For hydrogen-free and non-deformed Nb and Ta, the resonant vibrational period P and internal friction Q−1 of the specimen after low temperature 20 MeV proton irradiation arc investigated. In Ta, a strong dislocation pinning is firstly observed during irradiation at 5.8 K suggesting random diffusion of self-interstitial atoms (SIA's) at 5.8 K. After the saturation of the pinning effects, the linear increase in P,ΔP/P (i.e. the decrease in the Young modulus Y, -ΔY/Y) with increasing dose ΔΦ t is revealed during irradiation at 5.8 to 20 K in the dose range up to the total Frenkel pair production, CFP, of ≈ 500 at ppm. the magnitude of (ΔY/Y)/CFP is a few percent of those reported in Mo and Ag. The linear ΔP/P vs. ΔΦ t found in the wide CFP range suggests that in Ta during irradiation, the SIA's survived are mainly those trapped by impurity atoms and SIA clusters are formed little. On the other hand, in non-deformed Nb irradiated at 5.3 K or above, a linear increase in P with dose is observed from the beginning and (ΔY/Y)/CFP is four times larger than in Ta. Above a CFP of 80 at ppm, (ΔP/P)/ΔΦ t shows a deviatory increase. The non-observation of pinning in non-deformed Nb is not in contradiction with the random diffusion of SIA at 5.3 K but indicate that SIA's on dislocations in Nb are unstable as suggested in a previous work on dislocation pinning in deformed Nb. In Nb during irradiation, the SIA's tend to form more SIA-clustcrs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fusion materials and technologies · Metal and Thin Film Mechanics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.