105 Hz. Similar behaviour is exhibited by tan σ. The values of K and tan σ for TbAsO4 crystals at 106 Hz and 30 °C are 8.3 and 3.40 × 10−3, respectively. K increases slowly with temperature up to about 190 °C beyond which the increase is faster and considerably frequency dependent. γ-ray irradiation increases the low-frequency K and tan σ values but has practically no effect on the high-frequency values. Log σ versus 1/T plots at different frequencies give the activation energy for conduction in the intrinsic region as 0.70 eV. Log ΔK against 1/T plots (ΔK is the difference between the dielectric constant at any temperature and the value at 30 °C) yields an activation energy value of 0.65 eV in the same temperature region. This suggests that the same charge carriers are responsible for the two processes (increase in K and σ) in the high-temperature region.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Solid-state spectroscopy and crystallography · Photorefractive and Nonlinear Optics · Luminescence Properties of Advanced Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.