A comparative study of zinc tracer diffusion profiles in LEC, SSD, and CVD GaP

E. Nebauer

Publisher page

Abstract

Zinc tracer concentration profiles C(x) in LEC, CVD, and SSD GaP samples are measured at 850 °C. In agreement with published investigations it is found that the single-crystalline Czochralski material having about 105 disloctions/cm2 shows only the bulk part in C(x) down to some 1017 Zn atoms/cm3. The C profiles of well-grown CVD layers agree with those of the LEC crystals, but those of layers having high dislocation densities exhibit exponential tail regions. Similarly in polycrystalline SSD material the C distributions consist of two parts, the fast component being due to grain-boundary diffusion. Es werden bei 850 °C Zink-Tracer-Konzentrationsprofile C(x) in LEC, CVD und SSD GaP Proben vergleichsweise gemessen. In Übereinstimmung mit anderweitig veröffentlichten Arbeiten wird gefunden, daß Czochralski-Material (mit größenordnungsmäßig 105 Versetzungen/cm2) bis zu einigen 1017 Zn-Atomen/cm3 herab nur die Volumendiffusionskomponente in C(x) aufweist. Die C(x)-Profile von CVD-Schichten passabler Perfektion stimmen mit denen von LEC-Kristallen überein, hingegen zeigen Schichten mit hohen Versetzungsdichten exponentielle Schwanzregionen. In ähnlicher Weise besitzen die C(x)-Verteilungen von polykristallinem Material zwei Abschnitte, wobei die schnelle Komponente durch Korngrenzendiffusion zustandekommt.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Copper Interconnects and Reliability · Semiconductor materials and interfaces · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.